Beider E.Ya., Petrova G.N. The thermoplastic binder for polymeric composite materials // Proceedings of VIAM. 2015. No. 11. Ст. 05. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-11-5-5.

The thermoplastic binder for polymeric composite materials

Beider E.Ya., Petrova G.N.
Abstract

Properties of thermoplastic binder on the basis of superstructural thermoplastics are given in the article. The algorithm of actions is described at selection of binder on the basis of thermoplastics for manufacture of PCM. On example of polysulphone the influence of molecular weight on thermal-physical, mechanical and rheological properties of the thermoplastic binder is studied. Influence of physical condition of binder (powder, film, fiber, granules) on manufacturing technology of prepregs of PCM is shown.

Reference list
  1. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  2. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  4. Kablov E.N. Nauka kak otrasl ekonomiki [Science as economy industry] //Nauka i zhizn. 2009. №10. S. 6–12.
  5. Petrova G.N., Beider E.Ya. Konstrukcionnye materialy na osnove armirovannyh termoplastov [Constructional materials on the basis of the reinforced thermoplastics] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 4–40.
  6. Nozdrina L.V., Korotkova V.I., Beider Je.Ja. Termoplastichnye polimery dlya konstrukcionnyh materialov. Obzor [Thermoplastic polymers for constructional materials. Review] //Tehnologiya. Ser. «Konstrukcii iz kompozicionnyh materialov». 1991. №1. S. 3–10.
  7. Mihajlin Yu.A. Konstrukcionnye polimernye kompozicionnye materialy [Constructional polymeric composite materials]. SPb.: Nauchnye osnovy i tehnologii. 2008. S. 100–570.
  8. Perov B.V. Termoplasty, napolnennye voloknami [The thermoplastics filled with fibers] /V kn. Termoplasty konstrukcionnogo naznachenija; Pod red. E.B. Trostjanskoj. M.: Himija. 1975. S. 187–216.
  9. Termoplasty konstrukcionnogo naznachenija [Thermoplastics of constructional assignment] /Pod red. E.B. Trostjanskoj. M.: Himija. 1975. 240 s.
  10. Dovgjalo V.A., Zinovev S.N., Pomerantseva K.P., Yurkevich O.R. O vliyanii tehnologii prepregov na konstrukcionnye svojstva ugleplastikov [About influence of technology of prepregs on constructional properties ugleplastikov] //Doklady AN BSSR. 1986. T. 30. №3.
  11. S. 237–239.
  12. Gunyaev G.M., Chursova L.V., Komarova O.A., Gunyaeva A.G. Konstrukcionnye ugleplastiki, modificirovannye nanochasticami [Constructional coal the plastics modified by nanoparticles] //Aviacionnye materialy i tehnologii. 2012. №S. S. 277–286.
  13. Kerber M.L., Vinogradov V.M., Golovkin G.S., Gorbatkina Ju.A. i dr. Polimernye kompozicionnye materialy: struktura, svojstva, tehnologiya [Polymeric composite materials: structure, properties, technology]. SPb.: Professiya. 2008. S. 30–32, 62–72.
  14. Zelenskij E.S., Kuperman A.M., Lebedeva O.V. Armirovannye plastiki na osnove termoplastichnyh svjazujushhih [The reinforced plastics on the basis of the thermoflexible binding] //Tehnologiya. Ser. «Konstrukcii iz kompozicionnyh materialov». 1991. №1. S. 10–21.
  15. Mihajlin Yu.A. Termoplastichnye kompozicionnye materialy [Термопластичные композиционные материалы] //Polimernye materialy. 2007. №7. S. 8.
  16. Perepelkin K.E. Armirujushhie volokna i voloknistye polimernye kompozity [Reinforcing fibers and fibrous polymeric composites]. M.: Nauchnye osnovy i tehnologii. 2009. 658 s.
  17. Polimernye kompozicionnye materialy. Svojstva. Struktura. Tehnologii [Polymeric composite materials. Properties. Structure. Technologies] /Pod red. A.A. Berlina. SPb.: Professiya. 2009. 560 s.
  18. Berlin A.A., Volfson S.A., Oshmyan V.G., Enikolopov N.S. Principy sozdaniya kompozicionnyh polimernyh materialov [Principles of creation of composite polymeric materials]. M.: Himiya. 1990. 238 s.
