Nazarkin R.M., Kolodochkina V.G., Ospennikova O.G., Orlov M.R. The irreversible structural modifications of single crystals fine structure of Ni-based superalloys at enduring operation of turbine blades // Proceedings of VIAM. 2015. No. 12. Ст. 03. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-12-3-3.

The irreversible structural modifications of single crystals fine structure of Ni-based superalloys at enduring operation of turbine blades

Nazarkin R.M., Kolodochkina V.G., Ospennikova O.G., Orlov M.R.
Abstract

The results of researches of single-crystal rotor blades from cast Ni-based superalloy ZhS32-VI in process of long-time life cycle testing of gas turbine engine (high-pressure turbine) are represented for microstructure and substructure. It is shown that precipitation of TCP-phases particles in the alloy during high-temperature testing is accompanied by the decreasing of crystal lattice constant of γ-solid solution. It is verified by data of x-ray diffraction analysis, x-Ray microanalysis and scanning electron microscopy. The point is proposed that decreasing of alloying element content in the γ-solid solution as result of TCP-phases precipitation (rich with the refractory elements) leads to the fall of the high-temperature resistance of the material. Also, a TCP-phases make negative influence on mechanical properties of the alloy due to the local destruction of coherency for interphase boundaries in zone of development of TCP-phases particles.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Ospennikova O.G. Strategiya razvitiya zharoprochnyh splavov i stalej specialnogo naznacheniya, zashhitnyh i teplozashhitnyh pokrytij [Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings] //Aviacionnye materialy i tehnologii. 2012. №S. S. 19–36.
  3. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlya aviacionnogo dvigatelestroeniya [Creation of modern heat resisting materials and technologies of their production for aviation engine building] //Krylya Rodiny. 2012. №3–4. S. 34–38.
  4. Orlov M.R. Strategicheskie napravleniya razvitiya Ispytatelnogo centra FGUP «VIAM» [Strategic directions of development of the Test center FSUE «VIAM»] //Aviacionnye materialy i tehnologii. 2012. №S. S. 387–393.
  5. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharo-prochnye splavy novogo pokoleniya [Nickel foundry hot strength alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  6. Petrushin N.B., Ospennikova O.G., Visik E.M., Rassohina L.I., Timofeeva O.B. Zharoprochnye nikelevye splavy nizkoj plotnosti [Heat resisting nickel alloys of low density] //Litejnoe proizvodstvo. 2012. №6. S. 5–11.
  7. Kablov E.N. Fiziko-mehanicheskie i tehnologicheskie osobennosti sozdaniya zharoprochnyh splavov, soderzhashhih renij [Physicomechanical and technological features of creation of the hot strength alloys, containing reniye] //Vestnik Moskovskogo universiteta. Ser. 2: Himiya. 2005. T. 46. №3. S. 155–167.
  8. 4. Kablov E.N., Muboyadzhyan S.A. Zharostojkie i teplozashhitnye pokrytiya dlja lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE] //Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
  9. Kablov E.N., Petrushin N.V., Bronfin M.B., Alekseev A.A. Osobennosti monokristallicheskih zharoprochnyh nikelevyh splavov, legirovannyh reniem [Features of the single-crystal heat resisting nickel alloys alloyed by rhenium] //Metally. 2006. №5. S. 47–57.
  10. Bondarenko Yu.A., Kablov E.N. Napravlennaya kristallizaciya zharoprochnyh splavov s povyshennym temperaturnym gradientom [The directed crystallization of hot strength alloys with the raised temperature gradient] //MiTOM. 2002. №7. S. 20–23.
  11. Bondarenko Yu.A., Kablov E.N., Morozova G.I. Vliyanie vysokogradientnoj napravlennoj kristallizacii na strukturu i fazovyj sostav zharoprochnogo splava tipa Rene-N5 [Influence of the high-gradient directed crystallization on structure and phase composition of hot strength alloy of the Rene-N5 type] //MiTOM. 1999. №2. S. 15–18.
  12. Morozova G.I. Zakonomernost formirovaniya himicheskogo sostava γ′/γ-matricy mnogokomponentnyh nikelevyh splavov [Pattern of forming of chemical composition γ′/γ-matrix multicomponent nickel alloys] //Doklady Akademii nauk. 1991. T. 320. №6. S. 1413–1416.
  13. Kablov E.N., Petrushin N.V. Kompyuternyj metod konstruirovaniya litejnyh zharoprochnyh nikelevyh splavov [Computer method of designing of cast heat resisting nickel alloys] /V kn. Litejnye zharoprochnye splavy. Effekt S.T. Kishkina /Pod red. E.N. Kablova. M.: Nauka. 2006. S. 56–78.
  14. Ospennikova O.G., Orlov M.R., Kolodochkina V.G., Nazarkin R.M. Strukturnye izmeneniya i povrezhdenie monokristallicheskih rabochih lopatok turbiny v processe resursnyh ispytanij aviacionnogo gazoturbinnogo dvigatelya [Structural changes and injury of single-crystal working turbine blades in the course of resource tests of the aviation gas turbine engine] //Deformaciya i razrushenie materialov. 2014. №8. S. 22–29.
  15. Orlov M.R., Yakimova M.S., Letov A.F. Analiz rabotosposobnosti monokristallicheskih lopatok turbiny vysokogo davleniya v sostave nazemnyh gazoturbinnyh ustanovok [The analysis of operability of single-crystal turbine blades of high pressure as a part of land gas turbine units] //Aviacionnye materialy i tehnologii. 2012. №S. S. 399–407.
  16. Samojlov A.I., Nazarkin R.M., Moiseeva N.S. Opredelenie misfita vo fragmentirovannyh monokristallah nikelevyh zharoprochnyh splavov [Definition miss-fit in fragmental single crystals of nickel hot strength alloys] //Trudy VIAM. 2013. №5. St. 02 (viam-works.ru).
  17. Samojlov A.I., Nazarkin R.M., Moiseeva N.S. Misfit kak istochnik i kriterij rabotosposobnosti zharoprochnyh nikelevyh splavov [Misfit as source and criterion of operability of heat resisting nickel alloys] //Zavodskaya laboratoriya. Diagnostika materialov. 2013. T. 79. №6. S. 33–36.
  18. Kablov E.N., Orlov M.R., Ospennikova O.G. Mehanizmy obrazovanija poristosti v monokristallicheskih lopatkah turbiny i kinetika ee ustranenija pri gorjachem izostaticheskom pressovanii [Mechanisms of formation of porosity in single-crystal turbine blades and kinetics of its elimination at hot isostatic pressing] //Aviacionnye materialy i tehnologii. 2012. №S. S. 117–129.