Tyumeneva T.Y., Kogtenkov A.S., Lukina N.F., Chursova L.V. Influence of fillers on properties of adhesives of industrial rubber assignment // Proceedings of VIAM. 2014. No. 4. Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2014-0-4-5-5.

Influence of fillers on properties of adhesives of industrial rubber assignment

Tyumeneva T.Y., Kogtenkov A.S., Lukina N.F., Chursova L.V.
Abstract
The description of researches of influence of fillers on properties of earlier developed adhesives and new development of VIAM Federal State Unitary Enterprise in the field of the adhesives of industrial rubber assignment intended for aviation engineering is provided. The main properties of adhesives of cold curing and the adhesives intended for compound of rubbers with metals in the course of curing, containing different fillers are stated. Advantages of new development in comparison with existing or applied earlier are shown.
Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Grashhenkov D.V., Chursova L.V. Strategija razvitija polimernyh kompozicionnyh i funkcional'nyh materialov [The development strategy of polymer composite and functional materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  3. Kardashov D.A., Petrova A.P. Polimernye klei [Polymer adhesives]. M.: Himija. 1983. 256 s.
  4. Petrova A.P., Donskoj A.A., Chalyh A.E., Shherbina A.A. Klejashhie materialy. Germetiki [Adhesives. Sealants]: Spravochnik. SPb.: NPO «Professional». 2008. 589 s.
  5. Lukina N.F., Dement'eva L.A., Petrova A.P., Tyumeneva T.Y. Properties of adhesives and adhesive materials used in aviation industry //Polymer Science. Series D. 2009. T. 2. №3. P. 147–154.
  6. Petrova A.P., Lukina N.F., Dement'eva L.A., Tjumeneva T.Ju., Avdonina I.A., Zhadova N.S. Klei dlja aviacionnyh materialov [Adhesives for aircraft materials] //Rossijskij himicheskij zhurnal. 2010. T. IV. №1. S. 46–52.
  7. Dement'eva L.A., Tjumeneva T.Ju., Sharova I.Ju. Klei s ponizhennoj gorjuchest'ju dlja aviacionnoj tehniki [Adhesives with reduced flammability for aircraft] /V sb. dokladov VI Mezhdunarodnoj konf. «Polimernye materialy ponizhennoj gorjuchesti». VoGTU. 2011. S. 127–128.
  8. Sytyj Ju.V., Sagomonova V.A., Kisljakova V.I., Bol'shakov V.A. Novye vibropogloshhajushhie materialy [New vibration-absorbing materials] //Aviacionnye materialy i tehnologii. 2012. №2. S. 51–54.
  9. Petrova A.P. Osnovnye jetapy tehnologii skleivanija [Main stages of bonding technology] //Klei. Germetiki. Tehnologii. 2014. №2. S. 24–30.
  10. Lukina N.F., Dement'eva L.A., Petrova A.P., Tjumeneva T.Ju. Svojstva kleev i klejashhih materialov dlja izdelij aviacionnoj tehniki [Properties of adhesives and adhesive materials for aircraft products] //Klei. Germetiki. Tehnologii. 2009. №1. S. 14–24.
  11. Petrova A.P., Lukina N.F., Dement'eva L.A., Tyumeneva T.Y., Avdonina I.A., Zhadova N.S. Adhesives for aviation equipment //Russian Journal of General Chemistry. 2011. T. 81. №5. P. 1014–1021.
  12. Petrova A.P., Lukina N.F. Klei dlja mnogorazovoj kosmicheskoj sistemy [Adhesives for reusable space system] //Trudy VIAM. 2013. №4. St. 04 (viam-works.ru).
  13. Sharova I.A., Petrova A.P. Obzor po materialam Mezhdunarodnoj konferencii po klejam i germetikam WAC-2012 [Browse by materials of the International conference on adhesives and sealants WAC-2012] //Trudy VIAM. 2013. №8. St. 06 (viam-works.ru).
  14. Lukina N.F., Dement'eva L.A., Petrova A.P., Serezhenkov A.A. Konstrukcionnye i termostojkie klei [Structural and heat-resistant adhesives] //Aviacionnye materialy i tehnologii. 2012. №S. S. 328–335.
  15. Volkov K.V., Danilenko V.V., Elin V.I. i dr. Sintez almaza iz ugleroda produktov detonacii VV [Synthesis of diamond from carbon detonation products VV] //Fizika gorenija i vzryva.1990. T. 3. №26. S. 123–125.
  16. Sakovich G.V., Titov V.M., Brylyakov P.M. Synthesis of diamonds clusters by explosion /In: Proc. X Intern. Conf. «High Energy Rate Fabrication». Ljubliana. 1989. P. 179–188.
  17. Tyumeneva T.Y., Lukina N.F. VKR-95 cold-setting adhesive with enhanced strength //Polymer Science. Series D. 2010. T. 3. №2. S. 114–116.
  18. Kleevaja kompozicija [The adhesive composition]: pat. 2471842 Ros. Federacija; opubl. 11.05.2011.
  19. Tjumeneva T.Ju., Kogtjonkov A.S., Lukina N.F., Chursova L.V. Uspehi v oblasti razrabotki kleev i tehnologij dlja izgotovlenija rezinotehnicheskih izdelij aviacionnogo naznachenija [Progress in the development of adhesives and technologies for the manu-facture of rubber products aviation applications] //Klei. Germetiki. Tehnologii. 2013. №10. S. 7–10.
  20. Tjumeneva T.Ju., Lukina N.F. Klei dlja skleivanija rezin mezhdu soboj i s drugimi materialami [Adhesives for bonding rubber between themselves and with other materials] /V sb. materialov dokladov seminara. CRDZ. 2008. S. 11–12.