Babashov V.G., Ivakhnenko Yu.A., Yudin A.V., Zimichev A.M. Ceramic material for parts of continuous casting units intended for production of non-ferrous alloys // Proceedings of VIAM. 2014. No. 12. Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2014-0-12-5-5.

Ceramic material for parts of continuous casting units intended for production of non-ferrous alloys

Babashov V.G., Ivakhnenko Yu.A., Yudin A.V., Zimichev A.M.
Abstract

The problem of creation of domestic materials to replace imported wear-subjected parts of units for continuous casting of non-ferrous metals and alloys has been solved. Properties of this heat insulating ceramic material based on silica and quartz fibers produced by vacuum molding compare favourable with Wollaston fibers used abroad.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N., Grashhenkov D.V., Isaeva N.V. i dr. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Promising high-temperature ceramic composite materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.
  3. Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Aljuminievye deformiruemye splavy [Aluminium wrought alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
  4. Ivahnenko Ju.A., Babashov V.G., Zimichev A.M., Tinjakova E.V. Vysokotemperaturnye teploizoljacionnye i teplozashhitnye materialy na osnove volokon tugoplavkih soedinenij [High-temperature insulating and heat-proof materials for fiber-based refractory compounds] //Aviacionnye materialy i tehnologii. 2012. №S. S. 380–385.
  5. Kablov E.N., Shhetanov B.V., Ivahnenko Ju.A., Balinova Ju.A. Perspektivnye armirujushhie vysokotemperaturnye volokna dlja metallicheskih i keramicheskih kompozicionnyh materialov [Prospective reinforcing fibers for high temperature ceramic composites and metal materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru).
  6. Shhetanov B.V., Balinova Ju.A., Ljuljukina G.Ju., Solov'eva E.P. Struktura i svojstva nepreryvnyh polikristallicheskih volokon α-Al2O3 [Structure and properties of continuous fibers of polycrystalline α-Al2O3] //Aviacionnye materialy i tehnologii. 2012. №1. S. 13–17.
  7. Grashhenkov D.V., Shhetanov B.V., Tinjakova E.V., Shheglova T.M. O vozmozhnosti ispol'zovanija kvarcevogo volokna v kachestve svjazujushhego pri poluchenii legkovesnogo teplozashhitnogo materiala na osnove volokon Al2O3 [The possibility of using a silica fiber as a binder in the preparation of a lightweight heat-fiber-based material Al2O3] //Aviacionnye materialy i tehnologii. 2011. №4. S. 8–14.
  8. Grashhenkov D.V., Balinova Ju.A., Tinjakova E.V. Keramicheskie volokna oksida aljuminija i materialy na ih osnove [Ceramic alumina fibers and materials based on them] //Steklo i keramika. 2012. №4. S. 32–36.
  9. Shhetanov B.V., Ivahnenko Ju.A., Babashov V.G. Teplozashhitnye materialy [Heat-proof materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 12‒19.
  10. Alekseenko A.A., Bajbekova E.V., Kuznecov S.N. i dr. Issledovanie problemy zatjagivanija stakanov pri razlivke na sortovoj MNLZ malouglerodistoj nizkokremnistoj stali, raskislennoj aljuminiem [Study of the problem tightening glasses when casting on the CCM low-siliceous mild steel, aluminum killed] //Jelektrometallurgija. 2007. №3. S. 4–18.
  11. Sposob poluchenija voloknistogo keramicheskogo materiala [A method for producing a ceramic fiber material]: pat. 2358954 Ros. Federacija; opubl. 20.06.2009.
  12. Kolyshev S.G., Basargin O.V., Butakov V.V. Jeksperimenty po opredeleniju prochnosti pri rastjazhenii obrazcov iz legkovesnyh gibkih voloknistyh materialov [Experiments to determine the tensile strength of the samples of lightweight fibrous materials floppy] //Vse materialy. Jenciklopedicheskij spravochnik. 2014. №5. S. 8‒11.
  13. Basargin O.V., Shheglova T.M., Kolyshev S.G. Opredelenie vysokotemperaturnyh prochnostnyh harakteristik materialov iz oksidnoj keramiki [Determination of high-temperature strength characteristics of the ceramic oxide material] //Steklo i keramika. 2013. №2. S. 6‒9.
  14. Lugovoj A.A., Babashov V.G., Karpov Ju.V. Temperaturoprovodnost' gradientnogo teploizoljacionnogo materiala [The thermal diffusivity of the gradient insulating material] //Trudy VIAM. 2014. №2. St. 02 (viam-works.ru).