The influence of heating technology on the duration of the curing process of polymer composite materials

Malysheva G.V., Guzeva T.A., Grachshencov D.V., Raskutin A.E.
Abstract

The results of experimental studies of the properties of organoplastics made using wet-wound technology using an epoxy binder are presented. Curing was carried out in two different ways: in the electric and microwave stoves when using two modes of increasing the temperature at a given value (single-stage and three-stage). It is shown that the use of microwave heating allows not only to significantly shorten the curing time, but also leads to an increase in the modulus of elasticity. Values of shrinkage, porosity and size of their standard deviation are given, itis experimentally established that use of microwave heating leads to increase in standard deviation.

Keywords
polymer composite materials, organoplastics, curing technology, microwave heating.
Reference list
  1. Kablov E.N., Chursova L.V., Lukina N.F., Kutsevich K.E., Rubtsova E.V., Petrova A.P. Issledovanie epoksidno-polisulfonovykh polimernykh sistem kak osnovy vysokoprochnykh kleev aviatsionnogo naznacheniya [Research of epoxy and polysulfonic polymeric systems as bases of high-strength adhesives of aviation assignment] // Klei. Germetiki. Tekhnologii. 2017. №3. S. 7–12.
  2. Raskutin A.E. Rossiiskie polimernye kompozitsionnye materialy novogo pokoleniia, ikh osvoenie i vnedrenie v perspektivnykh razrabatyvaemykh konstruktsiiakh [Russian polymer composite materials of new generation, their exploitation and implementation in advanced developed constructions] // Aviacionnye materialy i tehnologii. 2017. №S. S. 349–367. DOI: 10.18577/2071-9140-2017-0-S-349-367.
  3. Kablov E.N., Buznik V.M. Sostoyanie i perspektivy arkticheskogo materialovedeniya [Condition and perspectives of the Arctic materials science] // Vestnik Rossijskoj akademii nauk. 2017. T. 87. №9. S. 827–839.
  4. Grashchenkov D.V. Strategiya razvitiya nemetallicheskih materialov, metallicheskih kompozicionnyh materialov i teplozashhity [Strategy of development of non-metallic materials, metal composite materials and heat-shielding] // Aviacionnye materialy i tehnologii. 2017. №S. S. 264–271. DOI: 10.18577/2071-9140-2017-0-S-264-271.
  5. Bazhenov S.L., Berlin A.A., Kulkov A.A., Oshmyan V.G. Polimernye kompozitsionnye materialy [Polymeric composite materials]. Dolgoprudnyj: Intellekt, 2010. 352 s.
  6. Petrova A.P., Malysheva G.V. Klei, kleevye svyazuyushchie, kleevye prepregi / pod obshch. red. E.N. Kablova [Glues, glue binding, glue prepregs / gen. ed. by E.N. Kablov]. M.: VIAM, 2017. 472 s.
  7. Baurova N.I., Zorin V.A. Primenenie polimernykh kompozitsionnykh materialov pri proizvodstve i remonte mashin: ucheb. posobie [Application of polymeric composite materials by production and repair of machines: manual]. M.: MADI, 2016. 264 s.
  8. Mikhajlin Yu.A. Voloknistye polimernye kompozitsionnye materialy v tekhnike [Fibrous polymeric composite materials in equipment]. SPb.: Nauchnye osnovy i tekhnologii, 2013. 720 s.
  9. Komkov M.A., Tarasov V.A. Tekhnologiya namotki kompozitnykh konstruktsij raket i sredstv porazheniya [Technology of winding of composite designs of rockets and means of defeat]. M.: Izd-vo MGTU im. N.E. Baumana, 2011. 431 s.
  10. Mishkin S.I., Raskutin A.E., Evdokimov A.A., Gulyaev I.N. Tekhnologii i osnovnye etapy stroitelstva pervogo v Rossii arochnogo mosta iz kompozitsionnykh materialov [Technologies and the main stages of construction of the arch bridge first in Russia from composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №6 (54). St. 05. Available at: http://www.viam-works.ru (accessed: July 12, 2018). DOI: 10.18577/2307-6046-2017-0-6-5-5.
  11. Guzeva T.A. Novye podkhody k povysheniyu effektivnosti proizvodstva detalej iz organoplastikov [New approaches to increase of production efficiency of details from organ plastics] // Vse materialy. Entsiklopedicheskij spravochnik. 2012. №7. S. 53–56.