Grigorenko V.B., Morozova L.V. Influence of conditions and use duration on degradation of structure of aluminum alloys of the type AMg4,5 and AMn // Proceedings of VIAM. 2017. No. 6 (54). Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2017-0-6-10-10.

Influence of conditions and use duration on degradation of structure of aluminum alloys of the type AMg4,5 and AMn

Grigorenko V.B., Morozova L.V.
Abstract

Complex research of products from AMg4,5 aluminum alloys and AMn after long-term operation for the purpose of identification of signs of degradation of material is conducted. Mechanical tests for assessment of strength properties of base material and welded seams, are carried out by methods of non-destructive testing, optical and scanning microscopy the material structure is investigated, the fractographic analysis of the destroyed samples is carried out. It is established that degradation signs at observance of operating conditions do not come to light.

Keywords
constructional aluminum alloys, fractographic, scanning electronic microscopy, strength, non-destructive testing, degradation of properties.
Reference list
  1. Beleckij V.M., Krivov G.A. Alyuminievye splavy (sostav, svojstva, tehnologiya, primenenie): spravochnik / pod obshh. red. I.N. Fridlyandera [Aluminum alloys (structure, properties, technology, application): directory / gen. ed. by I.N. Fridlyander]. Kiev: KOMINTEH, 2005. 365 s.
  2. Primenenie alyuminievyh splavov: spravochnik / M.B. Altman, G.N. Andreev, Yu.P. Arbuzov i dr. 2-e izd., pererab. i dop. [Application of aluminum alloys: directory / M.B. Altman, G.N. Andreev, Yu.P. Arbuzov et al. 2nd ed., rev. and add.]. M.: Metallurgiya, 1985. 344 s.
  3. Alyuminij: svojstva i fizicheskoe metallovedenie: spravochnik / pod red. Dzh. E. Hetcha. Per. s angl. [Aluminum: properties and physical metallurgical science: directory / ed. by J.E. Hetch. Trans from Engl.]. M.: Metallurgiya, 1989. 422 s.
  4. Sinyavskij V.S., Valkov V.D., Kalinin V.D. Korroziya i zashhita alyuminievyh splavov [Corrosion and protection of aluminum alloys]. M.: Metallurgiya, 1986. 368 s.
  5. Kozlova L.S., Sibileva S.V., Chesnokov D.V., Kutyrev A.E. Ingibitory korrozii (obzor) [Corrosion inhibitors (review)] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 67–75. DOI: 10.18577/2071-9140-2015-0-2-67-75.
  6. Korrozionnaya stojkost oborudovaniya himicheskih proizvodstv. Neftepererabatyvayushhaya promyshlennost: spravochnoe rukovodstvo / pod red. A.M. Suhotina, Yu.I. Archakova [Corrosion resistance of the equipment of chemical productions. Oil-processing industry: reference guide / ed. by A.M. Suhotin, Yu.I. Archakov]. L.: Himiya, 1990. 400 s.
  7. Kravchenko N.G., Petrova V.A. Opredelenie korrozionnoj agressivnosti aviacionnyh benzinov [Determination of aviation gasolines corrosion aggression] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №11 (47). St. 10. Available at: http://www.viam-works.ru (accessed: April 24, 2017). DOI: 10.18577/2307-6046-2016-0-11-10-10.
  8. Kutyrev A.E., Karimova S.A., Pavlovskaya T.G., Kuzin Ya.S. Issledovanie degradacii svojstv zashhitnyh kombinirovannyh pokrytij na alyuminievyh splavah s celyu razrabotki metodov prognozirovaniya ih srokov sluzhby [Research of properties degradation of protective combined coatings applied on aluminum alloys to develop methods of forecasting of their service life] //Aviacionnye materialy i tehnologii. 2015. №3 (36). S. 69–78. DOI: 10.18577/2071-9140-2015-0-3-69-78.
  9. Kablov E.N., Startsev O.V. Fundamentalnye i prikladnye issledovaniya korrozii i stareniya materialov v klimaticheskih usloviyah (obzor) [The basic and applied research in the field of corrosion and ageing of materials in natural environments (review)] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  10. Kurs M.G. Atmosfernaya korrozionnaya stojkost perspektivnyh Al–Li splavov pri provedenii naturno-uskorennyh ispytanij v usloviyah umerenno teplogo klimata [Atmospheric corrosion resistance of advanced Al–Li alloys by nature full-scale accelerated tests in the conditions of temperate warm climate] // Aviacionnye materialy i tehnologii. 2016. №2 (41). S. 88–94. DOI: 10.18577/2071-9140-2016-0-2-88-94.
  11. Rabkin D.M., Lozovskaya A.V., Sklabinskaya I.E. Metallovedenie svarki alyuminiya i ego splavov [Metallurgical science of welding of aluminum and its alloys]. Kiev: Naukova dumka, 1992. 160 s.
  12. Kablov E.N., Morozova L.V., Grigorenko V.B., Zhegina I.P., Fomina M.A. Issledovanie vliyaniya korrozionnoj sredy na process nakopleniya povrezhdenij i harakter razrusheniya konstrukcionnyh alyuminievyh splavov 1441 i V-1469 pri ispytaniyah na rastyazhenie i malociklovuyu ustalost [Research of influence of the corrosion environment on process of accumulation of damages and nature of destruction of structural aluminum alloys 1441 and V-1469 at tension tests and low-cyclic fatigue] // Materialovedenie. 2017. №1. S. 41–48.
  13. Morozova L.V., Zhegina I.P., Grigorenko V.B. Osobennosti deformacionnogo povedeniya splava V-1469 v usloviyah sovmestnogo vozdejstviya prilozhennoj nagruzki i korrozionno-aktivnoj sredy [Particular properties of deformation behavior of alloy V-1469 in conditions of joint influence of applied loading and active corrosion environment] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №9. St. 10. Available at: http://viam-works.ru (accessed: October 17, 2016). DOI: 10.18577/2307-6046-2016-0-9-10-10.
  14. Kurs M.G., Kutyrev A.E., Fomina M.A. Issledovanie korrozionnogo razrusheniya deformiruemyh alyuminievyh splavov pri laboratornyh i naturnyh ispytaniyah [Research of corrosion damage of wrought aluminium alloys at laboratory and full-scale tests] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №8 (44). St. 10. Available at: http://www.viam-works.ru (accessed: April 24, 2017). DOI: 10.18577/2307-6046-2016-0-8-10-10.
  15. Kablov E.N., Lukina E.A., Sbitneva S.V., Hohlatova L.B., Zajcev D.V. Formirovanie metastabilnyh faz pri raspade tverdogo rastvora v processe iskusstvennogo stareniya alyuminievyh splavov [Forming of metastable phases at disintegration of solid solution in the course of artificial aging of aluminum alloys] // Tehnologiya legkih splavov. 2016. №3. S. 7–17.
  16. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.