Kondrashov S.V., Shashkeev K.A., Popkov O.V., Solovyanchik L.V. Mechanical properties of CNT nanocomposites (review) // Proceedings of VIAM. 2016. No. 5 (41). Ст. 08. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-5-8-8.

Mechanical properties of CNT nanocomposites (review)

Kondrashov S.V., Shashkeev K.A., Popkov O.V., Solovyanchik L.V.
Abstract

A review of publications on polymer CNT nanocomposites mechanical properties is presented. A model of the polymer-CNT system using the Mori–Tanaka method is described. Mechanical properties of CNT- nanocomposites are shown to be mainly defined by the CNT distribution within the polymer matrix, not the intrinsic properties of nanotubes. CNT-containing systems based on polyamide and polycarbonate are thoroughly reviewed. Data on the effect of impurities size on mechanical properties of nanocomposites prepared by melt blending are provided. Data on the effect of CNTs on epoxy binders are provided. Nanotubes are shown to affect the degree of conversion during epoxy composite curing, nanocomposite glass point and matrix structure at the boundary layer near CNTs. Effect of functionalized and non-functionalized CNTs on mechanical properties of epoxy nanocomposites is considered. Work is executed within implementation of the complex scientific direction 15 « Nanostructured, amorphous mat

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Iijima S. Helical microtubules of graphitic carbon // Nature. 1991. V. 354. Р. 56–58.
  3. Thostenson E.T., Ren Z., Chow T.W. Advances in the science and technology of carbon nanotube and their composites: a review // Compos. Sci. Technol. 2001. V. 61. Р. 1899–1912.
  4. Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Prospects of using carbonaceous nanoparticles in binders for polymer composites // Russian nanotechnologies. 2013. V. 8. Issue 3–4. P. 163–185.
  5. Kablov E.N. Konstrukcionnye i funkcionalnye materialy – osnova jekonomicheskogo i nauchno-tehnicheskogo razvitiya Rossii [Constructional and functional materials – basis of economic and scientific and technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64–67.
  6. Kislyakov P.P., Hohlov Yu.A., Krynin A.G., Kondrashov S.V. Poluchenie i primenenie polimernoj plenki s prozrachnym elektroprovodyashhim pokrytiem na osnove oksida indiya, legirovannogo olovom [Receiving and application of polymer film with transparent electroconducting coating on the basis of the indium oxide alloyed by tin] // Trudy VIAM : elektron. nauch.-tenhich. zhurn. 2013. №11. St. 06. Available at: http://viam-works.ru (accessed at: September, 15 2015).
  7. Yurkov G.Yu., Kondrashov S.V., Kraev I.D. Nanokompozity na osnove polijetilena vysokogo davleniya i nanochastic kobal'ta: sintez, struktura i svojstva [Nanocomposites based on high-density polyethylene and cobalt nanoparticles: synthesis, structure and properties] // Aviacionnye materialy i tehnologii. 2014. №S2. S. 29–33.
  8. Akatenkov R.V., Anoshkin I.V., Belyaev A.A., Bitt V.V., Bogatov V.A., Dyachkova T.P., Kutsevich K.E., Kondrashov S.V., Romanov A.M., Shirokov V.V., Horobrov N.V. Vliyanie strukturnoj organizacii uglerodnyh nanotrubok na radiojekraniruyushhie i elektroprovodyashhie svojstva nanokompozitov [Influence of the structural organization of carbon nanotubes on radio shielding and electrocarrying-out properties of nanocomposites] // Aviacionnye materialy i tehnologii. 2011. №1. S. 35–42.
  9. Akatenkov R.V., Kondrashov S.V., Fokin A.S., Marahovskij P.S. Osobennosti formirovaniya polimernyh setok pri otverzhdenii jepoksidnyh oligomerov s funkcializovannymi nanotrubkami [Features of forming of polymeric grids when curing epoxy oligomers with functionalizing nanotubes] // Aviacionnye materialy i tehnologii. 2011. №2. S. 31–37.
  10. Gunyaev G.M., Kablov E.N., Aleksashin V.M. Modificirovanie konstrukcionnyh ugleplastikov uglerodnymi nanochasticami [Modifying constructional ugleplastikov carbon nanoparticles] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 5–11.
