Babin A.N. Resin system for new generation of polymer composite materials // Proceedings of VIAM. 2013. No. 4. Ст. 12. URL: https://www.viam-works.ru.

Resin system for new generation of polymer composite materials

Babin A.N.
Abstract

New composite materials are interesting for creation of new resin systems with special properties and application spheres, with different technology processings. The ecological and energy-effective technologies for production of materials are of great importance. Resin systems are created for wide classes of polymer systems, with complete estimation of resin systems and end products.