Nerush S.V., Evgenov A.G. Research of fine-dispersed metal powder of the heat resisting alloy of the EP648-VI brand for laser metal deposition (LMD) and also the assessment quality of welding of powder material on the nickel basis on working blades THP // Proceedings of VIAM. 2014. No. 3. Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2014-0-3-1-1.

Research of fine-dispersed metal powder of the heat resisting alloy of the EP648-VI brand for laser metal deposition (LMD) and also the assessment quality of welding of powder material on the nickel basis on working blades THP

Nerush S.V., Evgenov A.G.
Abstract

Fine-dispersed metal powders of the heat resisting alloy brand EP648-VI for laser metal deposition (LMD), obtained by method of atomization at a facility HERMIGA 10/100 VI are investigated. It is shown, that the obtained fine-dispersed powders when spraying by cold and hot gas have low oxygen content, the spherical form, the expressed dendritic structure in all range of the granulometric distribution. Adaptive laser metal deposition with application metal powder of the heat resisting alloy EP648-VI of the granulometric distribution 40–80 microns on working off technology of recovery of geometry extreme combs on the bandage shelf of working blades of the second step guarantees high quality of welding material (availability of defects of typemicrocracks, lack of penetrations is not revealed).

Reference list
  1. Shmotin Ju.N., Starkov R.Ju., Danilov D.V., Ospennikova O.G., Lomberg B.S. Novye materialy dlja perspektivnogo dvigatelja OAO «NPO „Saturn”» [New materials for advanced engine JSC «NPO „Saturn”»] //Aviacionnye materialy i tehnologii. 2012. №2. S. 6–8.
  2. Kablov E.N., Petrushin N.V., Vasilenok L.B., Morozova G.I. Renij v zharoprochnyh nikelevyh splavah dlja lopatok gazovyh turbin (prodolzhenie) [Measurements in high-temperature nickel alloys for gas turbine blades (continued)] //Materialovedenie. 2000. №3. S. 38–43.
  3. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharoprochnye nikelevye splavy dlja detalej gazoturbinnyh dvigatelej [High-temperature heat-resistant nickel alloys for turbine engine parts] //Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
  4. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jele-menty – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of current and future high-tech] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  5. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Casting nickel superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–51.
  6. Nerush S.V., Evgenov A.G. Proizvodstvo poroshkov pripoev i gotovyh polufabrikatov na ih osnove, a takzhe poroshkov zharoprochnyh splavov i stalej dlja additivnyh tehnologij [Manufacture of solder powder and semi-finished on their basis, as well as powders heat-resistant alloys and steels for additive technologies] /V sb. dokl. nauch.-tehnich. kongressa po dvigatelestroeniju (NTKD-2012). 2012. S. 344–347.
  7. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  8. Lykov P.A., Safonov E.V., Bromer K.A., Shul'c A.O. Poluchenie metallicheskih mikroporoshkov gazodinamicheskim raspyleniem [Preparation of metal spray micropowders gasdynamic] //Vestnik Juzhno-Ural'skogo gosudarstvennogo universiteta. Ser. «Mashi-nostroenie». 2012. Vyp. 33. S. 107–112.
  9. Evgenov A.G., Nerush S.V. Tehnologija poluchenija poroshkov i polufabrikatov pripoev, issledovanie melkodispersnyh poroshkov pripoev dlja diffuzionnoj vakuumnoj pajki, poluchennyh metodom atomizacii rasplava [Technology for producing powders and semi solders study of fine powders of alloys, diffusion vacuum brazing, obtained by atomization of the melt] /V sb. materialov V Vserossijskoj nauchno-tehnicheskoj konferencii molodyh specialistov. Ufa: UMPO. 2011. S. 159–162.
  10. Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Gorjunov A.V. Sovremennye tehnologii poluchenija prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokolenija [Modern technologies for bar stock of casting superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 97−105.
  11. Lykov P.A., Bromer K.A., Roshhin V.E., Bryndin S.A. Opredelenie tehnologicheskih parametrov poluchenija metallicheskih ul'tradispersnyh poroshkov [Determination of process parameters for producing a metallic ultrafine powders] //Vestnik Juzhno-Ural'skogo gosudarstvennogo universiteta. Ser. «Metallurgija». 2011. Vyp. 14. S. 17–19.
  12. Kablov E.N., Evgenov A.G., Ryl'nikov V.S., Afanas'ev-Hodykin A.N. Issledovanie melkodispersnyh poroshkov pripoev dlja diffuzionnoj vakuumnoj pajki, poluchennyh metodom atomizacii rasplava [Investigation of fine powders of alloys, diffusion vacuum brazing, obtained by atomization of the melt] //Vestnik MGTU im. N.Je. Baumana. 2011. Spec. vyp. «Perspektivnye konstrukcionnye materialy i tehnologii». S. 79–87.
  13. Ospennikova O.G., Evgenov A.G., Nerush S.V., Afanas'ev-Hodykin A.N. Issledovanie melkodispersnyh poroshkov pripoev na nikelevoj osnove primenitel'no k polucheniju vysokotehnologichnogo polufabrikata v vide samoklejashhejsja lenty na organicheskom svjazujushhem [Investigation of fine solder powder nickel-based high-tech applied to obtain a semi-self-adhesive tape on the organic binder] //Vestnik UGATU. 2012. №5 (50). S. 137–144.
  14. Ospennikova O.G. Strategija razvitija zharoprochnyh splavov i stalej special'nogo naznachenija, zashhitnyh i tehnologicheskih pokrytij [The development strategy of superalloys and special steel, protective coatings and technological] //Aviacionnye materialy i tehnologii. 2012. №S. S. 19–35.
  15. Lykov P.A., Roshhin V.E., Vorob'ev E.I. Vlijanie tehnologicheskih parametrov raspylenija metallicheskih rasplavov na granulometricheskij sostav poroshka i formu chastic poroshka [Effect of process parameters on the melt spraying of metal powder particle size distribution and shape of the powder particles] //Izvestija vuzov. Ser. «Chernaja metallurgija». 2012. №6. S. 21–23.
  16. Bersenev A.G., Logunov A.V., Logacheva A.I. Problemy povyshenija kachestva zharoprochnyh splavov, poluchaemyh metodom metallurgii granul [Problems of improving the quality of high-temperature alloys, obtained by granule metallurgy] //Vestnik MAI. 2008. T. 15. №3. S. 83–89.
  17. Safronov V.P., Rytov N.N., Jeskin G.I., Solujanov Ju.F. Sovershenstvovanie tehnologii gazostrujnogo raspylenija rasplava [Improving technology gas-jet spray melt] /V sb. statej «Metallurgija granul». Vyp. 1. M.: VILS. 1983. S. 59–63.
  18. Anuchin P.S., Shherbakov A.I., Kalicev V.A. i dr. Osobennosti proizvodstva zharoprochnyh poroshkovyh pripoev [Features production of heat-resistant powder solders] /V sb. statej «Metallurgija granul». Vyp. 1. M.: VILS. 1983. S. 154–159.
  19. Anoshkin N.F., Hodkin V.I., Rytov N.N. Razrabotka i vnedrenie tehnologii proizvodstva granul vysokotemperaturnyh pripoev metodom strujnogo raspylenija dlja pajki detalej iz nikelevyh splavov [Development and implementation of high-temperature solder pellet production by spray jet soldering parts of nickel alloys] /V sb. statej «Metallurgija granul». Vyp. 1. M.: VILS. 1983. S. 127–134.