Goundobin N.V., Titov V.I., Pilipenko L.V. Determination of low niobium content ( 0,01–0,1 wt.%) in high-strength steel // Proceedings of VIAM. 2016. No. 6 (42). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-6-3-3.

Determination of low niobium content ( 0,01–0,1 wt.%) in high-strength steel

Goundobin N.V., Titov V.I., Pilipenko L.V.
Abstract

Determination of low niobium content (0,01–0,1 wt. %) in the alloys having in their composition a large amount of alloying elements (which obstruct this determination), is a difficult task. Such types of alloys as steels, especially high-strength, are constantly subjected to modifications of their chemical composition to give them new properties, such as those associated with the impact toughness at various temperatures, lower thermal coefficient of linear expansion, temperature of hot forming and others. Niobium in small amounts (less than 0,9 wt. %) is added to various kinds of steel (chromium-nickel, high-strength, corrosion-resistant, high-strength welded, cemented, etc.). To control the low niobium content (0,01 wt. % higher) in high-strength steels with high accuracy (about 10% rel.) a method of spectrophotometric determination of niobium with reagent sulfochlorophenol C was developed. Niobium was preconcentrated at zirconium collector which was used in the course of analysis

Keywords
methods, niobium, optical density, relative error, reagent sulfochlorophenol C, collector (zirconium), spectrophotometry, high-strength steel, phenylarsonic acid.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Prioritetnye napravleniya razvitiya tehnologij proizvodstva zharoprochnyh materialov dlya aviacionnogo dvigatelestroeniya [The priority directions of development of production technologies of heat resisting materials for aviation engine building] // Problemy chernoj metallurgii i materialovedeniya. 2013. №3. S. 47–54.
  3. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  4. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlya vysokoteplonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for the high-heatloaded details of gas turbine engines] // Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 13–19.
  5. Shmotin Yu.N., Starkov R.Yu., Danilov D.V., Ospennikova O.G., Lomberg B.S. Novye materialy dlya perspektivnogo dvigatelya OAO «NPO „Saturn”» [New materials for the perspective engine of JSC «NPO „Saturn”»] // Aviacionnye materialy i tehnologii. 2012. №2. S. 6–8.
  6. Kablov E.N. Materialy dlya izdeliya «Buran» – innovacionnye resheniya formirovaniya shestogo tehnologicheskogo uklada [Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  7. Tonysheva O.A., Voznesenskaja N.M., Shalkevich A.B., Petrakov A.F. Issledovanie vlijanija vysokotemperaturnoj termomehanicheskoj obrabotki na strukturu, tehnologicheskie, mehanicheskie i korrozionnye svojstva vysokoprochnoj korrozionnostojkoj stali pere-hodnogo klassa s povyshennym soderzhaniem azota [Research of influence of high-temperature thermomechanical processing on structure, technological, mechanical and corrosion properties of high-strength corrosion-resistant steel of transitional class with the raised content of nitrogen] // Aviacionnye materialy i tehnologii. 2012. №3. S. 31–36.
  8. Tonysheva O.A., Voznesenskaya I.M., Eliseev E.A., Shalkevich A.B. Novaya vysokoprochnaya ekonomnolegirovannaya azotsoderzhashchaya stal povyshennoj nadezhnosti [The new high-strength containing steel of increased reliability economically alloyed nitrogen] //Aviacionnye materialy i tehnologii. 2012. №S. S. 84–88.
  9. Netesov V.M., Bereznyak P.A., Ozhigov L.S., Handak V.V. Vliyanie mikrolegirovaniya na martensitnoe prevrashhenie i svojstva reaktornyh stalej [Influence of microalloying on the martensite transformation and property reactor steels] // Voprosy atomnoj nauki i tehniki. 2003. №6. S. 24–27.
  10. Gibalo I.M. Analiticheskaya himiya niobiya i tantala [Analytical chemistry of niobium and tantalum]. M.: Nauka, 1967. 352 s.
  11. Elinson S.V. Novye fotometricheskie metody opredeleniya niobiya i tantala v metallah i splavah [New photometric methods of definition of niobium and tantalum in metals and alloys] // Sovremennye metody analiza materialov. M.: Metallurgiya, 1969. S. 3–17.
  12. Elinson S.V. Spektrofotometriya niobiya i tantala [Niobium and tantalum spectrophotometry]. M.: Atomizdat, 1973. 288 s.
  13. Gundobin N.V., Titov V.I., Pilipenko L.V., Dvoreckov R.M. Spektrofotometricheskoe opredelenie niobiya v zharoprochnyh nikelevyh splavah, soderzhashhih tantal [Spektrofotometric definition niobium in the heat resisting nickel alloys containing tantalum] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №8. St. 10. Available at: http://www.viam-works.ru (accessed: November 18, 2015). DOI: 10.18577/2307-6046-2014-8-10-10.
  14. Marchenko Z.N. Fotometricheskoe opredelenie jelementov [Photometric definition of elements]. M.: Mir, 1971. S. 276–282.
  15. Elinson S.V., Petrov K.I. Analiticheskaya himiya cirkoniya i gafniya [Analytical chemistry of zirconium and hafnium]. M.: Nauka, 1965. 267s.
  16. Savvin S.B., Propiscova A.L., Ohanova A.N. Sulfonitrofenol M – novyj reagent na palladij, niobij i drugie jelementy [Sulfonitrophenol M – new reagent on palladium, niobium and other elements] // Analiticheskaya himiya AN SSSR. 1969. T. 24. Vyp. 11. S. 1634–1641.