Ospennikova O.G., Pikulina L.V., Orlova V.Yu. Model compositions on the basis of synthetic materials. Peculiarity of physical and mechanical and technological properties // Proceedings of VIAM. 2018. No. 10 (70). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2018-0-10-37-44.

Model compositions on the basis of synthetic materials. Peculiarity of physical and mechanical and technological properties

Ospennikova O.G., Pikulina L.V., Orlova V.Yu.
Abstract

Reception of cast details with high geometrical accuracy a moulding method on melted models in mainly depends on quality of model compositions and their components as casting completely repeats model configuration. On the basis of the conducted research were developed and formulated requirements to model composition, the manufacturing technology is fulfilled, the method of quality control is developed and also the method of adjustment of technological modes of manufacturing models of parts of different nomenclature on a fluidity indicator of melt and viscosity of model compositions is proposed.

Keywords
model compositions, moulding on melted models, models, moulding, fluidity indicator of melt, viscosity.
Reference list
  1. Kablov E.N., Petrushin N.V., Svetlov I.L. Sovremennyye lityye nikelevyye zharoprochnyye splavy [Modern cast nickel superalloys] // Tr. Mezhdunar. nauch.-tekhn. konf. «Nauchnyye idei S.T. Kishkina i sovremennoye materialovedeniye». M., 2006. S. 39–55.
  2. Kablov E.N., Bondarenko Yu.A., Echin A.B. Razvitiye tekhnologii napravlennoy kristallizatsii liteynykh vysokozharoprochnykh splavov s peremennym upravlyayemym temperaturnym gradiyentom [Development of technology of cast superalloys directional solidification with variable controlled temperature gradient] // Aviacionnyye materialy i tehnologii. 2017. №S. S. 24–38. DOI: 10.18577/2071-9140-2017-0-S-24-38.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Kablov E.N. Osnovnyye napravleniya razvitiya litya lopatok gazovykh turbin [The main directions of development of the casting of gas turbine blades] // Lityye lopatki gazoturbinnykh dvigateley: splavy, tekhnologii, pokrytiya. M.: Nauka, 2006. S. 609–623.
  5. Kablov E.N., Svetlov I.L., Demonis I.M., Folomeykin Yu.I. Monokristallicheskiye lopatki s transpiratsionnym okhlazhdeniyem dlya vysokotemperaturnykh gazoturbinnykh dvigateley [Single-crystal blades with transpiration cooling for high-temperature gas turbine engines] // Aviacionnyye materialy i tehnologii. 2003. №1. S. 24–33.
  6. Kablov E.N., Bondarenko Yu.A., Yechin A.B., Surova V.A., Kablov D.E. Razvitiye protsessa napravlennoy kristallizatsii lopatok GTD iz zharoprochnykh i intermetallidnykh splavov s monokristallicheskoy strukturoy [Development of the process of directed crystallization of GTE blades from heat-resistant and intermetallic alloys with a single-crystal structure] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroyeniye. 2011. №SP2. S. 20–25.
  7. Kablov E.N., Tolorajya V.N. VIAM – osnovopolozhnik otechestvennoj tehnologii litya monokristallicheskih turbinnyh lopatok GTD i GTU [VIAM – the founder of domestic casting technology of single-crystal turbine blades of GTE and GTU] // Aviacionnye materialy i tehnologii. 2012. №S. S. 105–117.
  8. Kablov E.N., Bondarenko Yu.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [Development of process of the directed crystallization of blades of GTE from hot strength alloys with single-crystal and composition structure] // Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
  9. Kablov E.N., Bondarenko Yu.A. Novoye v tekhnologii proizvodstva lopatok GTD [New in the technology of production of GTE blades] // Aerokosmicheskiy kuryer. 1999. №2. S. 60–62.
