Petrova G.N., Sapego Yu. A., Larionov S.A., Platonov M.M., Laptev A.B. Fireproof thermoplastic materials for 3D-technologies // Proceedings of VIAM. 2017. No. 9 (57). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2017-0-9-7-7.

Fireproof thermoplastic materials for 3D-technologies

Petrova G.N., Sapego Yu. A., Larionov S.A., Platonov M.M., Laptev A.B.
Abstract

Results of researches of the fireproof thermoplastic materials developed in VIAM Federal State Unitary Enterprise for use in FDM of the additive technology 3D are given in article – the press. Requirements for level of utilization and technical characteristics to which such materials have to answer are formulated. Physical-mechanical, rheological and fireproof properties of the developed thermoplastic compositions on the basis of polycarbonate and polyamide are considered. Test results of the samples received on traditional casting technology under pressure and innovative way 3D – the press are given. It is shown that the developed materials on level of properties and technological effectiveness do not concede to foreign analogs. The interrelation between technological parameters of level-by-level synthesis of object (temperature of extrusion, camera temperature, orientation of molecules in strand) on the accuracy of the press and its strength properties is defined. The received pat

Keywords
polycarbonate, polyamide, fire safety, rheology, molten viscosity, 3D-press, fused deposition modeling (FDM), processing.
Reference list
  1. Mihajlin Yu.A. Termoustojchivye polimery i polimernye materialy na ih osnove [Thermo resistant polymers and polymeric materials on their basis] // Polimernye materialy. 2005. №4. S. 29–32.
  2. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  3. Kablov E.N., Semenova L.V., Petrova G.N., Larionov S.A., Perfilova D.N. Polimernye kompozicionnye materialy na termoplastichnoj matrice [Polymeric composite materials on thermoflexible matrix] // Izvestiya vuzov. Ser.: Himiya i himicheskaya tehnologiya. 2016. T. 59. №10. S. 61–71.
  4. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  5. Sudarushkin Yu.K., Gudimov M.M., Romanov D.S., Sokolov M.Yu. Primenenie lit'evyh polikarbonatov v aviapriborostroenii [Application of lityevy polycarbonates in avionics] // Aviacionnaya promyshlennost. 2003. №2. S. 48–52.
  6. Petrova G.N.. Bejder E.Ya., Starostina I.V. Molding termoplasty dlya izdelij aviacionnoj tehniki [Lityevye thermoplastics for products of aviation engineering] // Vse materialy. Enciklopedicheskij spravochnik. 2016. №6. S. 10–15.
  7. Kerber M.L., Vinogradov V.M., Golovkin G.S. i dr. Polimernye kompozicionnye materialy: struktura, svojstva, tehnologiya [Polymeric composite materials: structure, properties, technology]. SPb.: Professiya, 2011. S. 32–33.
  8. Petrova G.N., Zhuravleva P.L., Iskhodzhanova I.V., Beider E.Ya. Influence of Carbon Fillers on Properties and Structure of Polyethylene-Based Polymer Composites // Nanotechnologies in Russia. 2014. Vol. 9. No. 5–6. Р. 305–310.
  9. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazujushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] // Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  10. Beider E.Ya., Petrova G.N., Izotova T.F., Gureeva E.V. Kompozicionnye termoplastichnye materialy i penopoliimidy [Thermoplastic composite materials and foam polyimides] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №11. St. 01. Available at: http://www.viam-works.ru (accessed: February 07, 2017).
  11. Bejder E.Ya., Petrova G.N., Dykun M.I. Beider E.Ya., Petrova G.N., Dykun M.I. Appretirovanie uglerodnyh volokon-napolnitelej termoplastichnyh karboplastikov [Dressing of carbon fibers – fillers of thermoplastic carbon reinforced plastics] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №10. St. 03. Available at: http://www.viam-works.ru (accessed: July 12, 2017). DOI: 10.18577/2307-6046-2014-0-10-3-3.
