Murashov V.V., Laptev A.S. Contact liquids for creation of an acoustic contact at ultrasonic control of multi-layer structures from PCM // Proceedings of VIAM. 2015. No. 8. Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-8-10-10.

Contact liquids for creation of an acoustic contact at ultrasonic control of multi-layer structures from PCM

Murashov V.V., Laptev A.S.
Abstract

Ultrasonic methods of non-destructive testing and technical diagnostics, which require application of contact liquids for creation of an acoustic contact between the converter of a test device and the product under control are described. Three groups of contact liquids are considered. The contact liquid MBG-1 based on aqueous solution of polyvinyl alcohol offered by VIAM was investigated. Results of pilot studies of methods to remove the contact liquid after the control procedure are given

Reference list
  1. Kablov E.N. Kontrol' kachestva materialov – garantija bezopasnosti jekspluatacii aviacionnoj tehniki [Quality control of materials – security accreditation of operation of aviation engineering] //Aviacionnye materialy i tehnologii. 2001. №1. S. 3–8.
  2. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] //Nauka i zhizn'. 2010. №4. S. 2–7.
  3. Lukina N.F., Dement'eva L.A., Petrova A.P., Serezhenkov A.A. Konstrukcionnye i termostojkie klei [Constructional and heat-resistant glues] //Aviacionnye materialy i tehnologii. 2012. №S. S. 328–335.
  4. Petrova A.P., Lukina N.F. Klei dlja mnogorazovoj kosmicheskoj sistemy [Glues for reusable space system] //Trudy VIAM. 2013. №4. St. 04 (viam-works.ru).
  5. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  6. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  7. Smith R.A., Nelson L.J. et al. Automation of control and estimation of parameters of defects in parts of the PCM //Insight. 2009. V. 51. №2. Р. 82–87.
  8. Murashov V.V., Mishurov K.S. Ocenka prochnostnyh harakteristik ugleplastikov akusticheskim metodom [Assessment of strength characteristics ugleplastikov acoustic method] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 81–85.
  9. Murashov V.V. Opredelenie fiziko-mehanicheskih harakteristik i sostava polimernyh kompozicionnyh materialov akusticheskimi metodami [Definition of physicomechanical characteristics and composition of polymeric composite materials acoustic methods] //Aviacionnye materialy i tehnologii. 2012. №S. S. 465–475.
  10. Murashov V.V., Rumjancev A.F. Defektoskopija i diagnostika polimernyh kompozicionnyh materialov akusticheskimi metodami [Defektoskopiya and diagnostics of polymeric composite materials by acoustic methods] /V kn. 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Jubilejnyj nauch.-tehnich. sb. M.: VIAM. 2007. S. 342–347.
  11. Murashov V.V. K voprosu opredelenija uprugih i prochnostnyh svojstv polimernyh kompozicionnyh materialov akusticheskim kompleksnym metodom [To question of determination of elastic and strength properties of polymeric composite materials acoustic complex method] //Deformacija i razrushenie materialov. 2014. №11. S. 39–45.
  12. Bobrov V.T., Rozlovenko S.G., Murashov V.V. Materials characterization //Testing. Diagnostics. 2010. №2. P. 42–44.
  13. Murashov V.V., Kosarina E.I., Generalov A.S. Kontrol' kachestva aviacionnyh detalej iz polimernyh kompozicionnyh materialov i mnogoslojnyh kleenyh konstrukcij [Quality control of aviation details from polymeric composite materials and multi-layer kleeny designs] //Aviacionnye materialy i tehnologii. 2013. №3. S. 65–70.
  14. Murashov V.V. Kontrol' mnogoslojnyh kleenyh konstrukcij akustiko-teplovym metodom [Control of multi-layer kleeny designs by akustiko-thermal method] //Klei. Germetiki. Tehnologii. 2014. №9. S. 36–40.
  15. Murashov V.V. Nerazrushajushhij kontrol' kleevyh soedinenij [Non-destructive testing of glued joints] //Klei. Germetiki. Tehnolo-gii. 2008. №7. S. 21–28.
