Lukina N.F., Petrova A.P. Adhesives in shuttle structure // Proceedings of VIAM. 2013. No. 4. Ст. 05. URL: https://www.viam-works.ru.

Adhesives in shuttle structure

Lukina N.F., Petrova A.P.
Abstract

A list of the adhesive materials used in the shuttle «Buran» structure, as well as their basic physicomechanical properties and ways of application are presented. Purposes for the mentioned materials are presented.