  19. Gunyaev G.M., Kablov E.N., Aleksashin V.M. Modificirovanie konstrukcionnyh ugleplastikov uglerodnymi nanochasticami [Modifying constructional coal of plastics carbon nanoparticles] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 5–11.
  20. Krutko E.T., Prokopchuk N.R. Perspektivnye puti sozdaniya novyh termostojkih materialov na osnove poliimidov [Perspective ways of creation of new heat-resistant materials on the basis of polyimide] //Trudy BGTU. Ser. «Himiya, tehnologiya organicheskih veshhestv i biotehnologii». 2013. №4. S. 145–149.
  21. Petrova N.A. Stekloplastiki i ih syrevoe obespechenie v Rossii [Fibreglasses and their raw providing in Russia] //Polimernye materialy. 2008. №11. S. 33–36.
  22. Petrova G.N., Beider Je.Ja., Izotova T.F., Malyshenok S.V. Kompozicionnye termoplastichnye materialy – sposoby polucheniya i pererabotki [Composite thermoflexible materials – ways of receiving and processing] //Vse materialy. Enciklopedicheskij spravochnik. 2013. №10. S. 10–17.
  23. Beider E.Ya., Petrova G.N., Izotova T.F., Gureeva E.V. Kompozicionnye termoplastichnye materialy i penopoliimidy [Thermoplastic composite materials and foam polyimides] //Trudy VIAM. 2013. №11. St. 01 (viam-works.ru).
  24. Beider E.Ya., Malyshenok S.V., Petrova G.N. Kompozicionnye termoplastichnye materialy – svojstva i sposoby pererabotki [Composite thermoflexible materials – properties and ways of processing] //Plasticheskie massy. 2013. №7. S. 56–60.
  25. Uglerodnye volokna i uglekompozity [Carbon fibers and coal composites]: Per. s ang. /Pod red. Je. Fitcera. M.: Mir. 1988. 336 s.
  26. Beider E.Ya., Petrova G.N., Izotova T.F., Barbotko S.L. Stekloplastiki na termoplastichnoj matrice [Glass reinforced plastics on the basis of thermoplastic matrix] //Trudy VIAM. 2013. №7. St. 03 (viam-works.ru).
  27. Agafonova A.S., Kondrashov S.V. Osobennosti tehnologii izgotovlenija monolitnogo stekloplastika radiotehnicheskogo naznachenija (MSRT) [Features of a technology to manufacture monolithic glass-fiber plastics intended for radio engineering] //Aviacionnye materialy i tehnologii. 2014. №1. S. 30–33.
  28. Komarov G.A. Sostojanie, perspektivy i problemy primenenija PKM v tehnike [Condition, perspectives and problems of application of PKM in equipment] //Polimernye materialy. 2009. №2. S. 5–9.
  29. Davydova I.F., Kavun N.S. Stekloplastiki ‒ mnogofunkcionalnye kompozicionnye materialy [Fibreglasses ‒ multipurpose composite materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 253–260.
  30. Petrova G.N. Napravlennaja modifikacija polisulfonov i sozdanie na ih osnove litevyh i kompozicionnyh materialov [The directed updating of polysulphones and creation on their basis of lityevy and composite materials]: Avtoref. dis. k.t.n. M.: VIAM. 2011. S. 10–27.
  31. Petrova G.N., Beider E.Ya., Chebotarev V.P., Lovkov S.S., Sazikov V.I. Regulirovanie svojstv polisulfonov za schet modifikacii [Regulation of properties of polysulphones at the expense of updating] //Plasticheskie massy. 2010. №12. S. 23–27.
  32. Gunyaev G.M., Gofin M.Ya. Uglerod-uglerodnye kompozicionnye materialy [Carbon-carbon composite materials] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 62–90.
  33. Mihajlin Yu.A. Termoustojchivye polimery i polimernye materialy na ih osnove [Thermosteady polymers and polymeric materials on their basis] //Polimernye materialy. 2005. №8. S. 12–23.
  34. Beider E.Ya., Petrova G.N., Izotova T.F. Vliyanie appretov na svojstva termoplastichnyh stekloplastikov [An influence of coupling agent on properties of thermoplastic glass reinforced plastics] //Trudy VIAM. 2014. №9. St. 07 (viam-works.ru).
  35. Beider E.Ya., Petrova G.N., Dykun M.I. Appretirovanie uglerodnyh volokon-napolnitelej termoplastichnyh karboplastikov [Dressing of carbon fibers – fillers of thermoplastic carbon reinforced plastics] //Trudy VIAM. 2014. №10. St. 03 (viam-works.ru).
