Vakhromov R.O., Tkachenko E.A., Lukinа E.A., Selivanov A.A. Influence of homogenization annealing on structure and properties of ingots from 1933 alloy of Al–Zn–Mg–Cu system // Proceedings of VIAM. 2015. No. 11. Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-11-1-1.

Influence of homogenization annealing on structure and properties of ingots from 1933 alloy of Al–Zn–Mg–Cu system

Vakhromov R.O., Tkachenko E.A., Lukinа E.A., Selivanov A.A.
Abstract

Homogenizing annealing of ingots is held to dissolve the nonequilibrium excess phases, eliminating intergranular segregation and reduce internal stresses in the ingots of aluminum alloys. Simultaneously, there is a process of disintegration of solid solution of aluminum small additions of transition metals( manganese, chromium, zirconium) to form dispersoids. The influence of different modes of homogenization on the volume fraction of nonequilibrium structural components, the properties of the 1933 alloy ingot at elevated temperatures, density of distribution and size of Al3Zr dispersoid are represented.

Reference list
  1. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – a basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  2. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  3. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  4. Vahromov R.O., Tkachenko E.A., Popova O.I. Vliyanie osnovnyh legirujushhih komponentov, mikrodobavok i primesej na svojstva kovochnyh splavov sistemy Al–Zn–Mg–Cu [Influence of the main alloyng elements, microadditives and impurities on the properties of forging alloys of Al–Zn–Mg –Cu system] //Tsetnye Metally. 2013. №5 (845). S. 61–65.
  5. Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Alyuminievye deformiruemye splavy [Aluminum deformable alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
  6. Tarasov Yu.N., Vahromov R.O. Primenenie alyuminievyh splavov, razrabotannyh pod rukovodstvom akademika I.N. Fridlyandera, v otechestvennoj aviacionnoj tehnike [Application of aluminium alloys, developed under the guidance of аcademician I. N. Fridlyander, in Russian aviation engineering] //Tsvetnye Metally. 2013. № 9 (849). S. 37–39.
  7. Tarasov Yu.M., Antipov V.V. Novye materialy VIAM – dlya perspektivnoj aviacionnoj tehkniki proizvodstva OAO «OAK» [The VIAM new materials – for perspective aviation engineering of production of JSC «OAK»] //Aviacionnye materialy i tehnologii. 2012. №2. S. 5–6.
  8. Vahromov R.O., Tkachenko E.A., Popova O.I., Milevskaya T.V. Obobshhenie opyta primeneniya i optimizaciya tehnologii izgotovleniya polufabrikatov iz vysokoprochnogo alyuminievogo splava 1933 dlya silovyh konstrukcij sovremennoj aviacionnoj tehniki [Summarizing of the experience of usage and optimization of manufacturing technology semi-fished product of high strength aluminum alloy 1933 for the primary structures of modern aircraft] //Aviacionnye materialy i tehnologii. 2014. № 2. S. 34–39.
  9. Fridlyander I.N. Alyuminievye deformiruemye konstrukcionnye splavy [Aluminum deformable constructional alloys] //Metallurgiya. 1979. 208 s.
  10. Gomogenizaciya slitkov alyuminievyh splavov [Homogenization of ingots of aluminum alloys]. TR 50-31-70. M.: VILS.1970. 24 s.
  11. Fridlyander I.N. Metallovedenie alyuminievyh splavov [Metallurgical science of aluminum alloys]. M.: Nauka. 1985. 238 s.
  12. Belov N.A. Fazovyj sostav promyshlennyh i perspektivnyh alyuminievyh splavov [Phase structure of industrial and perspective aluminum alloys]. M.: Izd. dom MISiS. 2010. 511 s.
  13. Vahromov R.O., Tkachenko E.A., Antipov V.V. Zakonomernosti formirovaniya struktury i svojstv kovochnyh splavov sistemy Al–Zn–Mg–Cu c razlichnym soderzhaniem osnovnyh legiruyushhih komponentov, mikrodobavok i primesej [Regularities of formation of structure and properties of forging alloys of Al–Zn–Mg–Cu system with various maintenance of the main alloying components, microadditives and impurity] //Vestnik Samarskogo gosudarstvennogo ajerokosmicheskogo universiteta im. akademika S.P. Koroleva (Nacional'nogo issledovatel'skogo universiteta). 2012. № 5–1 (36). S. 215–222.
  14. Vakhromov R.O., Tkachenko E.A., Antipov V.V. Research and Development of High-Strength of Al–Zn–Mg–Cu Alloys //Proceedings 13th International Conference on Aluminum Alloys. 2012. P. 1514–1520.
  15. Lima S.T., Yun S.J., Namb S.W. Improved quench sensitivity in modified aluminum alloy 7175 for thick forging applications //Materials Science and Engineering, A. 2004. V. 371 (1–2). P. 82−90.
  16. Robinson J.S., Cudd R.L., Tanner T.D. Quench sensitivity and tensile property inhomogeneity in 7010 forgings //Journal of Materials Processing Technology. 2001. V. 119 (1−3). P. 261−267.
  17. Li Pei-yue, Bai-qing Xiong, Yong-an Zhang, Zhi-hui Li, Bao-hong Zhu, Feng Wang, Hong-wei Liu. Quench sensitivity and microstructure character of high strength AA7050 //Transactions of Nonferrous Metals Society of China. 2012. V. 22 (2). P. 268−274.
  18. Yu-lin Zheng, Cheng-bo Li, Sheng-dan Liu, Yun-lai Deng, Xin-ming Zhang. Effect of homogenization time on quench sensitivity of 7085 aluminum alloy //Transactions of Nonferrous Metals Society of China. 2014. V. 24. P. 2275−2281.
  19. Xin-ming Zhang, WenJun Liu, ShengDan Liu, MingZhe Zhou. Effect of processing parameters on quench sensitivity of an AA7050 sheet //Materials Science and Engineering, A. 2011. V. 528.
  20. P. 795–802.
  21. Li X.M., Starink M.J. Identification and analysis of intermetallic phases in overaged Zr-containing and Cr-containing Al−Zn−Mg−Cu alloys//Alloys Compd. 2011.V. 509. P. 471−476.
  22. Marlaud T., Deschamps A., Bley F., Lefebvre W., Baroux B. Influence of alloy composition and heat treatment on precipitate composition in Al−Zn−Mg−Cu alloys //Acta Materialia. 2010. V. 58 (1). P. 248−260.
  23. Conserva M., DI Russo E., Caloni O. Comparison of the Influence of Chromium Zirconium on the Quench Sensitivity of Al–Zn–Mg–Cu Alloys //Metallurgical Transactions. 1971. V. 2. 1227 p.
  24. Cposob izgotovleniya izdelij iz aljuminievyh deformiruemyh splavov [A way of production of products from aluminum deformable alloys]: pat. 2284367. Ros. Federaciya; opubl. 27.01.05.