  12. Sorokin A.E., Bejder E.Ya., Perfilova D.N. Vliyanie klimaticheskih faktorov na svojstva ugleplastika na polifenilensulfidnom svyazuyushhem [Effect of climatic factors on properties of carbon fiber reinforced plastic based on polyphenylenesulfide resin] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №1. St. 10. Available at: http://www.viam-works.ru (accessed: July 12, 2017). DOI: 10.18577/2307-6046-2015-0-1-10-10.
  13. Bejder E.Ya., Petrova G.N. Termoplastichnye svyazuyushhie dlya polimernyh kompozicionnyh materialov [The thermoplastic binder for polymeric composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №11. St. 05. Available at: http://viam-works.ru. (accessed: July 12, 2017). DOI: 10.18577/2307-6046-2015-0-11-5-5.
  14. Nazarov V.G., Stolyarov V.P., Petrova G.N., Gryaznov V.I., Buznik V.M. Osobennosti poverhnostnogo ftorirovaniya termoelastoplastov na osnove poliuretana i ego vliyanie na svojstva polimera [Features of surfacing fluorine of thermoelastoplastics on the basis of polyurethane and its influence on properties of polymer] // Perspektivnye materialy. 2016. №2. S. 52–60.
  15. Gryaznov V.I., Petrova G.N., Yurkov G.Yu., Buznik V.M. Smesevye termojelastoplasty so specialnymi svojstvami [Thermoplastic mixtures with special properties] // Aviacionnye materialy i tehnologii. 2014. №1. S. 25–29. DOI: 10.18577/2071-9140-2014-0-1-25-29.
  16. Sorokin A.E., Krasnov A.P., Zyuzina G.F. i dr. Stroenie i svojstva vysokomolekulyarnogo lit'evogo poliarilata [Structure and properties of high-molecular molding polyarylate] // Plasticheskie massy. 2012. №1. S. 8–12.
  17. Petrova G.N., Starostina I.V., Rumyanceva T.V. Issledovanie vozmozhnosti markirovki detalej iz polikarbonata [Study of the possibility of marking parts of polycarbonate] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №10. St. 11. Available at: http://www.viam-works.ru (accessed: February 08, 2017). DOI: 10.18577/2307-6046-2016-0-10-11-11.
  18. Kondrashov S.V., Shashkeev K.A., Petrova G.N., Mekalina I.V. Polimernye kompozicionnye materialy konstrukcionnogo naznacheniya s funkcionalnymi svojstvami [Constructional polymer composites with functional properties] // Aviacionnye materialy i tehnologii. 2017. №S. S. 405–419. DOI: 10.18577/2071-9140-2017-0-S-405-419.
  19. Petrova G.N., Larionov S.A., Platonov M.M., Perfilova D.N. Termoplastichnye materialy novogo pokoleniya dlya aviacii [Thermoplastic materials of new generation for aviation] // Aviacionnye materialy i tehnologii 2017. №S. S. 420–436. DOI: 10.18577/2071-9140-2017-0-S-420-436.
  20. Kryzhanovskij V.K., Burlov V.V., Panimatchenko A.D., Kryzhanovskaya Yu.V. Tehnicheskie svojstva polimernyh materialov [Engineering properties of polymeric materials]. SPb.: Professiya, 2005. 240 s.
  21. Kablov E.N. Additivnye tehnologii – dominanta nacional'noj tehnologicheskoj iniciativy [The additive technologies – dominant of national technological initiative] // Intellekt i tehnologii. 2015. №2 (11). S. 52–55.
  22. Dudeк P. FDM 3D printing technology in manufacturing composite elements // Archives of Metallurgy and Materials. 2013. Vol. 58. Iss. 4. DOI: 10.2478/amm-2013-0186.
  23. Novakova-Marcincinova L., Novak-Marcincin J. Verification of mechanical properties of abs materials used in FDM rapid prototyping technology // Proceedings in Manufacturing Systems. 2013. Vol. 8. Iss. 2. P. 87–92.
