The study of steel EP866Sh fretting resistance
Abstract
This article describes the experiments that were conducted to study fretting resistance steel EP866Sh. Strained bolt joints are made of the steel where the phenomenon of fretting occurs. Tests were conducted on a universal tribometer CETR UMT-3MT using R33HE1000 lower drive for reciprocating movement in the laboratory environment according to ASTM G204-10. During the experiments load intensity and the oscillation amplitude have changed. The method «pin-on-plate» was chosen to study the tribological properties of steel EP866. Estimated wear curves were conducted metallographic examination of samples.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strate-gicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 go-da» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1. S. 3–33.
- Mubojadzhjan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavinceva E.E. Zashhitnye i uprochnjajushhie ionno-plazmennye pokrytija dlja lopatok i drugih ot-vetstvennyh detalej kompressora GTD [Protective and strengthening ion-plasma coverings for blades and other responsible details of the GTD compressor] //Aviacionnye materialy i tehnologii. 2012. №S. S. 71–81.
- Mubojadzhjan S.A., Aleksandrov D.A., Gorlov D.S. Nanoslojnye uprochnjajushhie pokrytija dlja zashhity stal'nyh i titanovyh lopatok kompressora GTD [Nanolayer strength-ening coverings for protection of steel and titanic compressor blades of GTD] //Aviacionnye materialy i tehnologii. 2011. №3. S. 3–8.
- Litye lopatki gazoturbinnyh dvigatelej. Splavy, tehnologii, pokrytija [Cast blades of gas turbine engines. Alloys, technologies, coverings] /Pod obshh. red. E.N. Kablov. 2-e izd. M.: Nauka. 2006. S. 531–534.
- Vinogradov S.S., Terkulova Ju.A., Kurdjukova E.A., Nikiforov A.A. Iznosostojkoe, anti-frikcionnoe i frettingostojkoe pokrytie na osnove Ni–B [Anti wear, anti friction and fret-tingostoyky coating on the basis of Ni–B] //Trudy VIAM. 2015. №1. St. 02 (viam-works.ru).
- Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse ma-terialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
- Kablov E.N., Mubojadzhjan S.A., Budinovskij S.A., Pomelov Ja.A. Ionno-plazmennye zashhitnye pokrytija dlja lopatok gazoturbinnyh dvigatelej [Ion-plasma protecting covers for blades of gas turbine engines] //Konversija v mashinostroenii. 1999. №2. S. 42–47.
- Fouvry S, Duo P, Perrucchaut Ph. A quantitative approach of Ti-6Al-4V fretting damage: friction, wear and crack nucleation //Wear. 2004. V. 257. №9–10. P. 916–929.
- ASTM Standard G133-05 Standard Test Method for Linearly Reciprocating Ball-on-Flat Sliding Wear. 2010.
- Markova E.S., Jakusheva N.A., Pokrovskaja N.G., Shal'kevich A.B. Tehnologicheskie osobenno-sti proizvodstva martensitostarejushhej stali VKS-180 [Technological features of production of maraging VKS-180 steel] //Trudy VIAM. 2013. №7. St. 01 (viam-works.ru).
- Mubojadzhjan S.A., Lucenko A.N., Aleksandrov D.A., Gorlov D.S. Issledovanie vozmozhnosti povyshenija sluzhebnyh harakteristik lopatok kompressora metodom ionnogo modificirovanija poverhnosti [Research of possibility of increase of office characteristics of compressor blades by method of ionic modifying of surface] //Trudy VIAM. 2013. №1. St. 02 (viam-works.ru).
- Galojan A.G., Mubojadzhjan S.A., Egorova L.P., Bulavinceva E.E. Korrozionnostojkoe pokrytie dlja zashhity detalej GTD iz vysokoprochnyh konstrukcionnyh martensitostare-jushhih stalej na rabochie temperatury do 450°С [Corrosion resistant coating for protection of details of GTD from high-strength constructional maraging staly on working tempera-tures to 450°С] //Trudy VIAM. 2014. №6. St. 03 (viam-works.ru).
- Umanskij A.P., Pugachevskaja E.P., Himko A.N. Razrabotka tehnologii nanesenija novyh iznosostojkih kompozicionnyh pokrytij dlja uprochnenija detalej aviacionnyh dvigatelej [Development of technology of drawing new anti wear composition coatings for hardening of details of aircraft engines] //Aviacionno-kosmicheskaja tehnika i tehnologija. 2009. №9. S. 38–44.