Kuznetsova V.A., Shapovalov G.G. Tendencies of development of the erosion-resistant coatings (review) // Proceedings of VIAM. 2018. No. 11 (71). Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-11-74-85.

Tendencies of development of the erosion-resistant coatings (review)

Kuznetsova V.A., Shapovalov G.G.
Abstract

In this work the main tendencies of development in the field of creation of erosion resistant paint, polymer and complex coatings for protection of metal wares and composite materials are considered. The main principles by which it is necessary to be guided at creation of erosion resistant coatings are revealed. The main requirements causing choice of basic components of protecting cover are considered. Groups of technologies and structures of coverings in compliance with the carried-out analysis are revealed. Leaders in the field of development of erosion resistant coatings are also defined.

Keywords
erosion-resistant coatings, paint coatings, erosive influence, abrasive wear.
Reference list
  1. Istoriya aviatsionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshch. red. E.N. Kablova [History of Aeronautical Materials Science. VIAM – 80 years: years and people / gen. ed. by E.N. Kablov]. M.: VIAM, 2012. 520 s.
  2. Kablov Ee.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of the new generation - the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
  3. Simonenko E.P., Simonenko N.P., Derbenev A.V., Nikolaev V.A., Sevastyanov V.G., Kuznetsov N.T., Grashchenkov D.V., Kablov E.N. Synthesis of nanocrystalline silicon carbide using the sol-gel technique // Russian Journal of Inorganic Chemistry. 2013. Vol. 58. No. 10. P. 1143–1151.
  4. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  5. Lavrov A.V., Erasov V.S., Landik D.N. Ob odnom podhode k traktovke obedinennoj teorii prochnosti Ya.B. Fridmana [One of the approaches to interpretation of the united strength theory of Ya.B. Fridman] // Aviacionnye materialy i tehnologii. 2017. №2 (47). S. 87–94. DOI: 10.18577/2071-9140-2017-0-2-87-94.
  6. Platonov A.A. Polimernye kompozicionnye materialy na osnove proshitogo napolnitelya s povyshennoj udarostojkostyu [Polymer composite materials on a base of stitched preforms with high impact resistance] // Aviacionnye materialy i tehnologii. 2014. №4. S. 43–47. DOI: 10.18577/2071-9140-2014-0-4-43-47.
  7. Vinogradov S.S., Demin S.A., Balahonov S.V., Kirillova O.G. Neorganicheskie kompozicionnye pokrytiya – perspektivnoe napravlenie v oblasti zashhity ot korrozii uglerodistyh stalej [Inorganic composite coatings – a perspective direction in the field of anticorrosive protection of carbon steels] // Aviacionnye materialy i tehnologii. 2016. №2 (41). S. 76–87. DOI: 10.18577/2071-9140-2016-0-2-76-87.
  8. Ogneerozionnostoykiy broniruyushchiy sostav dlya zaryada iz ballistitnogo tverdogo raketnogo topliva: pat. 2316528 Ros. Federatsiya [Flame retardant reservation composition for the charge of ballistic solid rocket fuel: pat. 2316528 Rus. Federation]; zayavl. 16.08.06; opubl. 10.02.08.
  9. Antikorrozionnaya lakokrasochnaya kompozitsiya: pat. 2169165 Ros. Federatsiya [Anticorrosive paint and varnish composition: pat. 2169165 Rus. Federation]; zayavl. 29.12.99; opubl. 20.06.01.
  10. Urethane coating composition and process: pat. 4110317 US; field 10.01.1974; publ. 29.08.78.
  11. Coating composition process for the preparation of coatings and coated substrate: pat. 4576868 US; field 14. 09. 84; publ. 18.03.86.
  12. Antennyy obtekatel: pat. 2277738 Ros. Federatsiya [Antenna fairing: pat. 2277738 Rus. Federation]; zayavl. 23.11.04; opubl. 10.06.06.
  13. Clear paint and production thereof: pat. 6079069 JP; field 07.10. 83; publ. 04.05.85.
  14. Erosion resistant anti-icing coatings: pat. 2006281861 US; field 13. 06.05; publ. 14.12.06.
  15. Hydrophobic coating compositions, articles coated with said compositions, and processes for manufacturing same: pat. 7268179 US; field 30.09.03; publ. 11.09.07.
  16. A method for producing a protective layer, protective layer, and using the same component with a protective layer: app. 10329049 DE; field 09.12.03; publ. 13.01.05.
  17. Process for producing resin composition containing inorganic filler: pat. 60079423 EP; field 25. 09.96; publ. 10.09.97.
  18. White radiotransparent antistatic paints for satellites: pat. 0487366 FR; field 25.10.91; publ. 27.05.92.
  19. Kompozitsiya dlya antikorrozionnogo pokrytiya: pat. 2009153 Ros. Federatsiya [Composition for anti-corrosion coating: pat. 2009153 Rus. Federation]; zayavl. 23.11.92; opubl. 15.03.94.