  10. Kablov E.N., Kishkin S.T. Perspektivy primeneniya liteynykh zharoprochnykh splavov dlya proizvodstva turbinnykh lopatok GTD [Prospects for the use of foundry heat-resistant alloys for the production of turbine blades GTE] // Gazoturbinnyye tekhnologii. 2002. №1. S. 34–37.
  11. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Liteynyye zharoprochnyye splavy novogo pokoleniya [Foundry superalloys of new generation] // 75 let. Aviacionnyye materialy. M.: VIAM, 2007. S. 27–44.
  12. Kablov E.N. Materialy novogo pokoleniya – osnova innovatsiy, tekhnologicheskogo liderstva i natsionalnoy bezopasnosti Rossii [Materials of the new generation - the basis of innovation, technological leadership and national security of Russia] // Intellekt i tekhnologii. 2016. №2 (14). S. 16–21.
  13. Ospennikova O.G. Modelnyye kompozitsii na osnove sinteticheskikh materialov dlya lit'ya po vyplavlyayemym modelyam detaley GTD: avtoref. dis. … kand. tekhn. nauk [Model compositions based on synthetic materials for investment casting of GTE parts: abstract of a thesis, Cand. Sc. (Tech.)]. M.: Salyut, 2000. 32 s.
  14. Ospennikova O.G., Khayutin S.G. Struktura model'nykh kompozitsiy dlya lit'ya po vyplavlyayemym modelyam [The structure of model compositions for investment casting] // Materialovedeniye. 2009. №10. S. 46–51.
  15. Ospennikova O.G., Shutov A.N., Pikulina L.V., Dushkin A.M. Pattern compounds based on synthetic materials for casting gas-turbine engine blades [Casting gas-turbine engine blades] // Liteynoye proizvodstvo. 2003. №1. S. 21–29.
  16. Ospennikova O.G. Issledovanie i razrabotka parametrov tehnologicheskogo processa izgotovleniya modelej iz modelnyh kompozicij na osnove sinteticheskih voskov [Research and working out of parametres of technological process of manufacturing of models from modelling compositions on the basis of synthetic waxes] // Aviacionnye materialy i tehnologii. 2014. №3. S. 18–21. DOI: 10.18577/2071-9140-2014-0-3-18-21.
  17. Ospennikova O.G. Issledovanie vliyaniya napolnitelej na svojstva i stabilnost modelnyh kompozicij, vybor optimalnyh sostavov [Influence research of fillers on properties and stability of modelling compositions, a choice of optimum structures] // Aviacionnye materialy i tehnologii. 2014. №3. S. 14–17. DOI: 10.18577/2071-9140-2014-0-3-14-17.
  18. Kompozitsiya dlya izgotovleniya vyplavlyayemykh modeley: pat. 2447968 Ros. Federatsiya [Composition for the manufacture of melted models: pat. 2447968 Ros. Federation]; zayavl. 14.12.10, opubl. 20.04.12.
  19. Kompozitsiya dlya izgotovleniya vyplavlyayemykh modeley: pat. 2447969 Ros. Federatsiya [Composition for the manufacture of melted models: pat. 2447969 Ros. Federation]; zayavl. 14.12.10; opubl. 20.04.12.
  20. Kompozitsiya dlya izgotovleniya vyplavlyayemykh modeley: pat. 2182057 Ros. Federatsiya [Composition for the manufacture of melted models: pat. 2182057 Ros. Federation]; zayavl. 31.05.00; opubl. 10.05.02.
  21. Kompozitsiya dlya izgotovleniya vyplavlyayemykh modeley: pat. 2162386 Ros. Federatsiya [Composition for the manufacture of melted models: Pat. 2162386 Ros. Federation]; zayavl. 17.03.10; opubl. 27.01.01.
  22. Kompozitsiya dlya izgotovleniya vyplavlyayemykh modeley: pat. 2177387 Ros. Federatsiya [Composition for the manufacture of melted models: Pat. 2177387 Ros. Federation]; zayavl. 31.05.00; opubl. 27.12.01.
  23. Repyakh S.I. Tekhnologicheskiye osnovy lit'ya po vyplavlyayemym modelyam [Technological basis of investment casting]. Dnepropetrovsk: Lira, 2006. 1056 s.
  24. Kablov E.N., Deyev V.V., Narskiy A.R., Bondarenko Yu.A. Tekhnologiya udaleniya modelnykh mass iz keramicheskikh form dlya litya po vyplavlyayemym modelyam [Technology for removing model masses from ceramic molds for investment casting] // Liteynoye proizvodstvo. 2005. №3. S. 20–22.