Timoshkov P.N., Khrulkov A.V., Yazvenko L.N., Usacheva M.N. Composite materials for non-autoclave technology (review) // Proceedings of VIAM. 2018. No. 3 (63). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-3-37-48.

Composite materials for non-autoclave technology (review)

Timoshkov P.N., Khrulkov A.V., Yazvenko L.N., Usacheva M.N.
Abstract

The advantages of non-autoclaved molding technology in comparison with autoclave molding are considered in this article. The use of an autoclave ensures a high-quality curing of the polymer matrix, but because of the high cost of the apparatus, a non-autoclave method is widely used. Also, a molding scheme is given, the properties of the prepregs and resins for non-autoclaved molding of various manufacturers, the properties of the fiber fillers, the process of consolidating the prepreg with non-autoclave curing are analyzed.

Keywords
non-autoclave molding, porosity, viscosity, binder, resins.
Reference list
  1. Dushin M.I., Hrulkov A.V., Muhametov R.R. Vybor tehnologicheskih parametrov avtoklavnogo formovaniya detalej iz polimernyh kompozicionnyh materialov [A choice of technological parameters of autoclave formation of details from polymeric composite materials] // Aviacionnye materialy i tehnologii. 2011. №3. S. 20–26.
  2. Dushin M.I., Hrulkov A.V., Karavaev R.Yu. Parametry, vliyayushhie na obrazovanie poristosti v izdeliyah iz polimernyh kompozicionnyh materialov, izgotavlivaemyh bezavtoklavnymi metodami (obzor) [Parameters that influence the formation of porosity in the products made of polymer composite materials (PCM) produced by out-of-autoclave methods (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №2. St. 11. Available at: http://www.viam-works.ru (accessed: January 10, 2018). DOI: 10.18577/2307-6046-2015-0-2-11-11.
  3. Generalov A.S., Murashov V.V., Dalin M.A., Bojchuk A.S. Diagnostika polimernyh kompozitov ultrazvukovym reverberacionno-skvoznym metodom [Diagnostics of polymeric composites by ultrasonic reverberation transparent method] // Aviacionnye materialy i tehnologii. 2012. №1. S. 42–47.
  4. Dushin M.I., Doneckij K.I., Karavaev R.Yu. Ustanovlenie prichin obrazovaniya poristosti pri izgotovlenii PKM [Identification of the reasons of porosity formation when manufacturing composites] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №6 (42). St. 08. Available at: http://www.viam-works.ru (accessed: January 10, 2018). DOI: 10.18577/2307-6046-2016-0-6-8-8.
  5. Gusev Yu.A., Grigorev M.M., Timoshina L.N. Izgotovlenie etalonnyh obrazcov iz PKM s zadannoj poristostyu metodom vakuumnoj infuzii [Production of standard polymer composite samples with the set porosity by vacuum infusion] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №11. St. 06. Available at: http://www.viam-works.ru (accessed: January 10, 2018). DOI: 10.18577/2307-6046-2014-0-11-6-6.
  6. Dushin M.I., Muhametov R.R., Platonov A.A., Merkulova Yu.I. Issledovanie filtracionnyh harakteristik armiruyushhih napolnitelej i svyazuyushhih pri razrabotke tehnologii bezavtoklavnogo formovaniya polimernyh kompozicionnyh materialov [Study of filtration characteristics of reinforcing fillers and binders in the development of non-out-autoclave technology for polymer composite material] // Aviacionnye materialy i tehnologii. 2013. №2. S. 22–25.
  7. Raskutin A.E., Goncharov V.A. Komp'yuternoe modelirovanie tehnologicheskogo processa izgotovleniya PKM metodom vakuumnoj infuzii [Computer modeling of technological process of manufacturing of PCM by method of vacuum infusion] // Aviacionnye materialy i tehnologii. 2012. №S. S. 286–291.
  8. Kirillov V.N., Vapirov Yu.M., Drozd E.A. Issledovanie atmosfernoj stojkosti polimernyh kompozicionnyh materialov v usloviyah atmosfery teplogo vlazhnogo i umerenno teplogo klimata [Research of atmospheric firmness of polymeric composite materials in the conditions of the atmosphere of warm wet and moderately warm climate] // Aviacionnye materialy i tehnologii. 2012. №4. S. 31–38.
  9. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  10. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  11. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  12. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  13. Kablov E.N. Iz chego sdelat budushhee? Materialy novogo pokoleniya, tehnologii ih sozdaniya i pererabotki – osnova innovacij [Of what to make the future? Materials of new generation, technology of their creation and processing – basis of innovations] // Krylya Rodiny. 2016. №5. S. 8–18.
  14. Grunenfelder L.K., Centea T., Hubert P., Nutt S.R. Effect of room-temperature out-time on tow impregnation in an out-of-autoclave prepreg // Composites Part A: Applied Science Manufacturing. 2013. Vol. 45. P. 119–126.
  15. Centea T., Grunenfelder L.K., Nutt S.R. A review of out-of-autoclave prepregs – material properties, process phenomena and manufacturing considerations // Composites Part A: Applied Science Manufacturing. 2014. P. 132–154.
  16. Thorfinnson B., Biermann T. Degree of Impregnation of Prepregs – Effects on Porosity // Proceedings 32nd International SAMPE Symposium, Anaheim, CA: Society for the Advancement of Materials and Process Engineering. 1987. P. 9.
  17. Thorfinnson B., Biermann T. Production of Void Free Composite Parts Without Debulking // Proceedings 31st International SAMPE Symposium, Las Vegas, NV: Society for the Advancement of Materials and Process Engineering. 1986. P. 10.
  18. Kratz J., Hubert P. Anisotropic air permeability in out-of-autoclave prepregs: Effect on honeycomb panel evacuation prior to cure // Composites Part A: Applied Science Manufacturing. 2013. Vol. 49. P. 179–191.
  19. Grunenfelder L.K., Nutt S.R. Void formation in composite prepregs – Effect of dissolved moisture // Composites Science and Technology. 2010. Vol. 70. P. 2304–2309.
  20. Tavares S.S., Michaud V., Månson J.A.E. Through thickness air permeability of prepregs during cure // Composites Part A: Applied Science Manufacturing. 2009. Vol. 40. P. 1587–1596.