  16. Murashov V.V. Opredelenie sostava i plotnosti konstrukcionnyh ugleplastikov lazerno-akusticheskim sposobom ul'trazvukovogo kontrolja [Definition of structure and density constructional ugleplastikov in the laser and acoustic way of ultrasonic control] //Materialovedenie. 2014. №11. S. 24–29.
  17. Nagem R.J., Seng J.M., Williams J.H. Residual life predictions of composite aircraft structures via nondestructive testing. Part 1: Prediction methodology and via nondestructive //Materials Evalua-tion. 2000. V. 58. №9. Р. 1065–1074.
  18. Murashov V.V., Rumjancev A.F. Diagnostika sostava i svojstv polimernyh kompozitov v detaljah i konstrukcijah [Diagnostics of structure and properties of polymeric composites in details and designs] //Kontrol'. Diagnostika. 2008. №8. S. 13–17.
  19. Murashov V.V., Aleksashin V.M. Kontrol' prochnosti zony soedinenija jelementov integral'nyh konstrukcij iz polimernyh kompozitov ul'trazvukovym metodom [Control of durability of zone of connection of elements of integral designs from polymeric composites ultrasonic method] //Klei. Germetiki. Tehnologii. 2014. №7. S. 15–19.
  20. Murashov V.V. Vyjavlenie zon otsutstvija adgezionnogo soedinenija sloev v mnogoslojnyh konstrukcijah [Identification of zones of lack of adhesive connection of layers in multi-layer designs] //Klei. Germetiki. Tehnologii. 2013. №3. S. 29–31.
  21. Murashov V.V. Akusticheskie metody i sredstva kontrolja izdelij iz polimernyh materialov [Acoustic methods and control facilities of products from polymeric materials] //Defektoskopija. 1990. №9. S. 46–52.
  22. Murashov V.V., Generalov A.S. Kontrol' mnogoslojnyh kleenyh konstrukcij nizkochastotnymi akusticheskimi metodami [Control of multi-layer kleeny designs by low-frequency acoustic methods] //Aviacionnye materialy i tehnologii. 2014. №2. S. 59–67.
  23. Bakunov A.S., Murashov V.V., Sysoev A.M. Kontrol' lopastej vozdushnogo vinta sredstvami nizkochastotnoj akustiki [Control of blades of air screw by means of low-frequency acoustics] //Kontrol'. Diagnostika. 2012. №6. S. 72–74.
  24. Semerenko A.V. Ul'trazvukovoj kontrol' izdelij iz kompozicionnyh materialov, primenjajushhihsja v aviacionnoj otrasli promyshlennosti [Ultrasonic control of products from the composite materials which are applying in aviation industry] //Territorija NDT. 2014. №4. S. 57–61.
  25. Murashov V.V., Rumjancev A.F. Defekty monolitnyh detalej i mnogoslojnyh konstrukcij iz polimernyh kompozicionnyh materialov i metody ih vyjavlenija. Chast' 2. Metody vyjavlenija defektov monolitnyh detalej i mnogoslojnyh konstrukcij iz polimernyh kompozicionnyh materialov [Defects of monolithic details and multi-layer designs from polymeric composite materials and methods of their identification. Part 2. Methods of detection of defects of monolithic details and multi-layer designs from polymeric composite materials] //Kontrol'. Diagnostika. 2007. №5. S. 31–36, 41–42.
  26. Rose J. Achievements and prospects of development of the ultrasonic waveguide method of control //Materials Evaluation. 2010. V. 68. №5. P. 494–500.
  27. Murashov V.V. Nerazrushajushhij kontrol' zagotovok i detalej iz uglerod-uglerodnogo kompozicionnogo materiala dlja mnogorazovogo kosmicheskogo korablja «Buran» [Non-destructive testing of preparations and details from carbon - carbon composite material for the reusable Snow-storm spacecraft] //Trudy VIAM. 2013. №4. St. 05 (viam-works.ru).
  28. Murashov V.V. Kontrol' mnogoslojnyh kleenyh konstrukcij iz polimernyh kompozicionnyh materialov [Control of multi-layer kleeny designs from polymeric composite materials] //Klei. Germetiki. Tehnologii. 2011. №10. S. 16–23.