  11. Perepelkin K.E. Armiruyushhie volokna i voloknistye polimernye kompozity [Reinforcing fibers and fibrous polymeric composites]. SPb.: Izd-vo NOT, 2009. 379 s.
  12. Barber A.H., Cohen S.R., Wagner H.D. Measurement of carbon nanotube-polymer interfacial strength // Appl Phys Lett. 2003. V. 82 (23). Р. 4140–4142.
  13. Haque A., Ramasetty A. Theoretical study of stress transfer in carbon nanotube reinforced polymer matrix composites // Composite Structures. 2005. V. 71 (1). Р. 68–77.
  14. Fisher F.T., Bradshaw R.D., Brinson L.C. Fiber waviness in nanotube-reinforced polymer composites – I: Modulus predictions using effective nanotube properties // Composites Science and Technology. 2003. V. 63. Р. 1689–1703.
  15. Andrews R., Jacques D., Minot M., Rantell T. Fabrication of carbon multiwalled nanotube/polymer composites by shear mixing // Macromolecular Materials and Engineering. 2002.
  16. V. 287 (6). Р. 395–403.
  17. Shi D.-Li., Feng X.-Q., Huang Y.Y., Hwang K.Ch., Gao H. The Effect of Nanotube Waviness and Agglomeration on the Elastic Property of Carbon Nanotube-Reinforced Composites // Journal of engineering materials and technology. 2004. V. 126. P. 250–257.
  18. Mori T., Tanaka K. Average Stress in Matrix and Average Elastic Energy of Materials With Misfitting Inclusions // Acta Metall. 1973. V. 21. P. 571–574.
  19. Pegel S., Potschke P., Petzold G., Alig I., Dudkin S.M., Lellinger D. Dispersion, agglomeration, and network formation of multi walled carbon nanotubes in polycarbonate melts // Polymer. 2008. V. 49. P. 974–984.
  20. Villmow T., Kretzschmar B., Pötschke P. Influence of screw configuration, residence time, and specific mechanical energy in twin-screw extrusion of polycaprolactone/multi-walled carbon nanotube composites // Composites Science and Technology. 2010. V. 70. P. 2045–2055.
  21. Kasaliwal G.R., Pegel S., Göldel A., Pötschke P., Heinrich G. Analysis of agglomerate dispersion mechanisms of multiwalled carbon nanotubes during melt mixing in polycarbonate // Polymer. 2010. V. 51. P. 2708–2720.
  22. Chen L., Pang X.J., Yu Z.-L. Study on polycarbonate/multi-walled carbon nanotubes composite produced by melt processing // Materials Science and Engineering. A. 2007. V. 457. P. 287–291.
  23. Mack C., Sathyanarayana S., Weiss P., Mikonsaari I., Hübner C., Henningand F., lsner P.E.
  24. Twin-screw extrusion of multiwalled carbon nanotubes reinforced polycarbonate composites: Investigation of electrical and mechanical properties // IOP Conf. Ser.: Mater. Sci. Eng. 2012.
  25. DOI: 10.1088/1757-899X/40/1/012020.
  26. Pardo S.G., Arboleda L., Ares A., Garc X., Dopico S., Abad M.J. Toughening Strategies of Carbon Nanotube/Polycarbonate Composites with Electromagnetic Interference Shielding Properties // Polymer Composites. 2013. V. 34. №11. P. 1938–1949.
  27. Eitan A., Fisher F.T., Andrews R., Brinson L.C., Schadler L.S. Reinforce mentmechanisms in MWCNT-filled polycarbonate // Composites Science and Technology. 2006. V. 66. P. 1159–1170.
  28. Man Y.H., Liand Z.C., Zhang Z.J. Interface-Dependent Mechanical Properties in MWNT-Filled Polycarbonate // Materials Transactions. 2009. V. 50. №6. P. 1355–1359.
  29. Chin Y.-Ch. Design and Fabrication of Transparent Polycarbonate/Carbon Nanotube Composite Films // Electronic Theses, Treatises and Dissertations. 2007. Paper 3811.
  30. Meincke O., Kaempfer D., Weickmann H., Friedrich C., Vathauer M., Warth H. Mechanical properties and electrical conductivity of carbon-nanotube filled polyamide-6 and its blends with acrylonitrile/butadiene/styrene // Polymer. 2004. V. 45. P. 739–748.
