Beider E.Ya., Petrova G.N., Izotova T.F., Gureeva E.V. Thermoplastic composite materials and penopolyimids // Proceedings of VIAM. 2013. No. 11. Ст. 01. URL: https://www.viam-works.ru.

Thermoplastic composite materials and penopolyimids

Beider E.Ya., Petrova G.N., Izotova T.F., Gureeva E.V.
Abstract

In the article the mechanical properties of composite glass, carbon and organic plastics based on thermoplastic binders are given (CTM). The methods of manufacturing details from CTM by hot pressing, stamping, bending and welding are described. Properties of the developed flexible and rigid foams are considered.

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologiy ih pererabotki na period do 2030 goda [Strategic directions of the development of materials and technologies of their processing for the period until 2030] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Graschenkov D.V., Chursova L.V. Strategiya razvitiya kompozitsionnyh i funktsional'nyh materialov [Development strategy of composite and functional materials] //Aviatsionnye materialy i tehnologii. 2012. №S. S. 231–242.
  3. Petrova G.N., Barbot'ko S.L., Bolotina L.M., Chebotarev V.P. i dr. Pozharobezopasnye svoystva polisul'fonov [Fire-safe properties of polysulfones] //Plasticheskie massy. 2005. №1. S. 46–48.
  4. Petrova G.N., Beyder E.Ya. Konstruktsionnye materialy na osnove armirovannyh termoplastov [Structural materials based on reinforced thermoplastics] //Rossiyskiy himicheskiy zhurnal. 2010. T. LІV. №1. S. 30–40.
  5. Muhametov R.R., Ahmadieva K.R. i dr. Novye polimernye svyazuyuschie dlya perspektivnyh metodov izgotovleniya konstruktsionnyh voloknistyh PKM [Novel polymer binders for advanced production methods of structural fibrous polymer composites] //Aviatsionnye materialy i tehnologii. 2011. №2. S. 38–42.
  6. Beyder E.Ya., Petrova G.N., Izotova T.F., Barbot'ko S.L. Stekloplastiki na termoplastichnoy matritse [Thermoplastic-matrix fiber-glass plastics] //Trudy VIAM. 2013. №7. (elektronnyj zhurnal).
  7. Petrova G.N. Napravlennaya modifikatsiya polisul'fonov i sozdanie na ih osnove lit'evyh i kompozitsionnyh materialov [Directed modification of polysulfones and creation of molding and composite materials on their basis]: Avtoref. dis. k.t.n. M.: VIAM. 2011. S. 10–27.
  8. Komarov G.A. Sostoyanie, perspektivy i problemy primeneniya PKM v tehnike [Use of PCM in engineering. Current state, aspects and concerns] //Polimernye materialy. 2009. №2. S. 5–9.
  9. Petrova G.N., Beider E.Ya. Construction materials based on reinforced thermoplastics Chemistry and Materials Science [Construction materials based on reinforced thermo-plastics Chemistry and Materials Science] //Russian Journal of General Chemistry. 2011. V. 81. №5. P. 1001–1007.
  10. Kerber M.L., Vinogradov V.M., Golovkin G.S. i dr. Polimernye kompozitsionnye materialy: struktura, svoystva, tehnologiya [Polymer composite materials: structure, properties, technology]. SPb.: Professiya. 2011. S. 32–33
  11. Petrova G.N., Beyder E.Ya., Chebotarev V.P. i dr. Regulirovanie svoystv polisul'fonov za schet modifikatsii [Polysulfones properties control through modification] //Plasticheskie massy. 2010. №12. S. 23–27.
  12. Donetskiy K.I., Hrul'kov A.V. i dr. Primenenie obemno-armiruyuschih preform dlya izgotovleniya izdeliy iz PKM [Usage of Three-Dimensional Reinforcing Preforms for Production of Polymer Composite Articles] //Aviatsionnye materialy i tehnologii. 2013. №1. S. 35–39.
  13. Komarov G.V. Soedinenie detaley iz polimernyh materialov [Assembly of parts made of polymer materials]: Ucheb. posob. SPb.: Professiya. 2006. S. 337–443.
  14. Mihaylin Yu.A. Termoustoychivye polimery i polimernye materialy [Thermally stable polymers and polymer materials]. SPb.: Professiya. 2006. S. 240–347.
  15. Beyder E.Ya., Gureeva E.V., Petrova G.N. Penopoliimidy [Foamed polyimides] //Vse materialy. Entsiklopedicheskiy spravochnik. 2012. №6. S. 2–8.