Grigoriev M.M., Khrulkov A.V., Gurevich Y.M., Panina N.N. Manufacture of fiberglass skins using vacuum infusion using epoksiangidrid resin and a semipermeable membrane // Proceedings of VIAM. 2014. No. 2. Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2014-0-2-4-4.
Manufacture of fiberglass skins using vacuum infusion using epoksiangidrid resin and a semipermeable membrane
Abstract
We consider a method of manufacturing a batch of fiberglass skins based on epoxy-anhydride resin by infusion using a semi-permeable membrane in a single molding cycle. Тhe results of investigations of properties.
Reference list
- Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of the development of materials and technologies of their processing for the period until 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Grashhenkov D.V., Chursova L.V. Strategija razvitija kompozicionnyh i funkcional'nyh materialov [Strategy of development of composite and functional materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
- Kogan D.I., Chursova L.V., Petrova A.P. Polimernye kompozicionnye materialy, poluchennye putem propitki plenochnym svjazujushhim [The polymeric composite materials received by impregnation by the film binding] //Kompozicionnye materialy. 2011. №11. S. 2–6.
- Veshkin E.A., Postnov V.I., Abramov P.A. Puti povyshenija kachestva detalej iz PKM pri vakuumnom formovanii [Ways of improvement of quality of details from PKM at vacuum formation] //Izvestija Samarskogo nauchnogo centra RAN. 2012. T. 14. №4 (3). S. 831–838.
- Minakov V.T., Postnov V.I., Hpul'kov A.V., Postnov A.V., Pletin' I.I. Osobennosti skleivanija detalej iz PKM s ispol'zovaniem polimepnoj osnastki [Features of pasting of details from PKM with use of polymeric equipment] //Klei. Germetiki. Tehnologii. 2008. №5. S. 24–29.
- Muhametov P.P., Ahmadieva K.R., Chursova L.B., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of production of constructional fibrous PKM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
- Mihajlin Ju.A. Konstrukcionnye polimernye kompozicionnye materialy [Constructional polymeric composite materials]. SPb.: NOT. 2008. 820 s.
- Kerber M.L., Vinogradov V.M. Polimernye kompozicionnye materialy: struktura, svojstva, tehnologija [Polymeric composite materials: structure, properties, technology]. SPb.: Professija. 2009. 560 s.
- Alent'ev A.Ju., Jablokova M.Ju. Svjazujushhie dlja polimernyh kompozicionnyh materialov [Binding for polymeric composite materials]: Ucheb. posob. M.: MGU im. M.V. Lomonosova. 2010. 69 s.
- Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svjazujushhie dlja perspektivnyh metodov izgotovlenija PKM novogo pokolenija [Rasplavny binding for perspective methods of production of PKM of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
- Himicheskaja promyshlennost': Obzornaja informacija. Ser. «Jepoksidnye smoly i materialy na ih osnove». «Otverditeli dlja jepoksidnyh smol» [Chemical industry: Survey information. It is gray. "Epoxies and materials on their basis". "Hardeners for epoxies"]. M.: NIITJeHIM. 1983. 39 s.
- Bulanov I.M., Vorobej V.V. Tehnologija raketnyh i ajerokosmicheskih konstrukcij iz kompozicionnyh materialov [Technology of rocket and space designs from composite materials]. M.: MGTU im. N.Je. Baumana. 1998. 513 s.
- Kryzhanovskij V.K. Proizvodstvo izdelij iz polimernyh materialov [Production of products from polymeric materials]. SPb.: Professija. 2008. 460 s.
- Chursova L.V., Dushin M.I., Kogan D.I., Panina N.N., Kim M.A., Gurevich Ja.M., Platonov A.A. Plenochnye svjazujushhie dlja RFI-tehnologii [Film binding for RFI technology] //Rossijskij himicheskij zhurnal. 2010. T. LΙV. Vyp. «Materialy dlja aviakosmicheskoj tehniki». S. 63–67.
- Kogan D.I. Tehnologija izgotovlenija polimernyh kompozicionnyh materialov sposobom propitki plenochnym svjazujushhim [Manufacturing techniques of polymeric composite materials in the way of impregnation by the film binding]: Avtoref. dis. k.t.n. M.: VIAM. 2011. 26 s.
- Afanas'ev D.V., Oshhepkov M.Ju. Bezavtoklavnye tehnologii [Non-autoclave technologies] //Kompozitnyj mir. 2010. №9–10. S. 28–37.
- Hrul'kov A.V., Dushin M.I., Popov Ju.O., Kogan D.I. Issledovanija i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovanija PKM [Researches and development autoclave and non-autoclave technologies of formation of PKM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
- Dushin M.I., Hrul'kov A.V., Muhametov P.P. Vybor tehnologicheskih parametrov avtoklavnogo formovanija detalej iz polimernyh kompozicionnyh materialov [Choice of technological parameters of autoclave formation of details from polymeric composite materials] //Aviacionnye materialy i tehnologii. 2011. №3. S. 20–26.
- GOST 15139–69. Plastmassy. Metody opredelenija plotnosti (obꞌemnoj massy) [GOST 15139-69. Plastic. Methods of determination of density (volume weight)].