Khaskov M.A. Water sorbtion by epoxy-based nanocomposites with carbon nanotubes in glassy and rubber states of polymer matrix // Proceedings of VIAM. 2016. No. 6 (42). Ст. 07. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-6-7-7.

Water sorbtion by epoxy-based nanocomposites with carbon nanotubes in glassy and rubber states of polymer matrix

Khaskov M.A.
Abstract

The sorption of water by epoxy-based nanocomposites with carbon nanotubes in glassy and rubber states of polymer matrix was studied. It was shown, that at sorption of water by polymer matrix in glassy state the addition of carbon nanotubes causes decreasing of both the average diffusion coefficient and water uptake. The hydrothermal aging above the glass transition temperature (Tg) of polymer matrix results in inverse correlation. It is suggested, that the lower water sorption below Tg originates from reduced cure degree of polymer matrix and enhanced rate of structural relaxation of nano-modified polymer causing «mobility freezing» of polymer chains and, as a result, decreasing of water diffusion coefficient in polymer matrix. Enhanced water sorption by nano-modified composite above Tg, originates, probably, from a bigger fraction of free volume in polymer matrix. Work is executed within implementation of the complex scientific directions 13.1. «Binding for polymeric and composite

Keywords
polymers, nanocomposites, carbon nanotubes, glass transition temperature, water sorption, hydrothermal aging.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Perspektivy ispolzovaniya uglerodsoderzhashhih nanochastic v svyazuyushhih dlya polimernyh kompozicionnyh materialov [Perspectives of use of carbon-containing nanoparticles in binding for polymeric composite materials] // Rossijskie nanotehnologii. 2013. T. 8. №3–4. S. 24–42.
  3. Chursova L.V., Kim M.A., Panina N.N., Shvetsov E.P. Nanomodificirovannoe epoksidnoe svyazuyushhee dlya stroitelnoj industrii [Nanomodified epoxy binder for the construction industry] // Aviacionnye materialy i tehnologii. 2013. №1. S. 40–47.
  4. Gunyaev G.M., Kablov E.N., Aleksashin V.M. Modificirovanie konstrukcionnyh ugleplastikov uglerodnymi nanochasticami [Modifying constructional carbon of plastics carbon nanoparticles] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 5–11.
  5. Corcione C.E., Frigione M. Characterization of Nanocomposites by Thermal Analysis // Materials. 2012. V. 5. P. 2960–2980.
  6. Urvanov S.A., Haskov M.A., Alshevskij Yu.L., Karaeva A.R., Mordkovich V.Z., Bejlina N.Yu. Uglerodnye niti, kombinirovannye fullerenami i dlinnomernymi nanotrubkami [The carbon threads combined by fullerenes and lengthy nanotubes] // Izvestiya vysshih uchebnyh zavedenij. Ser.: Himiya i himicheskaya tehnologiya. 2013. T. 56. №7. S. 116–119.
  7. Kumar M.S.S., Raju N.M.S., Sampath P.S., Jayakumari L.S. Effects of nanomaterials on polymer composites – an expatiate view // Reviews on Advanced Materials Science. 2014. V. 38. P. 40–54.
  8. Njuguna J., Pielichowski K., Alcock J.R. Epoxy-Based Fibre Reinforced Nanocomposites: Current Status // Advanced Engineering Materials. 2007. V. 9. №10. P. 835–847.
  9. Karak N. Vegetable Oil-Based Polymers: Properties, Processing and Applications. Cambridge: Woodhead Publishing Limited. 2012. 612 p.
  10. Haskov M.A., Ahmadieva K.R., Kudryavceva A.N., Grebeneva T.A. Vliyanie fullerena S60 na kinetiku otverzhdeniya termoreaktivnyh svyazuyushhih na osnove jepoksidnyh smol [Influence of C60 fullerene on kinetics of curing thermosetting binding on the basis of epoxies] // Kompozity i nanostruktury (v pechati).
  11. Harris P.J.F. Carbon nanotube composites // International Materials Reviews. 2004. V. 49. №1. P. 31–43.
  12. Bolshakov V.A., Kondrashov S.V., Merkulova Y.I., Dyachkova T.P., Yurkov G.Y., Ilyichyov F.V. Issledovanie svojstv nanomodificirovannyh uglekompozitov do i posle termovlazhnostnogo stareniya [Research of nanomodified carbon composites before and after hydrothermal aging] //Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 61–66.
