Sidorov V.V., Rigin V.E., Filonova E.V., Timofeeva O.B. The structure investigations and properties of VGM4-VI and VGM5-VI single crystal alloys with increased phosphorus quantity // Proceedings of VIAM. 2014. No. 3. Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2014-0-3-2-2.

The structure investigations and properties of VGM4-VI and VGM5-VI single crystal alloys with increased phosphorus quantity

Sidorov V.V., Rigin V.E., Filonova E.V., Timofeeva O.B.
Abstract

The effect of phosphorus impurity on structure transformation and stress rupture properties of VGM4-VI and VGM5-VI single crystal alloys was investigated. It was es-tablished that a phosphorus at increased content (above 0,01%) reduces the stress rup-ture properties. Using the scanning electron microscope method it was established that a phosphorus at increased content (above 0,01%) increases a quantity of microcracks near rupture place, favours more intensive proceeding the process of hardenable γ'-phase coagulation, enriches the areas near eutectic γ'-phase and favours melt of the structure components at heat treamtent. For neutralization of harmful phosphorus influence in alloys the rear earth metal – lanthanum application is effective.

Keywords
phosphorus, lanthanum, structure, st
Reference list
  1. Kablov E.N., Sidorov V.V., Rigin V.E., Gorjunov A.V. Sovremennye tehnologii poluchenija prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokolenija [Modern technologies for bar stock of casting superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. C. 97–105.
  2. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Casting nickel superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–51.
  3. Kablov D.E., Sidorov V.V., Min P.G. Vlijanie primesi azota na strukturu monokristallov zharoprochnogo nikelevogo splava ZhS30-VI i razrabotka jeffektivnyh sposobov ego rafinirovanija [Influence of nitrogen impurities on the structure of single-crystal superal-loy nickel alloy ZHS30-VI and develop effective ways of refining its] //Aviacionnye materialy i tehnologii. 2012. №2. S. 32–36.
  4. Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E., Kablov D.E. Osobennosti tehnologii vyplavki i razlivki sovremennyh litejnyh vysokozharoprochnyh nikelevyh splavov [Technology features modern smelting and casting casting nickel-base superalloys] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. Spec. vyp. «Perspektivnye konstrukcionnye materialy i tehnologii». S. 68–78.
  5. Sidorov V.V., Rigin V.E., Gorjunov A.V., Kablov D.E. Vysokojeffektivnye tehnologii i sovremennoe oborudovanie dlja proizvodstva shihtovyh zagotovok iz litejnyh zharo-prochnyh splavov [Enabling technologies and modern equipment for production of charge billets casting superalloys] //Metallurg. 2012. №5. S. 26–30.
  6. Kablov D.E., Chabina E.B., Sidorov V.V., Min P.G. Issledovanie vlijanija azota na strukturu i svojstva monokristallov iz litejnogo zharoprochnogo splava ZhS30-VI [In-vestigation of the influence of nitrogen on the structure and properties of single crystals of cast superalloy ZHS30-VI] //MiTOM. 2013. №8. S. 3–7.
  7. Kablov D.E., Beljaev M.S., Sidorov V.V., Komarova T.I. Issledovanie vlijanija primesi azota na malociklovuju ustalost' monokristallov zharoprochnogo nikelevogo splava ZhS30-VI [Investigation of the influence of nitrogen impurity on the low-cycle fatigue of single crystals heat-resistant nickel alloy ZHS30-VI] //MiTOM. 2012. №7. S. 46–47.
  8. Yaoxiao Zhu, John Radavich et al. The development and Long-Time Structual Stadility of a Low Segregation Hf Free Supperalloy – DZ 125 /In: Superalloys-2000. 2000. P. 329–339.
  9. Chao Yuan, Fengshi Yin et al. Effect of Phosphorus on Microstructore and High Temperature Properties of a Cast Ni-base Supperalloy //J. Mater. Sci. Technol. 2002. V. 18. №6. P. 555–557.