  20. Compositions for coatings: pat. 1502591 SU; field 31.03.87; publ. 23.08.89.
  21. Elastomeric formulation used in the construction of lightweight aircraft engine fan blades: pat. 6287080 US; field 15.11.99; publ. 11.09.01.
  22. Elastomer coated layer for erosion and/or fire protection: pat. 5908528 US; field 16.04.98; publ. 06.01.99.
  23. Elastomer coated layer for erosion and/or fire protection: pat. 5912195 US; field 16.04.98; publ. 15.06.99.
  24. Sostav dlya zashchitnogo pokrytiya: pat. 2290421 Ros. Federatsiya [Composition for a protective coating: pat. 2290421 Rus. Federation]; zayavl. 01.08.05; opubl. 27.12.06.
  25. Polimernaya kompozitsiya dlya pokrytiy: pat. 2333925 Ros. Federatsiya [Polymer composition for coatings: pat. 2333925 Rus. Federation]; zayavl. 11.05.07; opubl. 20.09.08.
  26. Sostav dlya zashchity polimernykh kompozitsionnykh materialov: pat. 2215012 Ros. Federatsiya [Composition for the protection of polymer composite materials: pat. 2215012 Rus. Federation]; zayavl. 27.11.01; opubl. 27.10.03.
  27. Composite coating for imparting particle erosion resistance: pat. 6706405 US; field 11. 02.02; publ. 16.03.04.
  28. Erosion resistant surface protection: pat. 5486096 US; field 30.06.94; publ. 23.01.96.
  29. Composite airfoil leading edge protection: pat. 5449273 US; field 21.03.94; publ. 12.09.95.
  30. Coating composition forming wear-resistant coat and article covered with the coat: pat. 630650; field 19.03.98; pub. 23.10.01.
  31. Method and apparatus for laying roadway materials: pat. 9711129 EU; field 20.09.96; publ. 27.03.97.
  32. Coating composition forming wear-resistant coat and article covered with the coat: pat. 0869154 JP; field 20.09.96; publ. 07.10.98.
  33. Composition for providing an abrasion resistant coating on a substrate with a matched refractive index and controlled tintability: pat. 6342097 US; field 20.04.00; publ. 29.01.02.
  34. Fast curable epoxy compositions containing imidazole-and 1-(aminoalkyl) imidazole-isocyanate adducts: pat. 8357764 US; field 30. 10.09; publ. 22.01.13.
  35. Erosion resistant films for use on heated aerodynamic surfaces: pat. 8096508 US; field 10.08.07; publ. 17.01.12.
  36. Method for the preparation of protective coatings having enhanced characteristics: pat. 972272 US; field 04.12.96; publ.13.11.97.
  37. Cycloaliphatic epoxy compounds: pat. 0946569 EU; field 16.12.97; publ. 20.08.03.
  38. Cycloaliphatic epoxy compounds: pat. 982709 Italy; field 16.12.97; publ. 13.08.98.
  39. Preparation method of temperature-resistant and erosion-resistant coating for walling of flue: pat. 101096460 CN; field 30.06.06; publ. 02.01.08.
  40. Organic-inorganic hybrid resin containing sesquialter siloxane and preparation method and use thereof: pat. 101139442 CN; field 22.08.07; publ. 07.12.11.
  41. Sostav dlya zashchity polimernykh kompozitsionnykh materialov: pat. 2215012 Ros. Federatsiya [Composition for the protection of polymer composite materials: pat. 2215012 Rus. Federation]; zayavl. 27.11.01; opubl. 27.10.03.
  42. Karabanov S.M., Suvorov D.V., Slivkin E.V. I dr. Uvelicheniye erozionnoy stoykosti pokrytiy elektrodov vakuumnykh i gazorazryadnykh kommutatsionnykh priborov [Increase of erosion resistance of coatings of electrodes of vacuum and gas-discharge switching devices] // Vestnik RGRTU. 2015. № 54. Ch. 2. S. 127–131.
  43. Kompozitnyye listy na osnove termoplasta, vklyuchayushchiye natural'nyye volokna: pat. 2386724 Ros. Federatsiya [Composite sheets based on thermoplastic, including natural fibers: pat. 2386724 Rus. Federation]; zayavl. 08.11.05; opubl. 20.04.10.
  44. Sistema zashchity ot erozionno-korrozionnogo razrusheniya korpusov morskikh sudov i sooruzheniy: pat. 2496916 Ros. Federatsiya [The system of protection against erosion-corrosion damage to the hulls of marine vessels and structures: pat. 2496916 Rus. Federation]; zayavl. 17.05.12; opubl. 27.10.13.
