Farafonov D.P., Degovets M.L., Rogalev A.M. Research of experimental compositions of wear-resistant alloys on the basis of cobalt for repair and hardening of working blades of high-pressure turbines by method of laser welding // Proceedings of VIAM. 2017. No. 8 (56). Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2017-0-8-5-5.

Research of experimental compositions of wear-resistant alloys on the basis of cobalt for repair and hardening of working blades of high-pressure turbines by method of laser welding

Farafonov D.P., Degovets M.L., Rogalev A.M.
Abstract

In article results of researches of heat resisting wear-resistant alloys on the basis of cobalt (systems Co–Cr–W–C, Co–Cr–Mo–Si) are provided. For the purpose of choice of composition of wear-resistant alloy for receiving the high-pure metalpowder composition designed for repair and hardening of high-pressure turbines blades by method of laser welding, comparative researches of properties of experimental cobalt-based alloys are conducted. By results of researches the alloys possessing optimum properties on wear resistances, heat resistance, weldability which can be used for development of technology of receiving from them powder compositions by atomization method are defined.

Keywords
wear resistance, friction coefficient, fretting corrosion, gas turbine engines, metalpowder compositions, hot strength alloys.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Tobar M.J., Amado J.M., Alvarez C. et al. Characteristics of Tribaloy T-800 and T-900 coatings on steel substrates by laser cladding // Surface and Coatings Technology. 2008. Vol. 202. P. 2297–2301.
  3. Petrik I.A., Perimilovskij I.A. Dalnejshee razvitie tehnologii uprochneniya bandazhnyh polok lopatok turbiny iz zharoprochnyh splavov [Further development of technology of hardening of bandage shelves of turbine blades from hot strength alloys ] // Tehnologicheskie sistemy. 2001. №3 (9). S. 90–92.
  4. Pejchev G.I., Zamkovoj V.E., Andrejchenko N.V. Sravnitelnye harakteristiki iznosostojkih splavov dlya uprochneniya bandazhnyh polok rabochih lopatok [Comparative characteristics of wear-resistant alloys for hardening of bandage shelves of working blades] // Aviacionno-kosmicheskaya tehnika i tehnologiya. 2010. №9 (76). S. 102–104.
  5. Dmitrieva G.P., Cherepova T.S., Kosorukova T.A., Nichiporenko V.I. Struktura i svojstva iznosostojkogo splava na osnove kobalta s karbidom niobiya [Structure and properties of wear-resistant alloy on the basis of cobalt with columbium carbide]// Metallofizika i novejshie tehnologii. 2015. T. 37. №7. S. 973–986.
  6. Migunov V.P., Chatynyan L.A., Ivanov E.V., Antonova G.S., Soloveva T.A. Iznosostojkie i antifrikcionnye materialy dlya uzlov treniya [Wearproof and antifriction materials for friction nodes] // Aviacionnaya promyshlennost. 1982. №8. S. 71–73.
  7. Pejchev G.I., Miloserdov A.B., Andrejchenko N.V. Issledovanie legkoplavkih evtektik v mikrostrukture iznosostojkogo splava HTN-61 [Research fusible eutectic in HTN-61 wear-resistant alloy microstructure] // Vestnik dvigatelestroeniya. 2012. №1. S. 211–214.
  8. Tihomirova T.V., Gajduk S.V. Issledovanie metodom CALPHAD vliyaniya otnosheniya volframa k kremniyu na fazovyj sostav i harakteristicheskie temperatury kobaltovogo splava [Research by the CALPHAD method of influence of the relation of tungsten to silicon on phase structure and characteristic temperatures of cobalt alloy] // Vestnik dvigatelestroeniya. 2014. №2. S. 206–210.
  9. Tihomirova T.V., Gajduk S.V., Belikov S.B. Issledovanie vliyaniya soderzhaniya nikelya na fazovyj sostav i harakteristicheskie temperatury kobaltovogo splava metodom CALPHAD [Research of influence of the nickel content on phase structure and characteristic temperatures of cobalt alloy the CALPHAD method] // Aviacionno-kosmicheskaya tehnika i tehnologiya. 2015. № 10. S. 45–48.