  13. Haskov M.A. O specifike opredeleniya temperatury steklovaniya vlagonasyshhennyh polimernyh kompozicionnyh materialov metodom dinamicheskogo mehanicheskogo analiza [About specifics of determination of glass transition temperature of vlagonasyshchenny polymeric composite materials method of the dynamic mechanical analysis] // Zavodskaya laboratoriya (v pechati).
  14. Efimov V.A., Shvedkova A.K., Korenkova T.G., Kirillov V.N. Issledovanie polimernyh konstrukcionnyh materialov pri vozdejstvii klimaticheskih faktorov i nagruzok v laboratornyh i naturnyh usloviyah [Research of polymeric constructional materials at influence of climatic factors and loadings in laboratory and natural conditions] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №1. St. 05. Available at: http://www.viam-works.ru (accessed: December 22, 2015).
  15. Kablov E.N., Startsev O.V. Fundamentalnye i prikladnye issledovanija korrozii i starenija materialov v klimaticheskih uslovijah (obzor) [The basic and applied research in the field of corrosion and ageing of materials in natural environments (review)] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  16. Kablov E.N., Kirillov V.N., Zhirnov A.D., Startsev O.V., Vapirov Yu.M. Centry dlya klimaticheskih ispytanij aviacionnyh PKM [The centers for climatic tests of aviation PCM] // Aviacionnaya promyshlennost. 2009. №4. S. 36–46.
  17. Komorowski J.P. Hydrothermal effects in continuous fibre reinforced composites. Part II: Physical properties // Aeronautical note NEA-AN-10. 1983. V. 22700. P. 1–56.
  18. Walter H., Shirangi H., Dermitzaki E., Wunderle B., Michel B. Study on the Effect of Moisture and Elevated Temperature on the Fracture Properties of Visco Elastic Polymers // Proceedings of the 12-th International Conference on Fracture. Ottawa. 2009. P. 1775–1783.
  19. Lee S.G., Choi J.I., Koh W., Jang S.S., Kim J., Kim G. Effect of Temperature on Water Molecules in a Model Epoxy Molding Compound: Molecular Dynamics Simulation Approach // IEEE Transactions On Components, Packaging And Manufacturing Technology. 2011. V. 1. №10. P. 1533–1542.
  20. Enns J.B., Gillham J.K. Effect of the extent of cure on the modulus, glass transition, water absorption, and density of an amine-cured epoxy // Journal of Applied Polymer Science. 1983. V. 28. №9. P. 2831–2846.
  21. Li L., Yu Y., Su H., Zhan G., Li S., Wu P. The Diffusion Mechanism of Water Transport in Amine-Cured Epoxy Networks // Applied Spectroscopy. 2010. V. 64. № 4. P. 458–465.
  22. Efimov V.A., Shvedkova A.K., Korenkova T.G., Kirillov V.N. Issledovanie polimernyh konstrukcionnyh materialov pri vozdejstvii klimaticheskih faktorov i nagruzok v laboratornyh i naturnyh usloviyah [Investigation of polymer composite materials under effect of climatic factors and loads in laboratory and environmental conditions] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 68–73.
  23. Lucas J.P., Zhou J. Moisture Interaction Characteristics and Fracture in Polymer Compo-sites // Proceedings of the Tenth International Conference on Composite Materials (ICCM-10). Canada. 1995. P. VI-247–VI-255.
  24. Starkova O., Chandrasekaran S., Prado L.A.S.A., Tölle F., Mülhaupt R., Schulte K. Hydrothermally resistant thermally reduced graphene oxide and multi-wall carbon nanotube based epoxy nanocomposites // Polymer Degradation and Stability. 2013. V. 98. P. 519–526.
  25. Pan M., Zhang C., Liu B., Mu J. Dielectric and Thermal Properties of Epoxy Resin Nanocomposites Containing Polyhedral Oligomeric Silsesquioxane // Journal of Materials Science Research. 2013. V. 2. №1. P. 153–162.
  26. Zulfli N.H.M., Bakar A.A., Chow W.S. Mechanical and water absorption behaviors of carbon nanotube reinforced epoxy/glass fiber laminates // Journal of Reinforced Plastics and Composites November. 2013. V. 32. №22. P. 1715–1721.