  31. Li J., Fang Zh., Tong L., Gu A., Liu F. Improving Dispersion of Multiwalled Carbon Nanotube sin Polyamide 6 Composites Through Amino-Functionalization // Journal of Applied Polymer Science. 2007. V. 106. P. 2898–2906.
  32. Liu H., Wang X., Fang P., Wang Sh., Qi X., Pan Ch., Xie G., Liew K.M. Functionalization of multi-walled carbon nanotubes grafted with self-generated functional groups and their polyamide
  33. 6 composites // Carbon. 2010. V. 48. P. 721–729.
  34. Ferreira T., Paiva M.C., Pontes A.J. Dispersion of carbon nanotubes in polyamide 6 for microinjection moulding // J. Polym Res. 2013. V. 20. P. 301.
  35. Paiva M., Simon F., Novais R., Ferreira T., Proença M., Xu W., Besenbacher F. Controlled Functionalization of Carbon Nanotubes by a Solvent-free Multicomponent Approach // ACSNano. 2010. V. 4 (12). P. 7379–7386.
  36. Nasir M., Mohammad I., Asad H., Shaukat S., Ahmad N.Kh. Polyamide-6-based composites reinforced with pristine or functionalized multi-walled carbon nanotubes produced using melt extrusion technique // Journal of Composite Materials. 2014. V. 48. №10. P. 1197–1207.
  37. Nasir M., Mohammad I., Asad H., Shaukat S. Polyamide 6/Multiwalled Carbon Nanotubes Nanocomposites with Modified Morphology and Thermal Properties // Polymers. 2013. V. 5.
  38. P. 1380–1391.
  39. Tager A.A. Fiziko-himiya polimerov / pod red. A.A. Askadskogo. 4-e izd., pererab. i dop. [Fiziko-himiya polymers / ed. by A.A.Askadsky. 4th ed, processed and added] M.: Nauchnyj mir, 2007. 573s.
  40. Xiao K.Q., Zhang L.C., Zarudi I. Mechanical and rheological properties of carbon nanotube-reinforced polyethylene composites // Composites Science and Technology. 2007. V. 67. P. 177–182.
  41. Prashantha K., Soulestin J., Lacrampe M.F., Krawczak P., Dupin G., Claes M. Masterbatch-based multi-walled carbon nanotube filled polypropylene nanocomposites: Assessment of rheological and mechanical properties // Composites Science and Technology. 2009. V. 69. P. 1756–1763.
  42. Siochi E.J., Working D.C., Park C., Lillehei P.T., Rouse J.H., Topping C.C., Bhattacharyya A.R., Kumar S. Melt processing of SWCNT-polyimide nanocomposite fibers // Compos. Part B: Eng. 2004. V. 35. P. 439–446.
  43. Irzhak V.I. Epoksidnye kompozicionnye materialy s uglerodnymi nanotrubkami [Epoxy composite materials with carbon nanotubes] // Uspehi himii. 2011. T. 80. №8. S. 821–840.
  44. Zhuang G.S., Sui G.X., Sun Z.S., Yang R. Pseudoreinforcement Effect of Multiwalled Carbon Nanotubes in Epoxy Matrix Composites // Journal of Applied Polymer Science. 2006. V. 102.
  45. P. 3664–3672.
  46. Liang Z., Gou J., Zhang C., Wang B., Kramer L. Investigation of molecular interactions between (10, 10) single-walled nanotube and Epon 862 resin/DETDA curing agent molecules // Materials Science and Engineering. A. 2004. V. 365. Issue 1–2. P. 228–234.
  47. Puglia D., Valentini L., Kenny J.M. Analysis of the Cure Reaction of Carbon Nanotubes/Epoxy Resin Composites Through Thermal Analysis and Raman Spectroscopy // Journal of Applied Polymer Science. 2003. V. 88. P. 452–458.
  48. Valentini L., Armentano I., Puglia D., Kenny J.M. Dynamics of amine functionalized nanotubes/epoxy composites by dielectric relaxation spectroscopy // Carbon. 2004. V. 42. P. 323–329.
  49. Zhou T., Wangaand X., Wang T. Cure reaction of multi-walled carbon nanotubes/diglycidylether of bisphenol A/2-ethyl-4-methylimidazole (MWCNTs/DGEBA/EMI-2,4) nanocomposites: effect of carboxylic functionalization of MWCNTs // Polym Int. 2009. V. 58. P. 445–452.
