Lomov S.B., Kuptsov R.S. Formation of structural composite material based on magnesium reinforced with refractory particles with different content of the reinforcing phase // Proceedings of VIAM. 2015. No. 5. Ст. 02. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-5-2-2.
Formation of structural composite material based on magnesium reinforced with refractory particles with different content of the reinforcing phase
Abstract
Results of the research dedicated to the time-dependent formation of composite granules are described in the paper. Results of research of technological parameters of briquettes formed from the produced composite granules are shown. Process parameters for production of metal composite material based on magnesium reinforced by refractory particles (10-30 % vol.) by extrusion are analyzed. Mechanical properties of the material were tested and test results were used for correction of the process parameters of composite material formation.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period to 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Istorija aviacionnogo materialovedenija. VIAM – 80 let: gody i ljudi [History of aviation materials science. VIAM – 80 years: years and people] /Pod. obshh. red. E.N. Kablova. M.: VIAM. 2012. 520 s.
- Shmotin Ju.N., Starkov R.Ju., Danilov D.V., Ospennikova O.G., Lomberg B.S. Novye materialy dlja perspektivnogo dvigatelja OAO «NPO „Saturn”» [New materials for the perspective engine of JSC NPO Saturn] //Aviacionnye materialy i tehnologii. 2012. №2. S. 6–8.
- Kablov E.N., Grashhenkov D.V., Isaeva N.V., Solncev S.S., Sevast'janov V.G. Vysokotemperaturnye konstrukcionnye kompozicionnye materialy na osnove stekla i keramiki dlja perspektivnyh izdelij aviacionnoj tehniki [High-temperature constructional composite materials on the basis of glass and ceramics for perspective products of aviation engineering] //Steklo i keramika. 2012. №4. S. 7–11.
- Kablov E.N., Shhetanov B.V., Shavnjov A.A. i dr. Svojstva i primenenie vysokonapolnennogo metallomatrichnogo kompozicionnogo materiala Al–SiC [Properties and application of the high-filled metalmatrix Al-SiC composite material] //Vestnik Nizhegorodskogo universiteta im. N.I. Lobachevskogo. 2011. №3–1. S. 56–59.
- Tarasov Ju.M., Antipov V.V. Novye materialy VIAM − dlja perspektivnoj aviacionnoj tehniki proizvodstva OAO «OAK» [The VIAM new materials − for perspective aviation engineering of production of JSC OAK] //Aviacionnye materialy i tehnologii. 2012. №2. S. 5–6.
- Beljaev M.S., Hvackij K.K., Gorbovec M.A. Sravnitel'nyj analiz rossijskogo i zarubezhnyh standartov ispytanij na ustalost' metallov [Comparative analysis Russian and foreign standards of fatigue tests of metals] //Trudy VIAM. 2014. №9. St. 11 (viam-works.ru).
- Erasov V.S., Grinevich A.V., Senik V.Ja., Konovalov V.V., Trunin Ju.P., Nesterenko G.I. Raschetnye znachenija harakteristik prochnosti aviacionnyh materialov [Calculated values of characteristics of durability of aviation materials] //Aviacionnye materialy i tehnologii. 2012. №2. S. 14–16.
- Lur'e S.A., Soljaev Ju.O. Modificirovannyj metod Jeshelbi v zadache opredelenija jeffektivnyh svojstv so sfericheskimi mikro- i nanovkljuchenijami [The modified method of Eshelbi in problem of determination of effective properties with spherical micro and nanoinclusions] //Vestnik PGTU. Mehanika. 2010. №1. S. 80–90.
- Singh Sarabjot, Junior B. Tech, Ryssel Heiner. Lifetime of power modules /In: 7 Indo-German winter academy. Proceedings. Germany. 2008.
- Gilleo K. MEMS/MOEMS Packaging Concepts, Designs, Materials and Processes /In: Nanoscience and Technology Series. USA. NY-Chicago: McGraw-Hill. 2005. 239 p.
- Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
- Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry in aviation materials science] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
- Hari Babu N., Zhongyun Fan, Eskin D.G. Application of external fields to technology of metal matrix composite materials //TMS-2013 Annual Meeting Supplemental Proceedings. 2013. P. 1037–1044.
- Kablov E.N., Shhetanov B.V., Grashhenkov D.V., Shavnev A.A., Njafkin A.N. Metalloma-trichnye kompozicionnye materialy na osnove Al–SiC [Metalmatrix composite materials on the basis of Al–SiC] //Aviacionnye materialy i tehnologii. 2012. №S. S. 373–380.
- Kablov E.N., Chibirkin V.V., Vdovin S.M. Izgotovlenie, svojstva i primenenie teplootvodjashhih osnovanij iz MMK Al–SiC v silovoj jelektronike i preobrazovatel'noj tehnike [Manufacturing, properties and application of the heat-removing bases from Al–SiC MMK in power electronics and converting equipment] //Aviacionnye materialy i tehnologii. 2012. №2. S. 20–22.