Bakradze M.M., Ovsepyan S.V., Shugaev S.A., Letnikov M.N. The influence of quenching on structure and properties nickel-based superalloy EK151-ID FORGINGS // Proceedings of VIAM. 2013. No. 9. Ст. 01. URL: https://www.viam-works.ru.

The influence of quenching on structure and properties nickel-based superalloy EK151-ID FORGINGS

Bakradze M.M., Ovsepyan S.V., Shugaev S.A., Letnikov M.N.
Abstract

The influence of quenching on structure and properties of high-alloy nickel-based superalloy EK151-ID was investigated. The statistical data of commercial EK151-ID superalloy small-sized GTE disc’s forgings under condition on FSUE «VIAM» was analyzed in this paper. The optimal heat treatment leads to increase of mechanical properties of this alloy was determined.