  50. Bae J., Jang J., Yoon S.-H. Cure Behavior of the Liquid-Crystalline Epoxy/Carbon Nanotube System and the Effect of Surface Treatment of Carbon Fillers on Cure Reaction // Macromol. Chem. Phys. 2002. V. 203. P. 2196–2204.
  51. Byun J., Kim D.S. Curing Behavior and Physical Properties of Epoxy Nanocomposites Comprising Amine-Functionalized Carbon Nanofillers // Polymer Composites. 2010. V. 31. №8. P. 1449–1456.
  52. Visco A.M., Calabrese L., Milone C. Cure Rate and Mechanical Properties of a DGEBF Epoxy Resin Modified with Carbon Nanotubes // Journal of Reinforced Plastics and Composites. 2009. V. 28. №8. P. 937–949.
  53. Xie H., Liu B., Sun Q., Yuan Z., Shen J., Cheng R. Cure Kinetic Study of Carbon Nanofibers/Epoxy Composites by Isothermal DSC // Journal of Applied Polymer Science. 2005. V. 96. P. 329–335.
  54. Xie H., Liu B., Yuan Z., Shen J., Cheng R. Cure Kinetics of Carbon Nanotube/Tetrafunctional Epoxy Nanocomposites by Isothermal Differential Scanning Calorimetry // Journal of Polymer Science. Part B: Polymer Physics. 2004. V. 42. №20. P. 3701–3712.
  55. Zhoua T., Wanga X., Zhub H., Wang T. Influence of carboxylic functionalization of MWCNTs on the thermal properties of MWCNTs/DGEBA/EMI-2,4 nanocomposites // Composites. Part A. 2009. V. 40. P. 1792–1797.
  56. Tseng Ch.H., Wang Ch.-Ch., Chen Ch.-Y. Functionalizing Carbon Nanotubes by Plasma Modification for the Preparation of Covalent-Integrated Epoxy Composites // Chem. Mater. 2007. V. 19.
  57. P. 308–315.
  58. Kim L.T., Kim H.-Ch., Kim S.-K., Kathi J. 2,3-Aminopropyltriethoxysilane Effect on Thermal and Mechanical Properties of Multi-walled Carbon Nanotubes Reinforced Epoxy Composites // Journal of Composite Materials. 2009. V. 43. №22. P. 2533–2541.
  59. Wang Sh., Liang R., Wang B., Zhang Ch. Covalent Addition of Diethyltoluenediamines Onto Carbon Nanotubes for Composite Application // Polymer Composites. 2009. V. 30. №8. P. 1050–1057.
  60. Wang Sh., Liang Zh., Liu T., Wang B., Zhang Ch. Effective amino-functionalization of carbon nanotubes for reinforcing epoxy polymer composites // Nanotechnology. 2006. V.17. P. 1551–1557.
  61. Thakre P.R., Bisrat Y., Lagoudas D.C. Electrical and Mechanical Properties of Carbon Nanotube-Epoxy Nanocomposites // Journal of Applied Polymer Science. 2010. V. 116. P. 191–202.
  62. Zhou Y.X., Wu P.X., Cheng Z.-Y., Ingram J., Jeelani S. Improvement in electrical, thermal and mechanical properties of epoxy by filling carbon nanotube // eXPRESS Polymer Letters. 2008.
  63. V. 2. №1. P. 40–48.
  64. Zhou Y., Pervin F., Lewis L., Jeelani Sh. Experimental study on the thermal and mechanical properties of multi-walled carbon nanotube-reinforced epoxy // Materials Science and Engineering. A. 2007. V. 452–453. P. 657–664.
  65. Miyagawa H., Rich M.J., Drzal L.T. Thermo-physical properties of epoxy nanocomposites reinforced by carbon nanotubes and vapor grown carbon fibers // Thermochimica Acta. 2006. V. 442.
  66. P. 67–73.
  67. Allaoui A., Baia S., Cheng H.M., Baia J.B. Mechanical and electrical properties of a MWNT/epoxy composite // Composites Science and Technology. 2002. V. 62. P. 1993–1998.
  68. Valentini L., Puglia D., Carniato F., Boccaleri E., Marchese L., Kenny J.M. Use of Plasma Fluorinated Single-walled Carbon Nanotubes for the Preparation of Nanocomposites with Epoxy Matrix // Composites Science and Technology. 2008. V. 68. P. 1008–1014.
