Skupov A.A., Ioda E.N., Panteleev M.D. New filler materials for welding of high-strength aluminum-lithium alloys // Proceedings of VIAM. 2016. No. 9 (45). Ст. 04. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-9-4-4.

New filler materials for welding of high-strength aluminum-lithium alloys

Skupov A.A., Ioda E.N., Panteleev M.D.
Abstract

Compositions of Al–Cu filler materials with additions of Sc, Hf, Nd, Ag to provide with improved resistance to hot cracking and mechanical properties of welding joints of high-strength aluminum-lithium alloys comparing with those obtained using the serial welding filler material SV-1201 are developed. It is shown that application of the developed filler materials is perspective for manufacturing welded structures and provides with increased operating reliability and durability.

Keywords
filler materials, welding, aluminum-lithium alloys, rare-earth metals, modification alloying of aluminum alloys.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Lukin V.I., Ospennikova O.G. Perspektivnye alyuminievye splavy i tehnologii ih soedineniya dlya izdelij aviakosmicheskoj tehniki [Perspective aluminum alloys and technologies of their connection for products of aerospace equipment] // Tez. dokl. 2-oj Mezhdunar. konf. «Alyuminij-21. Svarka i pajka». 2012. St. 8.
  3. Kablov E.N., Lukin V.I., Zhegina I.P., Ioda E.N., Loskutov V.M. Osobennosti i perspektivy svarki alyuminijlitievyh splavov [Features and perspectives of welding of aluminum lithium alloys] // Aviacionnye materialy i tehnologii. 2002. №4. S. 3–12.
  4. Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Alyuminievye deformiruemye splavy [Aluminum deformable alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
  5. Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
  6. Lukin V.I., Ioda E.N., Panteleev M.D., Skupov A.A. Vliyanie termicheskoj obrabotki na harakteristiki svarnyh soedinenij vysokoprochnyh alyuminijlitievyh splavov [Heat treatment influence on characteristics of welding joints of high-strength aluminum-lithium alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №4. St. 06. Available at: http://www.viam-works.ru (accessed: November 12, 2015). DOI: 10.18577/2307-6046-2015-0-4-6-6.
  7. Lukin V.I., Ospennikova O.G., Ioda E.N., Panteleev M.D. Svarka alyuminievyh splavov v aviakosmicheskoj promyshlennosti [Welding of aluminum alloys in the aerospace industry] // Svarka i diagnostika. 2013. №2. S. 47–52.
  8. Lukin V.I., Ioda E.N., Panteleev M.D., Skupov A.A., Ovchinnikov V.V. Svarka treniem s peremeshivaniem vysokoprochnyh alyuminij-litievyh splavov V-1461, V-1469 [Friction bonding with hashing high-strength aluminum-lithium alloys V-1461, V-1469] // Svarochnoe proizvodstvo. 2015. №7. S. 21–25.
  9. Nikiforov G.D. Metallurgiya svarki plavleniem alyuminievyh splavov [Metallurgy of fusion welding of aluminum alloys]. M.: Mashinostroenie, 1972. 164 s.
  10. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 01. Available at: http://www.viam-works.ru (accessed: February 18, 2015).
  11. Lukin V.I., Skupov A.A., Panteleev M.D., Gorelova L.P. Zavisimost svarivaemosti splavov sistemy Al–Mg (serii 5XXX) ot sootnosheniya legiruyushhih elementov (Sc, Zr i Mn) [Dependence of bondability of alloys of Al-Mg system (5XXX series) on ratio of doping elements (Sc, Zr and Mn)] // Svarka i Diagnostika. 2015. №4. S. 9–12.
  12. Lukin V.I., Skupov A.A., Panteleev M.D., Ioda E.N. Vliyanie dobavok skandiya na svarivaemost' alyuminievyh splavov sistemy Al–Mg [Influence of additives of scandium on bondability of aluminum alloys of Al-Mg system] // Svarka i diagnostika. 2016. №1. S. 13–15.
  13. Krupinski М., Labisz K., Dobranski L.A., Rdzawski Z. Derivative thermo analysis of the Al–Si cast alloy with addition of rare earths metals // Archives of Foundry Engineering. 2010. Vol. 10. P. 79–82.
  14. Wang Wen-tao, Zhang Xin-ming, Gao Zhi-guo, Jia Yu-zhen, Ye Ling-ying, Zheng Da-wei, Liu Ling. Influences of Ce addition on the microstructures and mechanical properties of 2519A aluminum alloy plate // Journal of Alloys and Compounds. 2010. No. 1–2. P. 366–371.
  15. Ivanova A.O., Vahromov R.O., Grigorev M.V., Senatorova O.G. Issledovanie vliyaniya malyh dobavok serebra na strukturu i svojstva resursnyh splavov sistemy Al–Cu–Mg [Effect of small additive of silver on structure and properties of Al–Cu–Mg alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №10. St. 01. Available at: http://www.viam-works.ru (accessed: January 25, 2016). DOI: 10.18577/2307-6046-2014-0-10-1-1.
  16. Mukhopadhyay A.K. and Reddy G.M. Influence of trace addition of Ag on the weldability of Al–Zn–Mg–Cu–Zr base 7010 alloy // Materials Science Forum. 2002. Vol. 396–402. P. 1665–1670.
  17. Ryabov D.K., Vakhromov R.O., Ivanova A.O. [An effect of small additions of elements with high solubility in aluminium on microstructure of ingots and cold-rolled sheets made of Al–Mg–Sc alloy] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №9. St. 05. Available at: http://www.viam-works.ru (accessed: January 25, 2016). DOI: 10.18577/2307-6046-2015-0-9-5-5
  18. Elagin V.I. Legirovanie deformiruemyh alyuminievyh splavov perehodnymi metallami [Alloying of deformable aluminum alloys transition metals]. M.: Metallurgiya, 1975. 248 s.
  19. Dric A.M., Ovchinnikov V.V. Rezultaty issledovanij svarivaemosti vysokoprochnyh splavov sistemy Al–Cu–Li–Mg, legirovannyh serebrom, skandiem i cirkoniem [Results of researches of bondability of high-strength alloys of the Al–Cu–Li–Mg system alloyed by silver, scandium and zirconium] // Tehnologiya legkih splavov. 2011. №1. S. 29–38.