  36. Zaborskaya L.V., Yurkevich O.R., Dovgyalo V.A., Pisanova E.V. Issledovanie zakonomernostej sovmeshheniya dispersnogo polisulfona s armiruyushhimi voloknami pri poluchenii kompozitnyh materialov [Research of patterns of combination of disperse polysulphone with reinforcing fibers when receiving composite materials] //Mehanika kompozitnyh materialov. 1991. №3. S. 403–407.
  37. Ustinov V.A., Beider E.Ya. Primenenie kompozicionnyh materialov s termoplastichnoj matricej [Application of composite materials with thermoflexible matrix] //Konstrukcii iz kompozicionnyh materialov. 1991. №1. S. 21–28.
  38. Petrova G.N., Beider E.Ya., Perfilova D.N., Rumyanceva T.V. Pozharobezopasnye litevye termoplasty i termojelastoplasty [Fire safety of injection molding thermoplastics and TPE materials] //Trudy VIAM. 2013. №11. St. 02 (viam-works.ru).
  39. Abrosimov A.P. Evropejskij rynok termoplastichnyh elastomerov i sovremennye tendencii [European market of thermoflexible elastomer and current trends] //Promyshlennoe proizvodstvo i ispolzovanie elastomerov. 2010. №3. S. 29–34.
  40. Petrova G.N., Perfilova D.N. i dr. Termoplastichnye jelastomery dlya zameny rezin [Thermoflexible elastomer for replacement of rubbers] //Aviacionnye materialy i tehnologii. 2012. №S. S. 302–308.
  41. Petrova G.N., Rumyanceva T.V. i dr. Termoelastoplasty – novyj klass polimernyh materialov [Thermoelastoplastics – new class of polymeric materials] //Aviacionnye materialy i tehnologii. 2010. №4. S. 20–25.
  42. Volfson S.I. Dinamicheski vulkanizovannye termoelastoplasty [Dynamically vulkanizovanny thermoelastoplastics]. M.: Nauka. 2004. S. 5–12.
  43. Novokshonov V.V., Musin I.N., Kimelblat V.I. Optimizaciya svojstv maslostojkih termoplastichnyh elastomernyh kompozicij [Optimization of properties of oilproof thermoflexible elastomeric compositions] //Plasticheskie massy. 2009. №3. S. 24–27.
  44. Mihajlin Yu.A., Kerber M.L., Gorbunova I.Yu. Svyazujushhie dlya polimernyh kompozicionnyh materialov [Binding for polymeric composite materials] //Plasticheskie massy. 2002. №2. S. 14–21.
  45. Richardson M. Promyshlennye polimernye kompozicionnye materialy [Промышленные полимерные композиционные материалы]. M.: Himiya. 1980. 472 s.
  46. Beider E.Ya. Aerodispersnye pokrytiya v izdeliyah aviacionnoj tehniki [Aero disperse coverings in products of aviation engineering]: Avtoref. dis. … k.t.n. M.: VIAM. 1970. S. 10–25.
  47. Yurkevich O.R. Osnovy tehnologii kompozicionnyh materialov i pokrytij, formiruemyh v gazodispersnyh polimernyh potokah [Bases of technology of composite materials and the coverings created in gazodispersny polymeric flows]: Avtoref. dis. … d.t.n.: Gomel: IMMS. 1985. S. 12–36.
  48. Yurkevich O.R. O haraktere rastekaniya polimernoj kapli po poverhnosti tverdogo tela [About nature of spreading of polymeric drop on surface of solid body] //Novoe v reologii polimerov. 1981. Ch. 2. S. 126–128.
  49. Golovkin G.S., Goncharenko V.A., Dmitrenko V.P. Volokonnaya tehnologiya termoplastichnyh kompozicionnyh materialov [Fiber technology of thermoflexible composite materials]. M.: MAI. 1993. 232 s.
  50. Golovkin G.S., Rybkina E.G. i dr. Tkanye polufabrikaty organoplastov iz plavkih i neplavkih volokon [Woven semi-finished products of organic laminates from fusible and not fusible fibers] /V sb. Voprosy aviacionnoj nauki i tehniki. Ser. «Aviacionnye materialy». M.: VIAM. 1988. №1. S. 15–20.
  51. Mihajlin Yu.A. Termoreaktivnye svyazuyushhie PKM [Thermosetting binding PKM] //Polimernye materialy. 2008. №10. S. 14–19.