  69. Hernandez-Perez A., Aviles F., May-Pat A., Valadez-Gonzalez A., Herrera-Franco P.J., Bartolo-Perez P. Effective properties of multiwalled carbon nanotube/epoxy composites using two different tubes // Composites Science and Technology. 2008. V. 68. P. 1422–1431.
  70. Gojny F.H., Schulte K. Functionalization effect on the thermo-mechanical behavior of multi-wall carbon nanotube/epoxy-composites // Composites Science and Technology. 2004. V. 64.
  71. P. 2303–2308.
  72. Shen J., Huang W., Wu L., Hu Y., Ye M. The reinforcement role of different amino-functionalized multi-walled carbon nanotubes in epoxy nanocomposites // Composites Science and Technology. 2007. V. 67. P. 3041–3050.
  73. Shen J., Huang W., Wu L., Hu Y., Ye M. Thermo-physical properties of epoxy nanocomposites reinforced with amino-functionalized multi-walled carbon nanotubes // Composites. Part A. 2007. V. 38. P. 1331–1336.
  74. Lau K., Lu M., Lam Ch., Cheung H., Sheng F.-L., Li H.-L. Thermal and mechanical properties of single-walled carbon nanotube bundle-reinforced epoxy nanocomposites: the role of solvent for nanotube dispersion // Composites Science and Technology. 2005. V. 65. P. 719–725.
  75. Loos M.R., Pezzin S.H., Amico S.C., Bergmann C.P., Coelho L.A.F. The matrix stiffness role on tensile and thermal properties of carbon nanotubes/epoxy composites // J. Mater. Sci. 2008. V. 43.
  76. P. 6064–6069.
  77. Zhuang G.S., Sui G.X., Sun Z.S., Yang R. Pseudoreinforcement Effect of Multiwalled Carbon Nanotubes in Epoxy Matrix Composites // Journal of Applied Polymer Science. 2006. V. 102.
  78. P. 3664–3672.
  79. Geng Y., Liu M.Y., Li J., Shi X.M., Kim J.K. Effects of surfactant treatment on mechanical and electrical properties of CNT/epoxy nanocomposites //Composites. Part A. 2008. V. 39.
  80. P. 1876–1883.
  81. Kim J.A., Seong D.G., Kang T.J., Youn J.R. Effects of surface modification on rheological and mechanical properties of CNT/epoxy composites // Carbon. 2006. V. 44. P. 1898–1905.
  82. Moniruzzaman M., Du F., Romero N., Winey K.I. Increased Flexural Modulus and Strength in SWNT / Epoxy Composites by a New Fabrication Method // Department of Materials Science & Engineering. Papers (MSE). 2006.
  83. Liao Y.-H., Marietta-Tondin O., Liang Zh., Zhang Ch., Wang B. Investigation of the dispersion process of SWNTs/SC-15 epoxyresin nanocomposites // Materials Science and Engineering. A. 2004.
  84. V. 385. P. 175–181.
  85. Xie H., Liu B., Yuan Z., Shen J., Cheng R. Cure Kinetics of Carbon Nanotube/Tetrafunctional Epoxy Nanocomposites by Isothermal Differential Scanning Calorimetry // Journal of Polymer Science. Part B: Polymer Physics. 2004. V. 42. P. 3701–3712.
  86. Allaoui A., Bounia N.E. How carbon nanotubes affect the cure kinetics and glass transition temperature of their epoxy composites? // eXPRESS Polymer Letters. 2009. V. 3. №9. P. 588–594.
  87. Chow W.Sh., Tan P.L. Epoxy/Multiwall Carbon Nanotube Nanocomposites Prepared By Sonication and Planetary Mixing Technique // Journal of Reinforced Plastics and Composites. 2010. V. 29. №15. P. 2331–2342.
  88. Ji A.F., Dyu Dzh., Tuliss M.D. Uprochnenie epoksidnyh smol [Hardening of epoxies] // Polimernye smesi. SPb.: Izd-vo NOT, 2009. T. 2. Funkcionalnye svojstva / pod red. D.R. Pola, K.B. Baknella. 605 s.
  89. Kunz-Douglass S., Beaumont P.W.R., Ashby M.F. A model for the toughness of epoxy-rubber particulate composites // J. Mater. Sci. 1980. V. 15. P. 1109–1123.