  24. Smirnov O.I., Skorodumov S.V. Modelirovanie tehnologii poslojnogo sinteza pri razrabotke izdelij slozhnoj formy [Modeling of technology of level-by-level synthesis when developing products of difficult form] // Sovremennye naukoemkie tehnologii. 2010. №4. S. 83–87.
  25. Lužanin O., Movrin D., Plančak M. Experimental investigation of extrusion speed and temperature effects on arithmetic mean surface roughness in FDM built spectmens // Journal for Technology of Plasticity. 2013. Vol. 38. No. 2. P. 179–191.
  26. Barnatt C. 3D printing: the next industrial revolution. CreateSpace Independent Publishing Platform, 2013. P. 8–20.
  27. 3D systems corporation: annual report. Washington D.C., 2012. P. 2.
  28. Canessa E., Fonda C., Zennaro M., Ranellucci A. Low-cost 3D printing // Reprap, Slic3r and the Future of 3D Printing / ed. by A. Ranellucci. Trieste, 2013. P. 75–78.
  29. Barbotko S.L., Volnyj O.S., Kirienko O.A., Shurkova E.N. Osobennosti ispytanij aviacionnyh materialov na pozharoopasnost. Chast 1. Ispytaniya na goryuchest'. Vliyanie tolshhiny obrazca na registriruemye harakteristiki [Features of tests of aviation materials on fire danger. Part 1. Tests for combustibility. Influence of thickness of sample on registered characteristics] // Pozharovzryvobezopasnost. 2015. №1. S. 40–49.
  30. Barbotko S.L., Volnyj O.S., Kirienko O.A., Shurkova E.N. Osobennosti ispytanij aviacionnyh materialov na pozharoopasnost. Chast 2. Ispytaniya na goryuchest – vliyanie prodolzhitelnosti ekspozicii plamenem gorelki [Features of tests of aviation materials on fire danger. Part 2. Tests for combustibility – influence of duration of exposure by torch flame] // Pozharovzryvobezopasnost. 2015. №3. S. 13–24.
  31. Barbotko S.L., Volnyj O.S., Kirienko O.A., Shurkova E.N. Osobennosti ispytanij aviacionnyh materialov na pozharoopasnost. Chast 3. Ispytaniya na dymoobrazovanie – vliyanie tolshhiny monolitnogo obrazca polimernogo kompozicionnogo materiala [Features of tests of aviation materials on fire danger. Part 3. Tests for smoke formation – influence of thickness of monolithic sample of polymeric composite material] // Pozharovzryvobezopasnost. 2015. №4. S. 7–23.
  32. Mihajlin Yu.A. Pokazateli ognestojkosti PM i metody ih opredeleniya [Indicators of fire resistance of PM and methods of their definition] // Polimernye materialy. 2011. №8. S. 32–34.
  33. Petrova G.N., Beider E.Ya., Perfilova D.N., Rumyantseva T.V. Pozharobezopasnye litevye termoplasty i termojelastoplastyv [Fire safety of injection molding thermoplastics and TPE materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №11. St. 02. Available at: http://www.viam-works.ru (accessed: February 07, 2017).
  34. Platonov M.M., Petrova G.N., Larionov S.A., Barbotko S.L. Polimernaya kompoziciya na osnove polidodekalaktama dlya tehnologii 3D-pechati rasplavlennoj polimernoj nityu [Polymer composition on the basis of polydodecanolactam for 3D-printing technology by melted polymer string] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №10 (46). St. 09. Available at: http://www.viam-works.ru (accessed: July 12, 2017). DOI: 10.18577/2307-6046-2016-0-10-9-9.
  35. Platonov M.M., Petrova G.N., Larionov S.A., Barbotko S.L. Optimizaciya sostava polimernoj kompozicii s ponizhennoj pozharnoj opasnostyu na osnove polikarbonata dlya tehnologii 3D-pechati rasplavlennoj polimernoj nityu [Optimization of structure of polymeric composition with the lowered fire danger on the basis of polycarbonate for technology of the 3D-press the melted polymeric thread] // Izvestiya vuzov. Himiya i himicheskaya tehnologiya. 2017. T. 60. №1. S. 87–94.
  36. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.