Ponomarenko D.A., Skugorev A.V., Sidorov S.A., Shpagin A.S. Influence of heat exchange between workpiece and die on forming process of aerospace parts by special isothermal presses // Proceedings of VIAM. 2016. No. 10 (46). Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-10-3-3.

Influence of heat exchange between workpiece and die on forming process of aerospace parts by special isothermal presses

Ponomarenko D.A., Skugorev A.V., Sidorov S.A., Shpagin A.S.
Abstract

The forming process of aerospace parts by special isothermal hydraulic presses of 6,3 and 16 MN with additional technical equipment is considered. Technological capabilities of their effective use for manufacturing parts of various typical sizes from Titanium-based, Nickel – based and other alloys in air environment using ZhS6U cast alloy dies are shown. Influence of low-speed forming in various temperature gradients between workpiece and die on power parameters of forging, forming process of workpieces and their structure changes are studied. The article presents the possibility of using the heat exchange between workpiece and die to improve deformation process. The work is executed within implementation of the complex scientific direction 10.2. «Isothermal deformation on air of heterophased difficult-to-form superalloys of new generation» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Keywords
isothermal presses, heat deformation, deformation rate, heat exchange, titanium-based alloys, nickel-based superalloys, temperature conditions, temperature gradient, force stats, forming process, structure changes.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Ponomarenko D.A., Moiseev N.V., Skugorev A.V. Shtampovka diskov GTD iz zharoprochnykh splavov na izotermicheskikh pressakh [Punching of disks GTD from hot strength alloys on isothermal presses] // Aviacionnye materialy i tekhnologii. 2013. №1. S. 13–16.
  3. Ponomarenko D.A., Moiseev N.V., Skugorev A.V. Effektivnaya tehnologiya izgotovleniya diskov GTD iz zharoprochnyh nikelevyh splavov [Effective manufacturing techniques of disks GTE from heat resisting nickel alloys] // Kuznechno-shtampovochnoe proizvodstvo. Obrabotka materialov davleniem. 2013. №10. S. 13–17.
  4. Lomberg B.S., Bakradze M.M., Chabina E.B., Filonova E.V. Vzaimosvyaz struktury i svojstv vysokozharoprochnykh nikelevykh splavov dlya diskov gazoturbinnykh dvigatelej [Interrelation of structure and properties of high-heat resisting nickel alloys for disks of gas turbine engines] // Aviacionnye materialy i tekhnologii. 2011. №2. S. 25–30.
  5. Razuvaev E.I., Lebedev D.Yu., Bubnov M.V. Formirovanie ultramelkozernistoj i nanorazmernoj struktury v metallah i splavah metodami deformacii [Forming of ultrafine grained and nanodimensional structure in metals and alloys deformation methods] // Aviacionnye materialy i tehnologii. 2010. №3. S. 3–8.
  6. Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Prioritetnye napravleniya razvitiya tehnologij proizvodstva zharoprochnyh materialov dlya aviacionnogo dvigatelestroeniya [The priority directions of development of production technologies of heat resisting materials for aviation engine building] // Problemy chernoj metallurgii i materialovedeniya. 2013. №3. S. 47–54.
  7. Razuvaev E.I., Moiseev N.V., Kapitanenko D.V., Bubnov M.V. Sovremennye tehnologii obrabotki metallov davleniem [Modern technologies of plastic working of metals] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №2. St. 03. Available at: http://www.viam-works.ru (accessed: September 10, 2015). DOI: 10.18577/2307-6046-2015-0-2-3-3.
  8. Kishkin S.T. Sozdanie, issledovanie i primenenie zharoprochnyh splavov: izbrannye tr. (K 100-letiyu so dnya rozhdeniya) [Creation, research and application of hot strength alloys: chosen works (To the 100 anniversary)]. M.: Nauka, 2006. 407 s.
  9. Savushkin A.N., Kashapov O.S., Golynec S.A. Vliyanie skorosti nagruzheniya na mehanicheskie svojstva zharoprochnyh titanovyh splavov [An influence of loading rate on mechanical properties of heat-resistant titanium alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 04. Available at: http://www.viam-works.ru (accessed: September 10, 2015). DOI: 10.18577/2307-6046-2015-0-3-4-4.
  10. Kablov E.N. Aviacionnoe materialovedenie v XXI veke. Perspektivy i zadachi [Aviation materials science in the XXI century. Perspectives and tasks] // Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002: yubilejnyj nauch.-tehnich. sb. M.: MISIS–VIAM, 2002. S. 23–47.
  11. Kashapov O.S., Novak A.V., Nochovnaya N.A., Pavlova T.V. Sostoyanie, problemy i perspektivy sozdaniya zharoprochnyh titanovyh splavov dlya detalej GTD [Condition, problems and perspectives of creation of heat resisting titanium alloys for GTE details] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №3. St. 02. Available at: http://www.viam-works.ru (accessed: September 10, 2015).
  12. Skugorev A.V., Burhanova A.A., Nochovnaya N.A., Izotova A.Yu. Effektivnost primeneniya izotermicheskoj deformacii pri izgotovlenii shtampovok iz titanovyh splavov [Efficiency of application of isothermal deformation when manufacturing punchings from titanium alloys] // Titan. 2013. №1 (39). S. 31–34.
  13. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlya aviacionnogo dvigatelestroeniya [Creation of modern heat resisting materials and technologies of their production for aviation engine building] // Krylya Rodiny. 2012. № 3–4. S. 34–38.
  14. Kablov E.N., Golubovskij E.R. Zharoprochnost nikelevyh splavov: ucheb. posobie [Thermal stability of nickel alloys: manual]. M.: Mashinostroenie, 1998. 464 s.
  15. Bakradze M.M., Ovsepyan S.V., Shugaev S.A., Letnikov M.N. Vliyanie rezhimov zakalki na strukturu i svojstva shtampovok diskov iz zharoprochnogo nikelevogo splava EK151-ID [The influence of quenching on structure and properties nickel-based superalloy EK151-ID forgings] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №9. St. 01. Available at: http://www.viam-works.ru (accessed: September 10, 2015).
  16. Kablov E.N., Ospennikova O.G., Lomberg B.S. Kompleksnaya innovacionnaya tehnologiya izotermicheskoj shtampovki na vozduhe v rezhime sverhplastichnosti diskov iz superzharoprochnyh splavov [Complex innovative technology of isothermal punching on air in mode of superplasticity of disks from superhot strength alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 129–141.