  29. Murashov V.V., Mishurov K.S. Opredelenie poristosti ugleplastikov v aviacionnyh konstrukcijah ul'trazvukovym metodom [Determination of porosity ugleplastikov in aviation designs ultrasonic method] //Aviacionnye materialy i tehnologii. 2015. №2. S. 88–92.
  30. Nerazrushajushhij kontrol': Spravochnik: V 8 t. [Non-destructive testing] /Pod obshh. red. V.V. Kljueva. T. 3. I.N. Ermo-lov, Ju.V. Lange. Ul'trazvukovoj kontrol'. 2-e izd., ispr. M.: Mashinostroenie. 2006. 864 s.
  31. Zeighami M., Hohorvar F. Control of glue joints by immersion method of reflection //Materials Evaluation. 2009. №8. P. 945–954.
  32. Murashov V.V., Rumjancev A.F. Opredelenie prochnosti soedinenija detalej integral'nyh konstrukcij iz polimernyh kompozicionnyh materialov ul'trazvukovym metodom [Determination of durability of connection of details of integral designs from polymeric composite materials ultrasonic method] //Kontrol'. Diagnostika. 2006. №4. S. 45–51.
  33. Murashov V.V., Rumjancev A.F., Ivanova G.A., Fajzrahmanov N.G. Diagnostika struktury, sostava i svojstv polimernyh kompozicionnyh materialov [Diagnostics of structure, structure and properties of polymeric composite materials] //Aviacionnye materialy i tehnologii. 2008. №1. S. 17–24.
  34. Karabutov A.A., Murashov V.V., Oraevsky A.A., Podymova N.B. Nondestructive characterization of layered composite materials with a laser optoacoustic sensor /In: Nondestructive Evaluation of Materials and Composites II. San Antonio: Published by SPIE – The International Society for Optical Engineering. 1998. V. 3396. P. 103–111.
  35. Sposob opredelenija fiziko-mehanicheskih harakteristik polimernyh kompozicionnyh materialov i ustrojstvo dlja ego osushhestvlenija [Way of definition of physicomechanical characteristics of polymeric composite materials and the device for its implementation]: pat. 2214590 Ros. Federacija; opubl. 20.10.2003. Bjul. №29.
  36. Kablov E., Murashov V., Rumyantsev A. Diagnostics of Polymer Composites by Acoustic Methods //Ultrasound. Kaunas: Tecnologija. 2006. №2. Р. 7–10.
  37. Sposob opredelenija prochnostnyh harakteristik polimernyh kompozicionnyh materialov [Way of definition of strength characteristics of polymeric composite materials]: pat. 2461820 Ros. Federacija; opubl. 20.09.2012. Bjul. №26.
  38. Sposob opredelenija stepeni polimerizacii kompozicionnyh materialov [Way of definition of polymerization degree of composite materials]: pat. 2274856 Ros. Federacija; opubl. 20.04.2006. Bjul. №11.
  39. Sposob opredelenija prochnosti soedinenija detalej integral'nyh konstrukcij iz polimernyh kompozicionnyh materialov [Way of determination of durability of connection of details of integral designs from polymeric composite materials]: pat. 2262099 Ros. Federacija; opubl. 10.10.2005. Bjul. №28.
  40. Sposob opredelenija fiziko-mehanicheskih harakteristik i sostava polimernyh kompozicionnyh materialov v konstrukcijah ul'trazvukovym metodom [Way of definition of physicomechanical characteristics and composition of polymeric composite materials in designs ultrasonic method]: pat. 2196982. Ros. Federacija; opubl. 20.01.2003. Bjul. №2.
  41. Kontaktnaja zhidkost' dlja ul'trazvukovogo kontrolja [Contact liquid for ultrasonic control]: a.s. 534684 SSSR; opubl. 05.11.1976. Bjul. №41.
  42. Murashov V.V., Batizat V.P., Guljaeva V.V. Kontaktnaja zhidkost' dlja ul'trazvukovogo kontrolja [Contact liquid for ultrasonic control] //Defektoskopija. 1978. №5. S. 99–100.