Antipov V.V., Chesnokov D.V., Kozlov I.A., Volkov I.A., Petrova A.P. Surface preparation aluminum alloy V-1469 before use in the composition of layered hybrid material // Proceedings of VIAM. 2018. No. 4 (64). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-4-59-65.

Surface preparation aluminum alloy V-1469 before use in the composition of layered hybrid material

Antipov V.V., Chesnokov D.V., Kozlov I.A., Volkov I.A., Petrova A.P.
Abstract

Despite the increased interest of designers to composite polymeric materials (PCM), aluminum alloys are the main structural material of the aviation industry. Particular attention is paid to aluminum-lithium alloys and hybrid materials based on them, such as SIAL, which are layered materials of a new generation. SIALs are layered hybrid metal-polymer materials, which consist of thin sheets of structural aluminum alloys and GRP based on adhesive melt-type binders and glass fiber fillers with different reinforcement structures. The article provides information on the preparation of the surface of the aluminum-lithium alloy V-1469, which was selected for use in SIAL for the manufacture of wing panel panels. In this paper, the issue of protecting such alloys from corrosion and giving their surfaces special properties, in particu-lar, ensuring good adhesion of epoxy adhesive binders, is considered. Various types of anodic oxidation of the surface of aluminum alloys for bonding are conside

Keywords
aluminum alloys, laminated hybrid material, glue prepreg, surface preparation, anodic oxidation, electrolytes, corrosion.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [In-novative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Karimova S.A., Pavlovskaya T.G. Razrabotka sposobov zashhity ot korrozii konstrukcij, rabotayushhih v usloviyah kosmosa [Development of corrosion protection methods for structures operating under space conditions] // Aviacionnye materialy i tehnologii. 2013. №S1. S. 35–40.
  4. Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
  5. Kablov E.N. Korroziya ili zhizn [Corrosion or life] // Nauka i zhizn. 2012. №11. S. 16–21.
  6. Anihovskaya L.I., Pavlovskaya T.G., Dementeva P.A., Petrova A.P. Podgotovka poverhnosti pod skleivanie [Surface preparation under pasting] // Klei. Germetiki. Tehnologii. 2008. №7. S. 32–35.
  7. Illarionov E.I., Kolobnev N.I., Gorbunov P.Z., Kablov E.N. Alyuminievye splavy v aviakosmicheskoj tehnike [Aluminum alloys in aerospace equipment]. M.: Nauka, 2001. 192 s.
  8. Kolobova Z.N., Pavlovskaya T.G., Anihovskaya L.I., Karimova S.A. Razrabotka sposobov podgotovki poverhnosti pri remonte kleenyh konstrukcij iz alyuminievyh splavov [Development of ways of surface preparation at repair of glued designs from aluminum alloys] // Aviacionnye materialy i tehnologii. M.: VIAM, 2002. Vyp.: Remontnye tehnologii v aviastroenii. S. 73–76.
  9. Fridlyander I.N., Senatorova O.G., Lukina N.F., Antipov V.V. Sloistye alyumopolimernye materialy SIAL [SIAL layered aluminapolymeric materials] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007. M.: VIAM, 2007. S. 188–192.
  10. Vojtovich V.A. Sposoby podgotovki poverhnosti izdelij iz metallov i splavov [Ways of surface preparation of products from metals and alloys] // Klei. Germetiki. Tehnologii. 2005. №9. S. 19–23.
  11. Karimova S.A., Pavlovskaya T.G., Petrova A.P. Podgotovka alyuminievyh splavov s primeneniem anodnogo oksidirovaniya [Preparation of aluminum alloys using anodic oxida-tion] // Klei. Germetiki. Tehnologii. 2014. №1. S. 34–48.
  12. Averyanov E.E. Spravochnik po anodirovaniyu [Directory on anodizing]. M.: Mashinostroenie, 1988. 132 s.
  13. Karimova S.A., Kutyrev A.E., Pavlovskaya T.G., Zaharov K.E. Nizkotemperaturnoe uplotnenie anodno-oksidnyh pokrytij na detalyah iz alyuminievyh splavov [Low temperature sealing of anodic oxide coatings on parts of aluminum alloys] // Aviacionnye materialy i tehnologii. 2014. №4. S. 9–17. DOI: 10.18577/2071-9140-2014-0-4-9-17.
  14. Kurs M.G., Karimova S.A. Naturno-uskorennye ispytaniya: osobennosti metodiki i sposoby ocenki korrozionnyh harakteristik alyuminievyh splavov [Salt-accelerated outdoor corrosion testing: methodology and evaluation of corrosion susceptibility of aluminum alloy] // Aviacionnye materialy i tehnologii. 2014. №1. S. 51–57. DOI: 10.18577/2071-9140-2014-0-1-51-57.
  15. Karimova S.A., Zhilikov V.P., Mihajlov A.P. Naturno-uskorennye ispytaniya alyuminievyh splavov v usloviyah vozdejstviya morskoj atmosfery [Natural accelerated tests of aluminum alloys in the conditions of influence of the sea atmosphere] // Korroziya: materialy i zashhita. 2012. №10. S. 1–3.
  16. Petrova A.P., Donskoj A.A. Kleyashhie materialy. Germetiki: spravochnik [Gluing materials. Hermetics: directory]. SPb.: Professional, 2008. 589 s.
  17. Petrovа A.P., Dementyevа L.A., Lukina N.F., Chursova L.V. [Adhesive binders for polymer composite materials based on carbon- and glass fillers] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №9. St. 11. Available at: http://www.viam-works.ru (accessed: Marcht 20, 2018). DOI: 10.18577/2307-6046-2015-0-9-11-11.