Babashov V.G., Butakov V.V., Basargin O.V., Nikitina V.J., Shcheglova T.M. The estimation of VTI-16TM anisotropy by comparison tensile strength of the samples, cut out in the longitudinal and cross direction // Proceedings of VIAM. 2015. No. 7. Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-7-9-9.
The estimation of VTI-16TM anisotropy by comparison tensile strength of the samples, cut out in the longitudinal and cross direction
Abstract
The results of the tensile strength of the flexible samples cut off from the VTI-16TM material in the longitudinal and cross direction, are presented in this paper. The aim of the investigation is to find out if the anisotropy presents in the material after rolling.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period to 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Kablov E.N., Shhetanov B.V., Abuzin Ju.A., Ivahnenko Ju.A. Metallicheskie i keramicheskie kompozicionnye materialy [Metal and ceramic composite materials] /V sb. materialov Mezhdunarodnoj nauch.-praktich. konf. «Sovremennye tehnologii – kljuchevoe zveno v vozrozhdenii otechestvennogo aviastroenija». Kazan'. 2008. T. 1. S. 181–188.
- Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S. Perspektivnye vysokotemperaturnye keramicheskie kompozicionnye materialy [Perspective high-temperature ceramic composite materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 20–24.
- Ivahnenko Ju.A., Babashov V.G., Zimichev A.M., Tinjakova E.V. Vysokotemperaturnye teploizoljacionnye i teplozashhitnye materialy na osnove volokon tugoplavkih soedinenij [High-temperature heatinsulating and heat-protective materials on the basis of fibers of high-melting connections] //Aviacionnye materialy i tehnologii. 2012. №S. S. 380–386.
- Tinjakova E.V., Grashhenkov D.V. Teploizoljacionnyj material na osnove mullito-korundovyh i kvarcevyh volokon [Heatinsulating material on the basis of mullito-korundovy and quartz fibers] //Aviacionnye materialy i tehnologii. 2012. №3. S. 43–46.
- Grashhenkov D.V., Balinova Ju.A., Tinjakova E.V. Keramicheskie volokna oksida aljuminija i materialy na ih osnove [Ceramic fibers of aluminum oxide and materials on their basis] //Steklo i keramika. 2012. №4. S. 32–36.
- Grashhenkov D.V., Shhetanov B.V., Tinjakova E.V., Shheglova T.M. O vozmozhnosti ispol'zovanija kvarcevogo volokna v kachestve svjazujushhego pri poluchenii legkovesnogo teplozashhitnogo materiala na osnove volokon Al2O3 [About possibility of use of quartz fiber as lightweight heat-protective material binding at receiving on the basis of Al2O3 fibers] //Aviacionnye materialy i tehnologii. 2011. №4. S. 8–14.
- Shhetanov B.V., Ivahnenko Ju.A., Babashov V.G. Teplozashhitnye materialy [Heat-protective materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 12–19.
- Babashov V.G., Shhetanov B.V. Gibkij nizkoplotnyj vysokotemperaturnyj material na osnove mullitokorundovogo volokna [Flexible low-density high-temperature material on the basis of mullitokorundovy fiber] //Sovremennye problemy nauki i obrazovanija. 2015. №1 (www.science-education.ru).
- Sposob poluchenija voloknistogo keramicheskogo materiala [Way of receiving fibrous ceramic material]: pat. 2433917 Ros. Federacija; opubl. 20.11.2011. Bjul. №32.
- Sposob poluchenija gibkogo teploizoljacionnogo materiala [Way of receiving flexible heatinsulating material]: zajavka na pat. 2014107962 Ros. Federacija; zaregist. 03.03.2014.
- Erasov V.S., Jakovlev N.O., Nuzhnyj G.A. Kvalifikacionnye ispytanija i issledovanija prochnosti aviacionnyh materialov [Qualification tests and researches of durability of aviation materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 440–448.
- Kolyshev S.G., Basargin O.V., Butakov V.V. Jeksperimenty po opredeleniju prochnosti pri rastjazhenii obrazcov iz legkovesnyh gibkih voloknistyh materialov [Experiments by determination of durability at stretching of samples from lightweight flexible fibrous materials] //Vse materialy. Jenciklopedicheskij spravochnik. Prilozhenie k zhurn. 2014. №5. S. 8–11.
- Zazhigaev L.S., Kish'jan A.A., Romanikov Ju.A. Metody planirovanija i obrabotki rezul'tatov fizicheskih jeksperimentov [Methods of planning and processing of results of physical experiments]. M.: Atomizdat. 1978. S. 180–182.