Kablov E.N., Gerasimov V. V., Visik E.M., Demonis I.M. Role of the directed solidification in the resource-saving production technologies of details of GTD // Proceedings of VIAM. 2013. No. 3. Ст. 01. URL: https://www.viam-works.ru.

Role of the directed solidification in the resource-saving production technologies of details of GTD

Kablov E.N., Gerasimov V. V., Visik E.M., Demonis I.M.
Abstract

The role of the directed of solidification heat resisting alloys as effective process in resource-saving technology is shown by production of small-sized disks of turbines; in-troduction in production of intermetallic alloys like VKNA with single-crystal structure; development of high-rhenium heat resisting alloys when molding single-crystal shovels of turbines.