Lomberg B.S., Moiseev N.V., Letnikov M.N., Korotkiy A.V. The influence of annealing temperature in original pre-deformation round bars on structure and mechanical properties of forgings made of EP742-ID alloy // Proceedings of VIAM. 2018. No. 5 (65). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-5-12-17.

The influence of annealing temperature in original pre-deformation round bars on structure and mechanical properties of forgings made of EP742-ID alloy

Lomberg B.S., Moiseev N.V., Letnikov M.N., Korotkiy A.V.
Abstract

Now to low-dimensional gas turbine engines (GTE) widely apply disks made in FSUE «VIAM» from heat resisting deformable alloy EP742-ID. Initial preparations of punchings of disks for low-dimensional GTE are the press bars with a diameter of 140–150 mm made by method of extrusion from ingots with a diameter of 320 mm of double vacuum smelting (VI+VDP). Recrystallization of original compacted round bars made of EP742-ID alloy, used as a blank to the isothermal forging process of small-sized disks for gas-turbine engine, has been researched. Influence of recrystallization annealing in a single-phase area on mechanical properties of forgings material after finish heat treatment has been determine in the article. The conclusion is in summary drawn that carrying out annealing before deformation at temperature on 15–25°C above Тп.рγʹ allows to increase stability of plastic properties (δ, ψ, KCU) punchings from alloy EP742-ID, and also it is essential to reduce number of re-testing and repeat

Keywords
recrystallization, recrystallization annealing, microstructure, mechanical properties.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  3. Kablov E.N. Materialy novogo pokoleniya – osnova innovacij, tekhnologicheskogo liderstva i nacionalnoj bezopasnosti Rossii [Materials of new generation – basis of innovations, technological leadership and national security of Russia] // Intellekt & Tekhnologii. 2016. №2 (14). S. 41–46.
  4. Ospennikova O.G. Strategiya razvitiya zharoprochnyh splavov i stalej specialnogo naznacheniya, zashhitnyh i teplozashhitnyh pokrytij [Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings] // Aviacionnye materialy i tehnologii. 2012. №S. S. 19–36.
  5. Novikov I.I. Teoriya termicheskoj obrabotki metallov [Theory of thermal processing of metals]. M.: Metallurgiya, 1986. 480 s.
  6. Kolachev B.A., Gabidullin R.M. Tekhnologiya termicheskoj obrabotki cvetnykh metallov i splavov. 2-e izd. [Technology of thermal processing of non-ferrous metals and alloys. 2nd ed.]. M.: Metallurgiya, 1992. 272 s.
  7. Gorelik S.S. Rekristallizaciya metallov i splavov [Recrystallizing of metals and alloys]. M.: Metallurgiya, 1978. S. 19–45.
  8. Supersplavy / pod red. Ch.T. Simsa, N.S. Stoloffa, U.K. Khagelya [Superalloys / ed. by Ch.T. Sims, N.S. Stoloff, U.K. Khagelya]. M.: Metallurgiya, 1995. T. II, kn. 1. 384 s.
  9. Ponomarenko D.A., Moiseev N.V., Skugorev A.V. Shtampovka diskov GTD iz zharoprochnykh splavov na izotermicheskikh pressakh [Punching of disks GTD from hot strength alloys on isothermal presses] // Aviacionnye materialy i tekhnologii. 2013. №1. S. 13–16.
  10. Ponomarenko D.A., Skugorev A.V., Sidorov S.A., Strokov V.V. Tekhnologicheskie vozmozhnosti specializirovannykh izotermicheskikh pressov siloj 6,3 i 16 MN v proizvodstve detalej aviacionno-kosmicheskogo naznacheniya [Technological capabilities specialized isothermal pressov with a force of 6,3 and 16 MN in production of details of aerospace assignment] // Kuznechno-shtampovochnoe proizvodstvo. Obrabotka metallov davleniem. 2015. №9. S. 36–41.
  11. Chabina E.B., Alekseev A.A., Filonova E.V., Lukina E.A. Primenenie metodov analiticheskoj mikroskopii i rentgenostrukturnogo analiza dlya issledovaniya strukturno-fazovogo sostoyaniya materialov [Application of methods of analytical microscopy and X-ray of the structural analysis for research of structural and phase condition of materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №5. St. 06. Available at: http://www.viam-works.ru (accessed: March 14, 2018).
  12. Kablov E.N., Golubovskij E.R. Zharoprochnost nikelevykh splavov: ucheb. posobie [Thermal stability of nickel alloys: manual]. M.: Mashinostroenie, 1998. 464 s.
  13. Chabina E.B., Filonova E.V., Lomberg B.S., Bakradze M.M. Struktura sovremennykh deformiruemykh nikelevykh splavov [Structure of modern deformable nickel alloys] // Vse materialy. Enciklopedicheskij spravochnik. 2012. №6. S. 22–27.
  14. Kablov E.N., Grashhenkov D.V., Uvarova N.E. Issledovaniya metodom infrakrasnoj spektroskopii strukturnyh izmenenij gelej v processe termicheskoj obrabotki pri poluchenii vysokotemperaturnyh steklokeramicheskih materialov po zol-gel tehnologii [Researches by method of infrared spectroscopy of structural changes of gels in heat treatment process when receiving high-temperature glassceramic materials on technology sol-gel] // Aviacionnye materialy i tehnologii. 2011. №2. S. 22–25.
  15. Bakradze M.M., Ovsepyan S.V., Shugaev S.A., Letnikov M.N. Vliyanie rezhimov zakalki na strukturu i svojstva shtampovok diskov iz zharoprochnogo nikelevogo splava EK151-ID [The influence of quenching on structure and properties nickel-based superalloy EK151-ID forgings] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №9. St. 01. Available at: http://www.viam-works.ru (accessed: March 14, 2018).