Ospennikova O.G., Naprienko S.A., Medvedev P.N., Krupnina O.A., Rogalev A.M. Features of the structure of Ti–6Al–4V alloy obtained by selective laser melting // Proceedings of VIAM. 2019. No. 10 (82). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2019-0-10-14-24.

Features of the structure of Ti–6Al–4V alloy obtained by selective laser melting

Ospennikova O.G., Naprienko S.A., Medvedev P.N., Krupnina O.A., Rogalev A.M.
Abstract

The paper analyzes the structural features of titanium alloy Ti–6Al–4V, obtained by selective laser melting (SLM). By methods of optical and scanning electron microscopy and x-ray diffraction analysis the characteristics of the structural and texture state of the material obtained in the synthesis are revealed. The study of defects characteristic of the titanium alloy obtained by this technology using scanning electron microscopy, x-ray spectral analysis and x-ray tomography was carried out.

Keywords
selective laser melting (SLM), titanium alloy Ti–6Al–4V, structural features, defect, x-ray tomography.
Reference list
  1. Lukina E.A., Filonova E.V., Treninkov I.A. Mikrostruktura i preimushhestvennye kristallograficheskie orientirovki zharoprochnogo nikelevogo splava, sintezirovannogo metodom SLS, v zavisimosti ot energeticheskogo vozdejstviya i termoobrabotki [The microstructure and preferential crystallographic orientation of nickel superalloy, synthesized by SLM method, depending of the energy impact and heat treatment] // Aviacionnye materialy i tehnologii. 2017. №1 (46). S. 38–44. DOI: 10.18577/2071-9140-2017-0-1-38-44.
  2. Kablov E.N., Evgenov A.G., Mazalov I.S., Shurtakov S.V., Zaytsev D.V., Prager S.M. Evolyutsiya struktury i svoystv vysokokhromistogo zharoprochnogo splava VZh159, poluchennogo metodom selektivnogo lazernogo splavleniya. Ch. I [The evolution of the structure and properties of the high-chromium heat-resistant alloy VZh159, obtained by selective laser fusion. Part I] // Materialovedeniye. 2019. №3. S. 9–17.
  3. Kablov E.N., Evgenov A.G., Mazalov I.S., Shurtakov S.V., Zaytsev D.V., Prager S.M. Evolyutsiya struktury i svoystv vysokokhromistogo zharoprochnogo splava VZh159, poluchennogo metodom selektivnogo lazernogo splavleniya. Ch. II [The evolution of the structure and properties of the high-chromium heat-resistant alloy VZh159, obtained by selective laser fusion. Part II] // Materialovedeniye. 2019. №4. S. 9–15.
  4. Evgenov A.G., Gorbovec M.A., Prager S.M. Struktura i mehanicheskie svojstva zharoprochnyh splavov VZh159 i EP648, poluchennyh metodom selektivnogo lazernogo splavleniya [Structure and mechanical properties of heat resistant alloys VZh159 and EP648, prepared by selective laser fusing] // Aviacionnye materialy i tehnologii. 2016. №S1. S. 8–15. DOI: 10.18577/2071-9140-2016-0-S1-8-15.
  5. Dynin N.V., Zavodov A.V., Oglodkov M.S., Khasikov D.V. Vliyaniye parametrov protsessa selektivnogo lazernogo splavleniya na strukturu alyuminiyevogo splava sistemy Al–Si–Mg [ The influence of process parameters of selective laser melting on the structure of aluminum alloy Al–Si–Mg system] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №10 (58). St. 01. Available at: http://www.viam-works.ru (accessed: June 20, 2019). DOI: 10.18577/2307-6046-2017-0-10-1-1.
  6. Ryabov D.K., Antipov V.V., Korolev V.A., Medvedev P.N. Vliyanie tehnologicheskih faktorov na strukturu i svojstva silumina, poluchennogo s ispolzovaniem tehnologii selektivnogo lazernogo sinteza [Effect of technological factors on structure and properties of Al–Si alloy obtained by selective laser melting] // Aviacionnye materialy i tehnologii. 2016. №S1. S. 44–51. DOI: 10.18577/2071-9140-2016-0-S1-44-51.
