Buyakina A.A., Letnikov M.N., Bakradze M.M., Shugaev S.A. The effect of thermomechanical and heat treatment parameters on structure and mechanical properties of superalloy VZH177 // Proceedings of VIAM. 2016. No. 10 (46). Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2016-0-10-2-2.

The effect of thermomechanical and heat treatment parameters on structure and mechanical properties of superalloy VZH177

Buyakina A.A., Letnikov M.N., Bakradze M.M., Shugaev S.A.
Abstract

The effect of parameters of thermomechanical and heat treatment on microstructure and phase composition change of alloy at all the stages of flat forgings production of new superalloy VG177 including ingot homogenization, isothermal forging and heat treatment is studied. The comparative tests results of tensile strength, impact strength and high-temperature strength are presented. The effect of long high temperature exposures simulating operation time on microstructure and mechanical properties of the item is investigated.

Keywords
Ni-base superalloy, homogenizing, isothermal forging, heat treatment, mechanical properties.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Ospennikova O.G., Lomberg B.S. Strategicheskie napravleniya razvitiya konstrukcionnyh materialov i tehnologij ih pererabotki dlya aviacionnyh dvigatelej nastoyashhego i budushhego [The strategic directions of development of constructional materials and technologies of their processing for aircraft engines of the present and the future] // Avtomaticheskaya svarka. 2013. №10. S. 23–32.
  3. Kablov E.N., Ospennikova O.G., Lomberg B.S. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlya aviacionnogo dvigatelestroeniya [Creation of modern heat resisting materials and technologies of their production for aviation engine building] // Krylya Rodiny. 2012. №3–4. S. 34–38.
  4. Locq D., Caron (Onera) P. On Some Advanced Nickel-Based Superalloys for Disk Applications // High Temperature Materials AL03-01. 2011. November. Issue 3. P. 1–9.
  5. Huron E.S., Bain K.R., Mourer D.P., Gabb T.Р. Development of High Temperature Capability P/M Disk Superalloys // Superalloys-2008, TMS. 2008. P. 181–189.
  6. Gabb T.P., Gayda J., Telesman J. Thermal and Mechanical Property Characterization of the Advanced Disk Alloy // NASA/TM-2005-213645. June, 2005.
  7. Gabb T.Р., Gayda J., Telesman J., Kantzos P.T. Realistic Subscale Evaluations of the Mechanical Properties of Advanced Disk Superalloys // NASA/TM-2003-212086. January, 2003.
  8. Kablov E.N., Ospennikova O.G., Lomberg B.S. Kompleksnaya innovacionnaya tehnologiya izotermicheskoj shtampovki na vozduhe v rezhime sverhplastichnosti diskov iz superzharoprochnyh splavov [Complex innovative technology of isothermal punching on air in mode of superplasticity of disks from superhot strength alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 129–141.
  9. Tian G., Zou J., Wang Y., Wang W. Hot Deformation Behaviors and Microstructure Evolution in a New PM Nickel-Base Superalloy // Advanced Materials Research. 2011. Vol. 278. P. 411–416.
  10. Ponomarenko D.A., Moiseev N.V., Skugorev A.V. Effektivnaya tehnologiya izgotovleniya diskov GTD iz zharoprochnyh nikelevyh splavov [Effective manufacturing techniques of disks GTD from heat resisting nickel alloys] // Kuznechno-shtampovoe proizvodstvo. 2013. №10. S. 13–17.
  11. Filonova E.V., Bakradze M.M., Kochubey A.Ya., Vavilin N.L. Issledovanie izmenenij strukturno-fazovogo sostoyaniya splava VZh175 v processe goryachej deformacii i termicheskoj obrabotki [Structural-phase evolution of VZH175-alloy during hot deformation and heat treatment] // Aviacionnye materialy i tehnologii. 2014. №3. S. 10–13. DOI: 10.18577/2071-9140-2014-0-3-10-13.
  12. Lomberg B.S., Bakradze M.M., Chabina E.B., Filonova E.V. Vzaimosvyaz struktury i svojstv vysokozharoprochnykh nikelevykh splavov dlya diskov gazoturbinnykh dvigatelej [Interrelation of structure and properties of high-heat resisting nickel alloys for disks of gas turbine engines] // Aviacionnye materialy i tehnologii. 2011. №2. S. 25–30.
  13. Ovsepyan S.V., Lomberg B.S., Bakradze M.M., Letnikov M.N. Termicheskaya obrabotka deformiruemyh zharoprochnyh nikelevyh splavov dlya diskov GTD [Thermal processing of deformable heat resisting nickel alloys for disks GTE] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP2. S. 122–130.
  14. Gayda J. Alloy 10: A 1300F Disk Alloy // NASA/TM-2000-210358. August, 2000.
  15. Gabb T.P., Gayda J., Kantzos P. The Grain Size-Temperature Response of Advanced Nickel-Base Disk Superalloys During Solution Heat Treatments // NASA/TM-2007-214912. December, 2007.
  16. Ovsepyan S.V., Lomberg B.S., Alalyikin A.A., Gerasimov D.E., Gromova A.A. Methods of structure preparing of superalloy for disc turbin applications for superplastic deformation // Material Science Forum. 1994. Vol. 170–172. P. 305–310.
  17. Sharpe H.J., Saxena A. Effect of Microstructure on High-Temperature Mechanical Behavior of Nickel-Base Superalloys for Turbine Disc Applications // EuroSuperalloys-2010 / Advanced Materials Research. 2011. Vol. 278. P. 259–264.
  18. Zharoprochnyj deformiruemyj splav na osnove nikelya i izdelie, vypolnennoe iz etogo splava: pat. 2280091 Ros. Federaciya [Heat resisting deformable alloy on the basis of nickel and the product executed from this alloy: pat. 2280091 Rus. Federation]; zayavl. 21.12.04; opubl. 20.07.06.