Sagomonova V.A., Kislyakova V.I., Tyumeneva T.Y., Bolshakov V.A. The influence of vibration damping materials' composition on their mechanical loss factor // Proceedings of VIAM. 2015. No. 10. Ст. 10. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-10-10-10.

The influence of vibration damping materials' composition on their mechanical loss factor

Sagomonova V.A., Kislyakova V.I., Tyumeneva T.Y., Bolshakov V.A.
Abstract

The research of mechanical loss factor (tgδ) of vibration damping materials of different composition: extensional damping material, materials with metallic and composite constraining layers and ones with different thickness and chemical nature adhesive layers is hereby provided. It has been shown that chemical nature and thickness of adhesive layer alters its damping properties and existence of constraining layer leads to increasing of mechanical loss factor.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry in aviation materials science] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  3. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  4. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  5. Vibropogloshhajushhij material [Vibropogloshchayushchy material]: pat. 2148497 Ros. Federacija; opubl. 10.05.2000.
  6. Teploizolirujushhij i vibropogloshhajushhij listovoj material [Heat-insulating and vibropogloshchayushchy sheet material]: pat. 2456178 Ros. Federa-cija; opubl. 20.07.2012.
  7. Germetizirujushhaja mastika i vibropogloshhajushhij polimernyj material na ee osnove [Pressurizing mastic and vibropogloshchayushchy polymeric material on its basis]: pat. 2421497 Ros. Federacija; opubl. 27.12.2011.
  8. Vibroshumopogloshhajushhij zvukoizolirujushhij material [Vibroshumopogloshchayushchy soundproofing material]: pat. 2340640 Ros. Federacija; opubl. 10.12.2008.
  9. Konstrukcionnyj sloistyj izolirujushhij material [Constructional layered isolating material]: pat. 2159185 Ros. Federacija; opubl. 20.11.2000.
  10. Vibropogloshhajushhij material [Vibropogloshchayushchy material]: pat. 2035256 Ros. Federacija; opubl. 20.05.1995.
  11. Ustrojstvo dlja gashenija vibracij truboprovodov [The device for clearing of vibrations of pipelines]: pat. 2234024 Ros. Federacija; opubl. 10.08.2004.
  12. Vibropogloshhajushhee ustrojstvo [Vibropogloshchayushchey device]: pat. 2117336 Ros. Federacija; opubl. 10.08.1998.
  13. Ustrojstvo kreplenija aviacionnyh dvigatelej [Device of fastening of aircraft engines]: poleznaja model' 18091 Ros. Federacija; opubl. 20.05.2001.
  14. Vibropogloshhajushhij material [Vibropogloshchayushchy material]: pat. 2235106 Ros. Federacija; opubl. 27.08.2004.
  15. Teploizolirujushhij i vibropogloshhajushhij listovoj material [Heat-insulating and vibropogloshchayushchy sheet material]: poleznaja model' 102567 Ros. Federacija; opubl.10.03.2011.
  16. Rongong J.A., Goruppa A.A., Buravalla V.R. Plasma deposition of constrained layer damping coatings //Journal of Mechanical Engineering Science. Part C. 2004. V. 218. P. 669–679.
  17. Sperling L.H. Sound and Vibration Damping with Polymers: Basic Viscoelastic Definitions and Concepts /In: American Chemical Society Symposium Series. Washington D.C. 1990. P. 5–23.
  18. Nikiforov A.S., Burdin S.V. Kombinirovannoe vibropogloshhajushhee pokrytie i ego primenenie [The combined vibropogloshchayushchy covering and its application] /V sb. materialov seminara «Vibropogloshhajushhie materialy i pokrytija i ih primenenie». L. 1974. S. 15–19.
  19. Gallimore C.A. Passive viscoelastic constrained layer damping application for a small aircraft landing gear system /In: Thesis submitted to the faculty of the Virginia Polytechnic Insitute and State University in partial fulfillment of the requirements for the degree of Master of Science in mechanical Engineering. Blackburg. VA. 2008. P. 1–102.
  20. Jones D.I.G. Shock and Vibration Handbook. NY: McGrow-Hill. 5-th edition. Chapter 37. 2011. (электронная версия).
  21. Kraev I.D., Obrazcova E.P., Jurkov G.Ju. Vlijanie morfologii magnitnogo napolnitelja na radiopogloshhajushhie harakteristiki kompozicionnyh materialov [Influence of morphology of magnetic filler on radio absorbing characteristics of composite materials] //Aviacionnye materialy i tehnologii. 2014. №S2. S. 10–14.
  22. Shul'deshov E.M., Lepeshkin V.V., Platonov M.M., Romanov A.M. Metod opredelenija akusticheskih harakteristik zvukopogloshhajushhih materialov v rasshirennom do 15 kGc diapazone chastot [Method of definition of acoustic characteristics of sound-proof materials in the range of frequencies expanded to 15 kHz] //Aviacionnye materialy i tehnologii (v pechati).
  23. Lukina N.F., Dement'eva L.A., Petrova A.P., Tjumeneva T.Ju. Svojstva kleev i klejashhih materialov dlja izdelij aviacionnoj tehniki [Properties of glues and gluing materials for products of aviation engineering] //Klei. Germetiki. Tehnologii. 2009. №1. S. 14–24.
  24. Tjumeneva T.Ju., Zhadova N.S., Lukina N.F. Razrabotki FGUP «VIAM» v oblasti kleev rezinotehnicheskogo naznachenija i samoklejashhihsja materialov [Development of VIAM Federal State Unitary Enterprise in the field of glues of industrial rubber assignment and being self-glued materials] //Trudy VIAM. 2014. №7. St. 04 (viam-works.ru).
  25. Askadskij A.A., Luchkina L.V., Nikiforova G.G. Vibropogloshhajushhie gradientnye polimernye materialy [Vibropogloshchayushchiye gradient polymeric materials] //Plasticheskie massy. 2007. №4. S. 30–33.
  26. Rao M.D. Recent applications of viscoelastic damping for noise control in automobiles and commercial airplanes //J. Sound and Vibration. 2003. №262. Р. 457–474.
  27. Gandhi F., Austruy J. Constrained-layer damping with gradient polymers for effectiveness over broad temperature ranges //The American Institute of Aeronautics and Astronautics Journal. 2007. V. 45. №8. P. 1885–1893.
  28. Fotsing E.R., Sola M., Ross A., Ruiz E. Lightweight damping of composite sandwich beams: Experimental analysis //Journal of Composite Materials. 2012 (http://jcm.sagepub.com).
  29. Systems and methods for reducing noise in aircraft fuselages and other structures: pat. 8042768 US; publ. 25.10.2010.
  30. Improved composite materials: pat. 0268945 US; publ. 03.11.2011.
  31. Structural composite material with improved acoustic and vibrational damping properties: pat. 8450225 US; publ. 28.05.2013.
  32. Multilayer and composition gradient structures with improved damping properties: pat. 0164907 US; publ. 28.06.2012.
  33. Polymer composites possessing improved vibration damping: pat. 0313307 US; publ. 13.12.2012.
  34. Composite components and heat-curing resins and elastomers: pat. 0034833 (US), publ. 09.02.2012.
  35. Nagasankar S., Balasivanandha P., Velmurugan R. Influence of the Different Fiber lay-ups on the Damping Characteristics of the Polymer Matrix //Journal of Applied Sciences. 2012. V. 12 (10). P. 1071–1074.