Nochovnaya N.A., Kochetkov A.S., Bokov K.A., Ivanov V.I. Research the characteristics of casting titanium superalloy VTI-4 // Proceedings of VIAM. 2017. No. 5 (53). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2017-0-5-2-2.

Research the characteristics of casting titanium superalloy VTI-4

Nochovnaya N.A., Kochetkov A.S., Bokov K.A., Ivanov V.I.
Abstract

The foundry characteristics of the VTI-4 intermetallic alloy have been determined for a vacuum arc furnace with a centrifugal casting of the melt into ceramic or metallic forms. It has been found that the VTI-4 intermetallic alloy has low casting characteristics in comparison with the VT5L alloy and Ti–16Al intermetallic alloy (mass. %): 40% more shrinkage, 44% less fluidity and 26–28% less fillability of the mold. The obtained casting characteristics of VTI-4 alloy can be used to develop an experimental foundry technology for the production of parts from it. The obtained casting characteristics of VTI-4 alloy can be used to develop an experimental foundry technology for the production of parts from it сomplex direction 7.1. «Intermetallic titanium alloys» («The strategic directions of development of materials and technologies of their processing for the period till 2030») [1]. The main trends and prospects in the field of development of new ortho alloys and technologies for their pr

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Tendencii i orientiry innovacionnogo razvitiya Rossii: sb. nauch.-inform. mater. 3-e izd., pererab. i dop. [Tendencies and reference points of innovative development of Russia: collection of scientific information materials. 3rd prod., rev. and add.]. M.: VIAM, 2015. 720 s.
  3. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] // Nauka i zhizn. 2010. №4. S. 2–7.
  4. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 01. Available at: http://www.viam-works.ru (accessed: March 02, 2017).
  5. Ilin A.A., Kolachev B.A., Polkin I.S. Titanovye splavy. Sostav, struktura, svojstva: spravochnik [Titanium alloys. Structure, structure, properties: directory]. M.: VILS–MATI, 2009. 520 s.
  6. Horev A.I., Nochovny N.A., Yakovlev A.L. Mikrolegirovanie redkozemelnymi metallami titanovykh splavov [Microalloying rare earth metals of titanium alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 206–212.
  7. Nochovnaya N.A., Panin P.V., Alekseev E.B., Bokov K.A. Ekonomnolegirovannye titanovye splavy dlya sloistyh metallopolimernyh kompozicionnyh materialov [Low-cost alloyed titanium alloys for metal-polymer laminates] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №11. St. 02. Available at: http://www.viam-works.ru (accessed: March 02, 2017). DOI: 10.18577/2307-6046-2014-0-11-2-2.
  8. Kablov D.E., Panin P.V., Shiryaev A.A., Nochovnaya N.A. Opyt ispolzovaniya vakuumno-dugovoj pechi ALD VAR L200 dlya vyplavki slitkov zharoprochnyh splavov na osnove aljuminidov titana [The use of ADL VAR L200 vacuum-arc furnace for ingots fabrication of high-temperature titanium aluminides base alloys] //Aviacionnye materialy i tehnologii. 2014. №2 (31). S. 27–33. DOI: 10.18577/2071-9140-2014-0-2-27-33.
  9. Skvorcova S.V., Filatov A.A., Dzunovich D.A., Panin P.V. Vliyanie soderzhaniya alyuminiya na deformiruemost' titanovyh splavov pri normalnoj temperature [Influence of the content of aluminum on deformability of titanium alloys at normal temperature] // Tehnologiya legkih splavov. 2008. №3. S. 40–45.
  10. Nochovnaya N.A., Panin P.V., Alekseev E.B., Bokov K.A. Sovremennye ekonomnolegirovannye titanovye splavy: primenenie i perspektivy razvitiya [Modern low-cost alloyed titanium alloys: application and development perspectives] // Metallovedenie i termicheskaya obrabotka metallov. 2016. №9 (735). S. 8–15.
  11. Nochovnaya N.A., Alekseev E.B., Yasinskij K.K., Kochetkov A.S. Specifika plavki i sposoby polucheniya slitkov intermetallidnyh titanovyh splavov s povyshennym soderzhaniem niobiya [Specifics of melting and ways of receiving ingots of intermetallidny titanium alloys with the raised content of niobium] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP2. S. 53–59.
  12. Nochovnaya N.A., Skvorcova S.V., Anishhuk D.S., Alekseev E.B., Panin P.V., Umarova O.Z. Otrabotka tehnologii opytnogo zharoprochnogo splava na osnove intermetallida Ti2AlNb [Working off of technology of pilot hot strength alloy on the basis of Ti2AlNb intermetallic compound] // Titan. 2013. №4 (42). S. 33–38.
  13. Alekseev E.B., Nochovnaya N.A., Skvorcova S.V., Panin P.V., Umarova O.Z. Opredelenie tehnologicheskih parametrov deformacii opytnogo zharoprochnogo splava na osnove intermetallida Ti2AlNb [Determination of technological parameters of deformation of pilot hot strength alloy on the basis of Ti2AlNb intermetallic compound] // Titan. 2014. №2 (44). S. 36–41.
  14. Alekseev E.B., Nochovnaya N.A., Panin P.V. Issledovanie struktury i fazovogo sostava opytnogo zharoprochnogo splava na osnove intermetallida Ti2AlNb v deformirovannom sostoyanii [Research of structure and phase composition of pilot hot strength alloy on the basis of Ti2AlNb intermetallic compound in the deformed condition] // Titan. 2014. №4 (46). S. 12–17.
  15. Alekseev E.B., Nochovnaya N.A., Ivanov V.I., Panin P.V., Novak A.V. Issledovanie vliyaniya alyuminiya na fazovyj sostav i termomehanicheskij rezhim izotermicheskoj shtampovki intermetallidnogo splava VTI-4 [Research of influence of aluminum on phase structure and thermomechanical mode of isothermal punching of intermetallic alloy VTI-4] // Tehnologiya legkih splavov. 2015. №1. S. 57–61.
  16. Alekseev E.B., Nochovnaya N.A., Panin P.V., Novak A.V. Tehnologicheskaya plastichnost, struktura i fazovyj sostav opytnogo titanovogo orto-splava, soderzhashhego 13% (po masse) alyuminiya [Technological plasticity, structure and phase composition of a pilot titanium ortho alloy with 13 wt. рct. aluminum] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №12. St. 08. Available at: http://www.viam-works.ru (accessed: March 02, 2017). DOI: 10.18577/2307-6046-2015-0-12-8-8.
  17. Nochovnaya N.A., Panin P.V., Alekseev E.B., Novak A.V. Issledovanie zakonomernostej formirovaniya strukturno-fazovogo sostoyaniya splavov na osnove orto- i gamma-alyuminidov titana v processe termomehanicheskoj obrabotki [Research of patterns of forming of structural and phase condition of alloys on basis ortho-and titanium gamma aluminides in the course of thermomechanical processing] // Vestnik RFFI. 2015. №1 (85). S. 18–26.