Probabilistic assessment of results reliability of monolithic CFRP structures ultrasonic non-destructive testing by phased arrays
Abstract
The research results and curves built on the developed mathematical algorithm of probability detection of defects by their size and also the comparative analysis of testing results reliability by using the ultrasonic phased arrays and single element piezoelectric convertor are shown. It is shown that probability of defect detection for ultrasonic testing of the monolithic CFRP structures by phased array technique is considerably higher than by using traditional piezoelectric transducers.
Keywords
CFRP, non-destructive testing, ultrasonic technique, phased arrays, probability of defect detection.
Reference list
- Kablov E.N. Aviatsionnoe materialovedenie v XXI veke. Perspektivy i zadachi [Aviation materials science in the XXI century. Perspectives and tasks] // Aviaсionnye materialy. Izbrannye trudy «VIAM» 1932–2002. M., 2002. S. 23–47.
- Kablov E.N. Konstruktsionnye i funktsionalnye materialy – osnova ekonomicheskogo i nauchno-tekhnicheskogo razvitiya Rossii [Constructional and functional materials – basis of economic and scientific and technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64–67.
- Merkulova Yu.I., Muhametov R.R. Nizkovyazkoe epoksidnoe svyazuyushhee dlya pererabotki metodom vakuumnoj infuzii [Development of a low-viscosity epoxy binder for processing by vacuum infusion] // Aviacionnye materialy i tehnologii. 2014. №1. S. 39–41.
- Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazuyushhie dlya perspektivnykh metodov izgotovleniya konstruktsionnyh voloknistykh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] // Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
- Dushin M.I., Khrulkov A.V., Platonov A.A., Akhmadieva K.R. Bezavtoklavnoe formovanie ugleplastikov na osnove prepregov, poluchennykh po rastvornoj tehnologii [Out-of-autoclave formation carbon plastics on the basis of the prepregs received on solution technology] // Aviacionnye materialy i tehnologii. 2012. №2. S. 43–48.
- Boychuk A.S. Nerazrushayushchiy kontrol detaley i konstruktsiy aviatsionnoy tekhniki iz polimernykh kompozitsionnykh materialov pri ispolzovanii ultrazvukovykh fazirovannykh reshetok [Non-destructive testing of details and designs of aviation engineering from polymeric composite materials when using the ultrasonic phased grids] // Tez. dokl. 19-y Vseros. nauch.-tekhnich. konf. po nerazrushayushchemu kontrolyu i tekhnicheskoy diagnostike. Samara, 2011. S. 289–291.
- Boychuk A.S., Generalov A.S., Dalin M.A., Stepanov A.V. Kontrol tekhnologicheskikh i ekspluatatsionnykh narusheniy sploshnosti ploskikh paneley iz polimernykh kompozitsionnykh materialov pri ispolzovanii ultrazvukovykh fazirovannykh reshetok [Control of technological and operating disturbances of continuity of flat panels from polymeric composite materials when using the ultrasonic phased grids] // Tez. dokl. Vseros. konferentsii po ispytaniyam i issledovaniyam materialov «TestMat-2012». M.: VIAM, 2012. S. 6.
- Boychuk A.S., Generalov A.S., Dalin M.A., Stepanov A.V. Nerazrushayushchiy kontrol tekhnologicheskikh narusheniy sploshnosti T-obraznoy zony integralnoy konstruktsii iz PKM s ispolzovaniem ultrazvukovykh fazirovannykh reshetok [Non-destructive testing of technological violations of continuity of the Tee zone of integral design from PCM with use of the ultrasonic phased grids] // Vse materialy. Entsiklopedicheskiy spravochnik. 2012. №10. S. 38–44.
- Boychuk A.S., Generalov A.S., Lozhkova D.S., Stepanov A.V. Kontrol T-obraznykh zon stringera iz PKM s ispolzovaniem ultrazvukovykh fazirovannykh reshetok [Control of Tee zones of stringer from PCM with use of the ultrasonic phased grids] // Radioelektronika, elektrotekhnika i energetika: tez. dokl. 18-y Mezhdunar. nauch.-tekhnich. konf. studentov i aspirantov. M., 2012. T. 2. S. 127–128.
- Boychuk A.S., Generalov A.S., Stepanov A.V. Yukhatskova O.V. Nerazrushayushchiy kontrol PKM s ispolzovaniem ultrazvukovykh fazirovannykh reshetok [Non-destructive testing of PCM with use of the ultrasonic phased grids] // Promyshlennye ASU i kontrollery. 2013. №2. S. 54–58.
- Boychuk A.S., Stepanov A.V, Kosarina E.I., Generalov A.S. Primenenie tehnologii ultrazvukovyh fazirovannyh reshetok v nerazrushayushhem kontrole detalej i konstruktsij aviacionnoj tehniki, izgotavlivaemyh iz PKM [Application of ultrasonic phased lattice technique for nondestructive testing of aviation FRP parts structures] // Aviacionnye materialy i tehnologii. 2013. №2. S. 41–46.
- Boychuk A.S., Generalov A.S., Stepanov A.V. Nondestructive testing of FRP by using phased array ultrasonic technology // Application of Contemporary Non-Destructive Testing in Engineering: abstracts of the 12th International Conference of the Slovenian Society for Non-Destructive Testing. Portorož, Slovenia. September 4–6, 2013.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Boychuk A.S., Generalov A.S., Lozhkova D.S., Stepanov A.V. Otsenka veroyatnosti obnaruzheniya defektov v ugleplastikakh pri ultrazvukovoy defektoskopii s ispolzovaniem fazirovannykh reshetok [Assessment of probability of detection of defects in ugleplastikakh at ultrasonic defects scope with use of the phased grids] // Radioelektronika, elektrotekhnika i energetika: tez. dokl. 19-y Mezhdunar. nauch.-tekhnich. konf. studentov i aspirantov. M.: MEI, 2013. T. 2. S. 106.
- Boychuk A.S., Generalov A.S., Dalin M.A., Stepanov A.V. Veroyatnostnaya otsenka dostovernosti rezultatov ultrazvukovogo nerazrushayushchego kontrolya konstruktsiy iz PKM, primenyaemykh v aviatsionnoy promyshlennosti [Probabilistic assessment of reliability of results of ultrasonic non-destructive testing of designs from PCM applied in the aviation industry] // Remont. Vosstanovlenie. Modernizatsiya. 2013. №9. S. 36–40.