Belous V.Ya., Loshchinina A.O., Varlamova V.E., Nikitin Ya.Yu. Corrosion resistance and preparation of a surface of a cold rolled tape from VNS9-Sh steel for production of metalpolymeric composite material // Proceedings of VIAM. 2015. No. 11. Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-11-10-10.

Corrosion resistance and preparation of a surface of a cold rolled tape from VNS9-Sh steel for production of metalpolymeric composite material

Belous V.Ya., Loshchinina A.O., Varlamova V.E., Nikitin Ya.Yu.
Abstract

The results of comparative tests of two meltings of cold rolled tape from VNS-9-Sh steel on intergranular corrosion and pitting corrosion are considered in this work. Possibility of preparation of the tape surface by means of etching in various acid solutions in order to manufacture metalpolymeric composite material is investigated. Values of a roughness and influence of etching on plasticity of material are defined.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  3. Kablov E.N. Aviacionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and perspectives] //Vestnik Rossijskoj akademii nauk. 2012. T. 72. №1. S. 3–12.
  4. Dushin M. I., Hrulkov A.V., Muhametov R.R., Chursova L.V. Osobennosti izgotovleniya izdelij iz PKM metodom propitki pod davleniem [Features of manufacturing of products from PCM impregnation method under pressure] //Aviacionnye materialy i tehnologii. 2012. №1. S. 18–26.
  5. Hrulkov A.V., Dushin M.I., Popov Yu.O., Kogan D.I. Issledovaniya i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovaniya PKM [Researches and development autoclave and out-of-autoclave technologies of formation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  6. Grigorev M.M., Kogan D.I., Tverdaya O.N., Panina N.N. Osobennosti izgotovleniya PKM metodom RFI [Features of manufacturing of PCM RFI method] //Trudy VIAM. 2013. №4. St. 03 (viam-works.ru).
  7. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazujushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  8. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svyazujushhie dlya perspektivnyh metodov izgotovleniya PKM novogo pokoleniya [Melt binding for perspective methods of production of PCM of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  9. Gunyaev G.M., Kablov E.N., Aleksashin V.M. Modificirovanie konstrukcionnyh ugleplastikov uglerodnymi nanochasticami [Modifying constructional ugleplastikov carbon nanoparticles] //Rossijskij himicheskij zhurnal. 2010. T. 54. №1. S. 5–11.
  10. Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Perspektivy ispolzovaniya uglerodsoderzhashhih nanochastic v svyazuyushchih dlya polimernyh kompozicionnyh materialov [Perspectives of use of carbon-containing nanoparticles in binding for polymeric composite materials] //Rossijskie nanotehnologii. 2013. T. 8. №3–4. S. 24–42.
  11. Kirillov V.N., Startsev O.V., Efimov V.A. Klimaticheskaya stojkost i povrezhdaemost polimernyh kompozicionnyh materialov, problemy i puti resheniya [Climatic firmness and damageability of polymeric composite materials, problems and solutions] //Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
  12. Kirillov V.N., Efimov V.A., Shvedkova A.K., Nikolaev E.V. Issledovanie vliyaniya klimaticheskih faktorov i mehanicheskogo nagruzheniya na strukturu i mehanicheskie svojstva PKM [Research of influence of climatic factors and mechanical loading on structure and the PCM mechanical properties] //Aviacionnye materialy i tehnologii. 2011. №4. S. 41–45.
  13. Stolyankov Yu.V., Ishodzhanova I.V., Antyufeeva N.V. K voprosu o defektah obrazcov dlya ispytanij ugleplastikov [On the question of carbon fiber reinforced plastics (CFRP) test specimen flaws] //Trudy VIAM. 2014. №10. St. 10 (viam-works.ru).
  14. Terentev V.F., Slizov A.K., Prosvirnin D.V. i dr. Vliyanie skorosti deformirovaniya rastyazheniem na mehanicheskie svojstva i fazovyj sostav trip-stali VNS-9-Sh [Influence of speed of deformation by stretching on mechanical properties and phase composition of VNS-9-Sh trip-steel] //Deformaciya i razrushenie materialov. 2014. №10. S. 40–43.
  15. Voznesenskaya N.M., Kapitanenko D.V., Tonysheva O.A., Eliseev E.A. Optimizaciya tehnologicheskih rezhimov polucheniya tonkih listov i lenty iz korrozionnostojkoj stali VNS-9-Sh [Optimization of technological modes of receiving thin sheets and tape from the VNS-9-Sh corrosion-resistant steel] //Metally. 2014. №1. S. 46–51.
  16. Gurvich L.Ya., Lashhevskij V.B. Korroziya i zashhita splavov v morskih usloviyah [Corrosion and protection of alloys in sea conditions] /V sb. Voprosy aviacionnoj nauki i tehniki. Ser. «Aviacionnye materialy». M.: VIAM. 1985. S. 64–81.