Kirichok P.F. Corrosion cracking of aluminum alloys and stainless steels: key features and test methods (review) // Proceedings of VIAM. 2018. No. 7 (67). Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-7-106-116.

Corrosion cracking of aluminum alloys and stainless steels: key features and test methods (review)

Kirichok P.F.
Abstract

Aggressive environments that lead to the occurrence of corrosion lesions of structures lead to significant changes in their mechanical characteristics and lead to a significant reduction in their bearing capacity and a decrease in durability. The danger of aggressive media exposure to highly loaded material is also due to the fact that in some cases the structural elements fail in a very short time, including with an emergency outcome. In the present work, the literature data, normative documentation and studies on the stress-corrosion cracking and loading methods of the test samples during the tests are analyzed. Particular attention is paid to tests with constant deformation, as the most common and least expensive test group and testing of samples under constant load. Recommendations are given on the timing of testing for stress-corrosion cracking of various metals and alloys.

Keywords
corrosion cracking, corrosion, aluminum alloys, stainless steels, test methods, hydrogen embrittlement.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  3. Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
  4. Kablov E.N. Aviatsionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and perspectives] // Vestnik Rossijskoj akademii nauk. 2002. T. 72. №1. S. 3–12.
  5. Kablov E.N. Aviatsionnoe materialovedenie v XXI veke. Perspektivy i zadachi [Aviation materials science in the XXI century. Perspectives and tasks] // Aviacionnye materialy. Izbrannye trudy VIAM 1932–2002. M.: MISIS–VIAM, 2002. S. 23–47.
  6. Kablov E.N., Startsev O.V., Medvedev I.M., Panin S.V. Korrozionnaya agressivnost' primorskoj atmosfery. Ch. 1. Faktory vliyaniya (obzor) [Corrosion aggression of the seaside atmosphere. P.1. Factors of influence (overview)] // Korroziya: materialy, zashchita. 2013. №12. S. 6–18.
  7. Kurs M.G., Kutyrev A.E., Fomina M.A. Issledovanie korrozionnogo razrusheniya deformiruemyh alyuminievyh splavov pri laboratornyh i naturnyh ispytaniyah [Research of corrosion damage of wrought aluminium alloys at laboratory and full-scale tests] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №8 (44). St. 10. Available at: http://www.viam-works.ru (accessed: May 3, 2018). DOI: 10.18577/2307-6046-2016-0-8-10-10.
  8. Kurs M.G., Laptev A.B., Kutyrev A.E., Morozova L.V. Issledovanie korrozionnogo razrusheniya deformiruemykh alyuminievykh splavov pri naturno-uskorennykh ispytaniyakh. Chast 1 [Study of corrosion destruction of deformable aluminum alloys at full-scale accelerated tests. Part 1] // Voprosy materialovedeniya. 2016. №1 (85). S. 116–127.URL: http://www.crism-prometey.ru (data obrashcheniya: 03.05.2018).
  9. Grinevich A.V., Lutsenko A.N., Karimova S.A. Raschetnye harakteristiki metallicheskih materialov s uchetom vlazhnosti [The design characteristic of metallic materials taking into account the humidity] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №7. St. 10. Available at: http://www.viam-works.ru (accessed: May 3, 2018). DOI: 10.18577/2307-6046-2014-0-7-10-10.
  10. Sinyavskij S.V. Soprotivlenie titanovykh splavov razlichnym vidam korrozionnogo rastreskivaniya [Resistance of titanium alloys to various types of corrosion cracking] // Tekhnologiya legkikh splavov. 2010. №4. S. 80–85.
  11. Ovchinnikov I.I. Issledovanie povedeniya obolochechnykh konstruktsij, ekspluatiruyushchikhsya v sredakh, vyzyvayushchikh korrozionnoe rastreskivanie [Investigation of the behavior of shell structures operating in environments causing corrosion cracking] // Naukovedenie: internet-zhurnal. 2012. №4 (13). S. 1–11. Available at: http://www.naukovedenie.ru(data obrashcheniya: 03.05.2018).
  12. Gerasimov V.V., Gerasimova V.V. Korrozionnoe rastreskivanie austenitnykh nerzhaveyushchikh stalej [Corrosion cracking of austenitic stainless steels]. M.: Metallurgiya, 1976. 176 s.
  13. Korchagin A.P. O vliyanii vodoroda na predel tekuchesti stali [On the effect of hydrogen on the yield strength of steel] // Izvestiya AN SSSR. Ser.: Metally. 1973. №5. S. 202–203.
  14. Krivonogov G.S., Kablov E.N. Rol granits zeren v okhrupchivanii vysokoprochnykh korrozionnostojkikh stalej [The role of grain boundaries in embrittlement of high-strength corrosion-resistant steels] // Metally. 2002. №1. S. 35–41.
  15. Kablov E.N., Krivonogov G.S. Effect of hydrogen on reliability of high-strength corrosion-resistant steels // Russian metallurgy (Metally). 2002. No. 1. P. 42–51.
  16. Romanov V.V. Korrozionnoe rastreskivanie metallov [Corrosion cracking of metals]. M.: Mashgiz, 1960. S. 166–169.
  17. Koch G.H. Tests for Stress-Corrosion Cracking // Advanced Materials & Processes. August, 2001. Available at: http://www.asminternational.org (accessed: May 3, 2018).
  18. Zakharova L.V. Vliyanie khimicheskogo sostava, termicheskoj obrabotki i struktury na stojkost' titanovykh splavov k rastreskivaniyu ot goryachesolevoj korrozii [Influence of chemical composition, thermal treatment and structure on cracking sensitivity of titanium alloys to hot-salt stress corrosion] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №9 (45). St. 11. Available at: http://www.viam-works.ru (accessed: May 3, 2018). DOI: 10.18577/2307-6046-2016-0-9-11-11.
  19. Zakharova L.V. Vliyanie kisloroda vozdukha i tolshchiny solevykh otlozheniy na korrozionnoe rastreskivanie titanovykh splavov pri vysokikh temperaturakh v kontakte s NaCl [Influence of oxygen of air and thickness of salt deposits on corrosion cracking of titanium alloys at high temperatures in contact with NaCl] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №10. St. 12. Available at: http://www.viam-works.ru (accessed: May 3, 2018). DOI: 10.18577/2307-6046-2014-0-10-12-12.