  7. Bogachev I.A., Sulyanova E.A., Sukhov D.I., Mazalov P.B. Issledovaniye mikrostruktury i svoystv korrozionnostoykoy stali sistemy Fe–Cr–Ni, poluchennoy metodom selektivnogo lazernogo splavleniya [ Microstructure and properties investigations of Fe–Cr–Ni stainless steel obtained by selective laser melting] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2019. №3 (75). St. 01. Available at: http://www.viam-works.ru (accessed: June 26, 2019). DOI: 10.18577/2307-6046-2019-0-3-3-13.
  8. Aloshin N.P., Murashov V.V., Evgenov A.G., Grigorev M.V., Shchipakov N.A., Vasilenko S.A., Krasnov I.S. Klassifikatsiya defektov metallicheskikh materialov, sintezirovannykh metodom selektivnogo lazernogo splavleniya, i vozmozhnosti metodov nerazrushayushchego kontrolya dlya ikh obnaruzheniya [Classification of defects in metallic materials synthesized by selective laser fusion, and the possibility of non-destructive testing methods for their detection] // Defektoskopiya. 2016. №1. S. 48–55.
  9. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  10. Dzunovich D.A., Alekseyev E.B., Panin P.V., Lukina E.A., Novak A.V. Struktura i svoystva listovykh polufabrikatov iz deformiruyemykh intermetallidnykh titanovykh splavov raznykh klassov [Structure and properties of sheet semi-finished products from various wrought intermetallic titanium alloys] // Aviacionnye materialy i tehnologii. 2018. №2 (51). S. 17–25. DOI: 10.18577/2071-9140-2018-0-2-17-25.
  11. Nochovnaya N.A. Issledovaniye vliyaniya parametrov izotermicheskoy deformatsii i termicheskoy obrabotki na strukturu i mekhanicheskiye svoystva shtampovki iz splava VT6ch. [Research of the influence of parameters of isothermal deformation and heat treatment on structure and mechanical properties punchings from alloy VT6ch] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2017. №10 (58). St. 03. Available at: http://www.viam-works.ru (accessed: July 10, 2019). DOI: 10.18577/2071-9140-2017-0-10-3-3.
  12. Antonysamy A.A., Meyer J., Prangnell P.B. Effect of build geometry on the b-grain structure and texture in additive manufacture of Ti/6Al/4V by selective electron beam melting // Materials characterization. 2013. Vol. 84. P. 153–168.
  13. Carter L.N., Martin C., Withers P.J., Attallah M.M. The influence of the laser scan strategy on grain structure and cracking behaviour in SLM powder-bed fabricated nickel superalloy // Journal of Alloys and Compounds. 2014. Vol. 615. P. 338–347.
  14. Cao L., Wan Y., Yang S., Pu J. The Tribocorrosion and Corrosion Properties of Thermally Oxidized Ti6Al4V Alloy in 0.9 wt. % NaCl Physiological Saline // Coatings. 2018. No. 8. P. 285. DOI: 10.3390/coatings8080285.
  15. Voronin N.V., Kutlubayev R.G., Mikhaylov E.A., Astanin V.V., Kayumova E.Z. Vliyaniye gazonasyshchennogo sloya na parametry akusticheskoy emissii pri nagruzhenii titanovogo splava VT1-0 [The effect of a gas-saturated layer on the parameters of acoustic emission during loading of a VT1-0 titanium alloy] // Ekspertiza promyshlennoy bezopasnosti i diagnostika opasnykh proizvodstvennykh obektov. 2015. №5. S. 165–167.
  16. Davydov S.I., Ovchinnikov A.V., Shvartsman L.Ya. i dr. Sovershenstvovaniye protsessa polucheniya titanovykh splavov putem razrabotki tekhnologii proizvodstva titana gubchatogo s zadannym soderzhaniyem kisloroda [Improving the process for producing titanium alloys by developing a technology for the production of sponge titanium with a given oxygen content] // Titan. 2011. №4 (34). S. 21–27.
  17. Diagrammy sostoyaniya dvoynykh metallicheskikh sistem: spravochnik v 3 t. / pod obshch. red. N.P. Lyakisheva [Diagrams of the state of double metal systems: a reference book in 3 vol. / gen. ed. N.P. Lyakishev]. M.: Mashinostroyeniye, 2001. T. 3, kn. I. 872 s.