Petrov A.V., Doriomedov M.S., Skripachyov S.Yu. Foreign experience of manufacturing products using recycled polymer composites (re-view) // Proceedings of VIAM. 2015. No. 12. Ст. 12. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-12-12-12.

Foreign experience of manufacturing products using recycled polymer composites (re-view)

Petrov A.V., Doriomedov M.S., Skripachyov S.Yu.
Abstract

The article describes the experience of several countries (Japan, USA, UK, Germany and others.) to reduce the negative impact on the environment and meet the legal requirements by manufacturing products of national economic destination of the recycled carbon fiber reinforced plastics, fiberglass reinforced plastics and fiber reinforced polypropylene. Some of the main technological processes using abroad in the manufacture of products from recycled polymers composite materials are described. At present, the solution of recycling problem is one of the aspects contributing to widespread adoption and application of polymeric composite materials in priority industries. This is due to the fact that today more and more consumers prefer those materials and products the negative influence of which on the environment in the process of manufacture, use and disposal would be minimal.

Keywords
polymer composite material, recycling, secondary use, fiber reinforced plastic.
Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  3. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  4. Vlasenko F.S., Raskutin A.E. Primenenie polimernyh kompozicionnyh materialov v stroitelnyh konstrukcijah [Applying FRP in building structures] //Trudy VIAM. 2013. №8. St. 03 (viam-works.ru).
  5. Doneckij K.I., Khrulkov A.V. Principy «zelenoj himii» v perspektivnyh tehnologiyah izgotovleniya izdelij iz PKM [Principles of «green chemistry» in perspective manufacturing technologies of PCM articles] //Aviacionnye materialy i tehnologii. 2014. №S2. S. 24–28.
  6. Petrov A.V., Doriomedov M.S., Skripachev S.Yu. Tehnologii utilizacii polimernyh kompozicionnyh materialov (obzor) [Recycling technologies of polymer composite materials (review)] //Trudy VIAM. 2015. №8. St. 09 (viam-works.ru).
  7. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazujushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  8. Adesso Advanced Materials. Available at: http://www.adessomaterials.com (Accessed: March 10, 2015).
  9. Connora Technologies. Available at: http://www.connoratech.com (Accessed: March 10, 2015).
  10. Job S. Recycling composites commercially (part 2) //Reinforced Plastics. 2014. V. 58. №5. P. 36–38.
  11. Reprocover. Available at: http://www.reprocover.com (Accessed: April 07, 2015).
  12. Job S. Recycling glass fibre reinforced composites – history and progress (part 1) //Reinforced Plastics. 2013. Available at: http://www.materialstoday.com (Accessed: April 09, 2015).
  13. AXION International's. Available at: http://www.axionintl.com (Accessed: April 29, 2015).
  14. IntegriCo Composites. Available at: http://integrico.com (Accessed: March 03, 2015).
  15. ReFiber. Available at: http://www.refiber.com (Accessed: April 23, 2015).
  16. Sposob pererabotki kompozicionnyh materialov [Way of processing of composite materials]: pat. WO 2002088277 A1; opubl. 07.11.2002.
  17. Hitachi Chemical Technical Report №56. Hitachi Chemical Co., Ltd. March. 2014.
  18. CFK Valley Stade Recycling. Available at: http://www.cfk-recycling.com (Accessed: April 07, 2015).
  19. Black S. Redesigning for simplicity and economy //High-Performance Composites. 2012. Available at: http://www.compositesworld.com (Accessed: March 18, 2015).
  20. Ustanovka dlya piroliza othodov kompozicionnyh materialov [Installation for pyrolysis of waste of composite materials]: pat. 2208203 Ros. Federaciya; opubl. 10.07.2003.
  21. Korotaev V.N. Razrabotka tehnologii utilizacii krupnogabaritnyh korpusov raketnyh dvigatelej, izgotovlennyh iz organicheskih kompozicionnyh plastikov [Development of technology of utilization of large outline packages of the rocket engines made of organic composition plastics]: Avtoref. dis. … kand. tehn.nauk. M.: RHTU im. D.I. Mendeleeva. 1996. 18 s.