Evteev A.А. Some aspects of development of optimal firing conditions for ceramic compositions containing eutectic additives // Proceedings of VIAM. 2016. No. 2 (38). Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-2-12-12.

Some aspects of development of optimal firing conditions for ceramic compositions containing eutectic additives

Evteev A.А.
Abstract

The methods used to analyze the regularities of thermally activated processes are discribed. It is shown that the most informative and reliable methods are the isothermal methods. The data on the initial components and their conversion ways to experimental samples in the technological scheme are presented. In the example of alumina materials modified with various amounts of various eutectic additives it was found that the sintering process obeys the equation of the first order kinetics formal. The apparent activation energy of sintering and initial patterns for the development of optimum firing mode of the materials are determined.

Keywords
alumina ceramics, sintering, sintering adds, eutectics, kinetic parameters, firing conditions.
Reference list
  1. Kablov E.N., Shchetanov B.V., Abuzin Tu.A., Ivahnenko Yu.A. Metallicheskie i keramicheskie kompozicionnye materialy [Metal and ceramic composite materials] / V sb. materialov Mezhdunarodnoj nauch.-praktich. konf. «Sovremennye tehnologii – klyuchevoe zveno v vozrozhdenii otechestvennogo aviastroeniya». T. 1. Kazan. 2008. S. 181–188.
  2. Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solntsev S.S. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Perspective high-temperature ceramic composite materials] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.
  3. Kablov E.N., Shhetanov B.V., Ivahnenko Yu.A., Balinova Yu.A., Semenova E.V. Volokna dioksida cirkoniya dlya novogo pokoleniya materialov aviacii i kosmosa [Zirconium dioxide fibers for new generation of materials of aircraft and space] / V sb. materialov XXV Mezhdunarodnoj konf. «Kompozicionnye materialy v promyshlennosti». Yalta. 2005. S. 320–323.
  4. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  5. Shchetanov B.V., Balinova Yu.A., Lyulyukina G.Yu., Soloveva E.P. Struktura i svojstva nepreryvnyh polikristallicheskih volokon α-Al2O3 [Structure and properties of continuous polycrystalline fibers α-Al2O3] // Aviacionnye materialy i tehnologii. 2012. №1. S. 13–17.
  6. Kirienko T.A., Balinova Yu.A. Fiziko-himicheskie svojstva mnogokomponentnyh rastvorov dlya keramicheskih materialov, soderzhashhih polivinilovyj spirt [Physical and chemical properties of multicomponent solutions for ceramic materials containing polyvinyl alcohol] // Aviacionnye materialy i tehnologii. 2014. №1. S. 34–38.
  7. Varrik N.M., Ivahnenko Yu.A., Maksimov V.G Oksid-oksidnye kompozicionnye materialy dlya gazoturbinnyh dvigatelej (obzor) [Oxide-oxide composites for gas-turbine engines] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №8. St. 03. Available at: http://www.viam-works.ru (accessed: July 20, 2015). DOI: 10.18577/2307-6046-2014-0-8-3-3.
  8. Balinova Yu.A., Lyulyukina G.Yu., Kirienko T.A., Arakcheeva L.V. Svojstva promyshlennogo silikazolya i vozmozhnost ego dorabotki dlya izgotovleniya alyumosilikatnyh materialov [Properties industrial silicasoly and possibility of its completion for manufacturing of silica-alumina materials] // Steklo i keramika. 2013. №12. S. 33–36.
  9. Evteev A.A., Lemeshev D.O., Zhitnyuk S.V., Makarov N.A. Keramika v sisteme ZrO2–Al2O3 s dobavkami jevtekticheskih sostavov [Ceramics in ZrO2-Al2O3 system with additives of evtektichesky structures] // Steklo i keramika. 2011. №8. S. 23–27.
  10. Evteev A.A., Lemeshev D.O., Makarov N.A. Osobennosti spekanija keramiki v sisteme oksid alyuminiya–dioksid cirkoniya s dobavkami jevtekticheskih sostavov [Features of agglomeration of ceramics in system aluminum-zirconium dioxide oxide with additives of evtectic structures] // Tehnika i tehnologiya silikatov. 2013. №4. S. 2–8.
  11. Evteev A.A., Makarov N.A. Nanostrukturirovannye energoeffektivnye keramicheskie materialy na osnove oksida alyuminiya i dioksida cirkoniya [The nanostructured power effective ceramic materials on the basis of aluminum oxide and zirconium dioxide] / V kataloge XII Vserossijskoj vystavki nauch.-tehnich. tvorchestva molodezhi. 2012.
  12. Gropyanov V. M., Nemec I. I., Bessmertnyj V. S., Krohin V.P. Neizotermicheskie metody kinetiki v tehnologii keramiki [Nonisothermal methods of kinetics in technology of ceramics]. Belgorod: BTISM im. I. A. Grishmanova, 1984. S. 3–17.
  13. Gropyanov V. M., Abbakumov V. G., Drozdeckaya G. V. Raschet energii aktivacii po dannym neizotermicheskoj kinetiki [Activation energy calculation according to nonisothermal kinetics] // Izvestiya vuzov SSSR. Ser. «Himiya i himicheskaya tehnologiya». 1976. T. 19. Vyp. 7. S. 1054.
  14. Gropyanov V. M., Abbakumov V. G. Integralnye metody analiza neizotermicheskoj kinetiki [Integral methods of the analysis of nonisothermal kinetics] // Izvestiya vuzov SSSR. Ser. «Himiya i himicheskaya tehnologiya». 1979. T. 22. Vyp. 2. S. 178.
  15. Ivensen V. A. Fenomenologiya spekaniya i nekotorye voprosy teorii [Phenomenology of agglomeration and some questions of the theory]. M.: Metallurgiya, 1985. 248 s.