  45. Zhestkov B.E., Terent’eva V.S. Cite as Multifunctional coating MAI D5 intended for the protection of refractory materials// Russian Metallurgy (Metally) 2010. Vol. 2010. Issue 1. P. 33–40.
  46. Sposob polucheniya materiala dlya vysokotemperaturnogo erozionnostoykogo zashchitnogo pokrytiya: pat. 2522552 Ros. Federatsiya [The method of obtaining material for high-temperature erosion-resistant protective coating: pat. 2522552 Rus. Federation]; zayavl. 01.11.12; opubl. 20.07.14.
  47. Coating for aerospace aluminum parts: pat. 6171704 US; field 29.12.95; publ. 09.01.01.
  48. Anti-fouling coating for turbomachinery: pat. 615954 US; field 28.07.99; publ. 12.12.00.
  49. Heat and rain erosion resistant coating: pat. 200802086 US; field 28.11.06; publ. 21.02.08.
  50. Erosions systems and components comprising the same: pat. 7875354 US; field 28.03.08; publ. 25.01.11.
  51. Abrasion resistant coatings: pat. 7736745 US; field 24.05.05; publ. 15.06.10.
  52. Thiophene-containing poly(arylene ether) sulfones: pat. 5410013 US; field 01.06.94; publ. 25.04.95.
  53. Removable magnetic liner and processes of production, installation, and use thereof: pat. 8287791 US; field 23.12.09; publ. 16.10.12.
  54. Processes for repairing erosion resistant coatings: pat. 2008248300 US; field 05.04.07; publ. 09.10.08.
  55. Erosion resistant surface and method of making erosion resistant surfaces: pat. 7968184 US; field 03.12.07; publ. 28.06.11.
  56. Two-component coating compositions and coatings produced therefrom for improving erosion resistance: pat. 2951466 EU; field 28.04.15; publ. 07.01.16.
  57. Method for producing a protective coating for a component of a turbomachine, the component itself and the respective machine: pat. 2010239873 EU; field 10.03.10; publ. 23.09.10.
  58. Preparation method for oxidized graphene erosion-resistant coating attached to iron surface: pat. 105215346 CN; field 30.08.15; publ. 06.01.16.
  59. Kuznetsova V.A. Erozionnostoykaya kompozitsiya na osnove trekhfaznoy sistemy: epoksidnyy oligomer–kauchuk–armiruyushchiy napolnitel: dis. … kand. tekhn. nauk [Erosion-resistant composition based on a three-phase system: epoxy oligomer–rubber–reinforcing filler: thesis, Cand. Sci. (Tech.)]. M.: VIAM, 1999. 129 s.
  60. Chernoyarov S.A., Ivanov A.V., Borkova A.N., Pomakhayeva L.I., Pomakhayev V.P., Anikhovskaya L.I., Kuznetsova V.A. Issledovaniya stoykosti k kapleudarnoy erozii steklotekstolita s polimernymi zashchitnymi pokrytiyami [Studies of resistance to droplet-impact erosion of fiberglass with polymeric protective coatings] // Aviacionnyye materialy i tehnologii. 2003. №3. S. 73–75.
  61. Borkova A.N. Erozionnaya stoykost aviatsionnykh materialov pri soudarenii s tverdymi (pylevymi) chastitsami: dis. … kand. tekhn. nauk [Erosion resistance of aviation materials in collisions with solid (dust) particles: thesis, Cand. Sci. (Tech.)]. M.: VIAM, 2006. 125 s.
  62. Astruc A., Joliff E., Chailan J.-F. et al. Incorporation of kaolin fillers into an epoxy polyamidoamine matrix for coatings // Progress in Organic Coatings. 2009. Vol. 65. Issue 1. P. 158–168.
  63. Omid G. Impact of erosion testing aspects on current and future flight conditions // Progress in Aerospace Science. 2011. Vol. 47. Issue 4. P. 280–303.
  64. Grundwürmer M., Nuyken O., Meyer M. Sol-gel derived erosion protection coatings against damage caused by liquid impact // 16th International Conference on Wear of Materials. 2007. Vol. 263. Issue 1–6. P. 318–329.
  65. Farhadinejad Z., Ehsani M., Moemen-Bellah S. Dynamic mechanical and thermal behavior evaluation of an epoxy/anhydride/nano-aluminum oxide composite system // High Performance Polymers. 2013. Vol. 25. Issue 5. P. 518–525.
  66. Li Ying Guo, Li Yan Wang, Xin Su. Research Progress of New Methods for Toughening Epoxy Resin // Advanced Materials Research. 2012. Vol. 490–495. P. 3598–3602.
  67. Stroganov V.F., Stroganova I.V. Filled epoxy polymer couplings with «shape memory» effect // Polymer Science (Series D). 2011. Vol. 4. Issue 3. P. 183–187.