  10. Pejchev G.I., Zamkovoj V.E., Andrejchenko N.V. Razrabotka analoga iznosostojkogo splava HTN61 povyshennoj zharostojkosti dlya gazoturbinnyh dvigatelej [Development of analog of XTH61 wear-resistant alloy of the increased heat resistance for gas turbine engines] // Aviacionno-kosmicheskaya tehnika i tehnologiya. 2007. №8 (44). S. 11–13.
  11. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  12. Kablov E.N., Ospennikova O.G., Lomberg B.S. Strategicheskie napravleniya razvitiya konstrukcionnyh materialov i tehnologij ih pererabotki dlya aviacionnyh dvigatelej nastoyashhego i budushhego [The strategic directions of development of constructional materials and technologies of their processing for aircraft engines of the present and the future] // Avtomaticheskaya svarka. 2013. №10. S. 23–32.
  13. Evgenov A.G., Nerush S.V., Vasilenko S.A. Poluchenie i oprobovanie melkodispersnogo metallicheskogo poroshka vysokohromistogo splava na nikelevoj osnove primenitelno k lazernoj LMD-naplavke [The obtaining and testing of the fine-dispersed metal powder of the high-chromium alloy on nickel-base for laser metal deposition] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №5. St. 04. Available at: http://www.viam-works.ru (accessed: May 15, 2017). DOI: 10.18577/2307-6046-2014-0-5-4-4.
  14. Nerush S.V., Evgenov A.G., Ermolaev A.S., Rogalev A.M. Issledovanie melkodispersnogo metallicheskogo poroshka zharoprochnogo splava na nikelevoj osnove dlya lazernoj LMD-naplavki [Research of finely divided metal powder of hot strength alloy on nickel basis for laser LMD welding] // Voprosy materialovedeniya. 2013. №4 (76). S. 98–107.
  15. Nerush S.V., Evgenov A.G. Issledovanie melkodispersnogo metallicheskogo poroshka zharoprochnogo splava marki EP648-VI primenitelno k lazernoj LMD-naplavke, a takzhe ocenka kachestva naplavki poroshkovogo materiala na nikelevoj osnove na rabochie lopatki TVD [Research of fine-dispersed metal powder of the heat resisting alloy of the EP648-VI brand for laser metal deposition (LMD) and also the assessment quality of welding of powder material on the nickel basis on working blades THP] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №3. St. 01. Available at: http://www.viam-works.ru (accessed: May 15, 2017). DOI: 10.18577/2307-6046-2014-0-3-1-1.
  16. Kablov E.N., Evgenov A.G., Ospennikova O.G., Semenov B.I., Semenov A.B., Korolev V.A. Metalloporoshkovye kompozicii zharoprochnogo splava EP648 proizvodstva FGUP «VIAM» GNC RF v tehnologiyah selektivnogo lazernogo splavleniya, lazernoj gazoporoshkovoj naplavki i vysokotochnogo litya polimerov, napolnennyh metallicheskimi poroshkami [Metalpowder compositions of EP648 hot strength alloy of production of FSUE «VIAM» SRC RF in technologies of the selection laser fusing, laser gas of powder welding and high-precision molding of the polymers filled with metal powders] // Izvestiya vysshih uchebnyh zavedenij. Mashinostroenie. 2016. №9 (678). S. 62–80.
  17. Kablov E.N. Additivnye tehnologii – dominanta nacionalnoj tehnologicheskoj iniciativy [The additive technologies are the dominant of national technological initiative] // Intellekt i tehnologii. 2015. №2 (11). S. 52–55.
  18. Soloveva T.A., Zadyabina T.B., Buntushkin V.P. Primenenie iznoso- i zharostojkih splavov dlya uprochneniya lopatok GTD [Application wear and heat resisting alloys for hardening of blades of GTE] // Aviacionnaya promyshlennost. 1982. №8. S. 25–26.
  19. Farafonov D.P., Migunov V.P., Aleshina R.Sh. Issledovanie tribotehnicheskih harakteristik materialov, primenyaemyh dlya uprochneniya bandazhnyh polok rabochih lopatok turbin GTD [Tribotechnical characteristics research of materials used for gas turbine engines blade shroud hardening] // Aviacionnye materialy i tehnologii. 2016. № S1. S. 24–30. DOI: 10.18577/2071-9140-2016-0-S1-24-30.
  20. Farafonov D.P., Bazyleva O.A., Rogalev A.M. Splavy dlya uprochneniya bandazhnyh polok rabochih lopatok GTD [Alloys for blade shroud hardening] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №9. St. 07. Available at: http://www.viam-works.ru (accessed: May 15, 2017). DOI: 10.18577/2307-6046-2016-0-9-7-7.
  21. Sims C.T. Superalloys 1984 // TMS-AIME. 1984. P. 399.