  27. Barkoula N.M., Paipetis A., Matikas T., Vavouliotis A., Karapappas P., Kostopoulos V. Environmental degradation of carbon nanotube-modified composite laminates: a study of electrical resistivity // Mechanics of Composite Materials. 2009. V. 45. №1. P. 21–32.
  28. Mir I.A., Kumar D. Carbon nanotube-filled conductive adhesives for electronic applica-tions // Nanoscience Methods. 2012. V. 1. P. 183–193.
  29. Ma P.-C., Siddiqui N.A., Marom G., Kim J.-K. Dispersion and functionalization of carbon nanotubes for polymer-based nanocomposites: A review // Composites Part A: Applied Science and Manufacturing. 2010. V. 41. №10. P. 1345–1367.
  30. Haskov M.A., Grebeneva T.A., Babin A.N. Vliyanie dobavok uglerodnyh nanotrubok na kinetiku otverzhdeniya jepoksidnyh smol do i posle zasteklovyvaniya [Influence of additives of carbon nanotubes on kinetics of curing of epoxies before glass transformation] // Kompozity i nanostruktury. 2014. T. 6. №1. S. 49–64.
  31. Crank J. The mathematics of diffusion. Oxford: Clarendon Press, 1975. 414 p.
  32. Liu W., Hoa S.V., Pugh M. Water uptake of epoxy–clay nanocomposites: Experiments and model validation // Composites Science and Technology. 2008. V. 68. №9. P. 2066–2072.
  33. Panin S.V., Startsev O.V., Krotov A.S. Diagnostika nachalnoj stadii klimaticheskogo stareniya PKM po izmeneniyu koefficienta diffuzii vlagi [Initial stage environmental degradation of the polymer matrix composites evaluated by Water diffusion coefficient] // Trudy VIAM : electron. nauch.-tehnich. zhurn. 2014. №7. St. 09. Available at: http://viam-works.ru (accessed: December 22, 2015). DOI: 10.18577/2307-6046-2014-0-7-9-9.
  34. Kablov E.N., Starcev O.V., Panin S.V. Vlagoperenos v ugleplastike s destruktirovannoj poverhnostyu [Moisture transfer in coal to plastics with destructured surface] // Doklady akademii nauk. 2015. T. 461. №2. S. 433–436.
  35. Klopffer M.H., Flaconnèche B. Transport Properties of Gases in Polymers: Bibliographic Review // Oil & Gas Science and Technology – Rev. IFP. 2011. V. 56. №3. P. 223–244.
  36. Shen C.-H., Springer G.S. Moisture Absorption and Desorption of Composite Materials // Journal of composite materials. 1976. V. 10. P. 2–20.
  37. Wei C., Srivastava D., Cho K. Thermal Expansion and Diffusion Coefficients of Carbon Nanotube-Polymer Composites // Nano Letters. 2002. V. 2. №6. P. 647–650.
  38. Fox T. G., Loshaek S. J. Influence of Molecular Weight and Degree of Crosslinking of the Specific Volume and Glass Temperature of Polymers // Journal of Polymer Science. 1955. V. 15. №80.
  39. P. 371–390.
  40. Pascault J.P., Sautereau H., Verdu J. et al. Thermosetting polymers. N-Y.: Marcel Dekker AG, 2002. 477 р.
  41. McCallum C.L., Bandosz T.J., McGrother S.C., Müller E. A., Gubbins K.E. A Molecular Model for Adsorption of Water on Activated Carbon: Comparison of Simulation and Experi-ment // Langmuir. 1999. V. 15. P. 533–544.
  42. Haskov M.A., Bolshakov V.A., Merkulova Yu.I., Grebeneva T.A. Vliyanie uglerodnyh na-notrubok na kineticheskie aspekty otverzhdeniya termoreaktivnyh svyazuyushhih na primere jepoksidnyh smol [Influence of carbon nanotubes on kinetic aspects of curing of thermosetting binding epoxies on example] // Izvestiya vysshih uchebnyh zavedenij. Ser.: Himiya i himicheskaya tehnologiya. 2015. T. 58. №7. S. 58–62.
  43. Blank W.J., He Z.A., Picci M. Catalysis of the epoxy-carboxyl reaction // Journal of Coatings Technology. 2002. V. 74. №926. P. 33–41.