  10. Zhuanggi H.V., Hongwei Song et al. Effect of Phosphorus on Microstructore and Creep Property of IN718b Superalloy //J. Mater. Sci. Technol. 2005. V. 21. P. 73–76.
  11. Kablov E.N., Petrushin N.V., Morozova G.I., Svetlov I.L. Fiziko-himicheskie faktory zharoprochnosti nikelevyh splavov, soderzhashhih renij [Physico-chemical factors of heat resisting nickel alloys containing rhenium] /V sb. Aviacionnye materialy i tehnologii. Vyp. «Vysokorenievye zharoprochnye splavy, tehnologii i oborudovanie dlja proizvodstva splavov i lit'ja monokristallicheskih turbinnyh lopatok GTD». M.: VIAM. 2004. S. 37–47.
  12. Kablov E.N., Svetlov I.L., Petrushin N.V. Nikelevye zharoprochnye splavy, legirovannye ruteniem [Nickel superalloys, ruthenium doped] /V sb. Aviacionnye materialy i tehnologii. Vyp. «Vysokorenievye zharoprochnye splavy, tehnologii i oborudovanie dlja proizvodstva splavov i lit'ja monokristallicheskih turbinnyh lopatok GTD». M.: VIAM. 2004. S. 80–90.
  13. Kablov E.N., Bondarenko Ju.A., Kablov D.E. Osobennosti struktury i zharoprochnyh svojstv monokristallov 001> vysokorenievogo nikelevogo zharoprochnogo splava, poluchennogo v uslovijah vysokogradientnoj napravlennoj kristallizacii [Structure and properties of single crystals of high-temperature 001> high-rhenium nickel superalloy prepared under the high-gradient directional crystallization] //Aviacionnye materialy i tehnologii. 2011. №4. S. 25–31.
  14. Kablov E.N., Bondarenko Ju.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [The development process of directional solidification of GTE blades with single crystal superalloys and composite structure] //Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
  15. Kablov E.N., Sidorov V.V. Mikrolegirovanie RZM – sovremennaja tehnologija povyshenija svojstv litejnyh zharoprochnyh nikelevyh splavov [Microalloying REM - modern technology enhancing properties of cast heat-resistant nickel alloys] //Perspektivnye materialy. 2001. №1. S. 23–24.
  16. Sidorov V.V., Timofeeva O.B., Kalicev V.A., Gorjunov A.V. Vlijanie mikrolegirovanija RZM na svojstva i strukturno-fazovye prevrashhenija v intermetallidnom splave VKNA-25-VI [Effect of microalloying REM on properties and structural phase transi-tions in the intermetallic alloy VKNA-25-VI] //Aviacionnye materialy i tehnologii. 2012. №4. S. 8–13.
  17. Harris G.K., Wahl J.B. Development in supperalloy castability and new applications for advanced supperalloys //Materials Science and Technology. 2009. V. 25. №2. P. 147–153.
  18. Gorjunov A.V., Sidorov V.V., Rigin V.E., Zajcev D.V. Formirovanie nanostrukturirovannogo sostojanija v litejnom zharoprochnom splave VZhM4-VI pri mikrolegirovanii ego lantanom [Formation of nanostructured state in casting superalloy VZHM4-VI in his microalloying lanthanum] //Aviacionnye materialy i tehnologii. 2013. №3. S. 39–43.
  19. Sidorov V.V., Goryunov A.V., Kolmakova N.A. Effect of lanthanum on the high-temperature strength of single-crystals of highly refractory alloy VZhM4-VI containing rhenium and ruthenium //Metal science and heat treatment. 2012. V. 54. №3–4. R. 126–130.
  20. Pang H.T., Edmonds I.M., Jones C.N., Stone H.J., Rae C.M. Effect of Y and La additions on the processing and properties of a second generation single crystal nickel-base supperalloy CMSX-4 /In: Supperalloys-2012: International symposium on supperalloys. 2012. P. 301–310.
  21. Sidorov V.V., Rigin V.E., Zajcev D.E., Gorjunov A.V. Formirovanie nanostrukturirovannogo sostojanija v litejnom zharoprochnom splave pri mikrolegirovanii ego lantanom [Formation of nanostructured state in casting superalloy with microalloying its lanthanum] //Trudy VIAM. 2013. №1. St. 01 (viam-works.ru).