Naumov I.S., Petrova A.P., Еliseev O.A., Barbotko S.L. Experimental research in the field of development of organic silicon rubbers with low flammability // Proceedings of VIAM. 2015. No. 10. Ст. 09. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-10-9-9.

Experimental research in the field of development of organic silicon rubbers with low flammability

Naumov I.S., Petrova A.P., Еliseev O.A., Barbotko S.L.
Abstract

A brief description of the manufacturing process of rubber compounds based on silicone rubber SKTV-1 and vulcanizates samples of the rubber compounds for research is provided. The description of the conducted researches of physic-mechanical properties and flammability of vulcanizates of rubber compounds on the basis of the silicone SKTV-1 rubber containing different quantity of flame retardants is given. By results of research vulcanizates properties the choice of flame retardants was made for receiving fire-resistant rubber on the basis of silicone rubber of the SKTV-1. Results of experimental research of samples of vulcanizates on the basis of the new organic silicon block copolymer possessing increased heat resistance are given.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry in aviation materials science] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  3. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] //Nauka i zhizn'. 2010. №4. S. 2–7.
  4. Bol'shoj spravochnik rezinshhika [Big directory of rezinshchik]. V 2 ch. M.: OOO «Tehinform». 2012. 1385 s.
  5. Shetc M. Siloksanovyj kauchuk [Siloxane rubber]. SPb.: Himija. 1975. 192 s.
  6. Gorenie, destrukcija i stabilizacija polimerov [Burning, destruktsiya and stabilization of polymers] /Pod red. G.E. Zaikova. SPb.: Nauchnye osnovy i tehnologii. 2008. 422 s.
  7. Tehnologija reziny: recepturostroenie i ispytanija [Technology of rubber: retsepturostroyeniye and tests]: Per. s angl. /Pod red. Dzh.S. Dika. SPb.: Nauchnye osnovy i tehnologii. 2010. 617 s.
  8. Gorjuchest' i dymoobrazujushhaja sposobnost' polimernyh materialov aviacionnogo naznachenija [Combustibility and smoke-generating ability of polymeric materials of aviation assignment] /Pod red. R.E. Shalina, B.I. Panshina. M.: VIAM. 1986. 104 s.
  9. Kodolov V.I. Zamedliteli gorenija polimernyh materialov [Decelerators of burning of polymeric materials]. M.: Himija. 1980. 269 s.
  10. Barbot'ko S.L., Shurkova E.N., Vol'nyj O.S., Skrylev N.S. Ocenka pozharnoj bezopasnosti polimernyh kompozicionnyh materialov dlja vneshnego kontura aviacionnoj tehniki [Assessment of fire safety of polymeric composite materials for external circuit of aviation engineering] //Aviacionnye materialy i tehnologii. 2013. №1. S. 56–59.
  11. Barbot'ko S.L., Shurkova E.N. O pozharnoj bezopasnosti materialov, ispol'zuemyh dlja izgotovlenija vneshnego kontura samoletov [About fire safety of the materials used for manufacturing of external circuit of airplanes] //Pozharovzryvobezopasnost'. 2011. T. 20. №10. S. 19–24.
  12. Petrova G.N., Bejder Je.Ja., Perfilova D.N., Rumjanceva T.V. Pozharobezopasnye lit'evye termoplasty i termojelastoplasty [Fireproof lityevy thermoplastics and thermoelastoplastics] //Trudy VIAM. 2013. №11. St. 02 (viam-works.ru).
  13. Petrova G.N., Rumjanceva T.V., Bejder Je.Ja. Vlijanie modificirujushhih dobavok na po-zharobezopasnye svojstva i tehnologichnost' polikarbonata [Influence of modifying additives on fireproof properties and technological effectiveness of polycarbonate] //Trudy VIAM. 2013. №6. St. 06 (viam-works.ru).
  14. Clough R.L. Aging Effects on Fire-Retardant Additives in Polymers //Journal of Polymer Science: Polymer Chemistry Edition. 1983. V. 21. P. 767–780.
  15. Shurkova E.N., Vol'nyj O.S., Izotova T.F., Barbot'ko S.L. Issledovanie vozmozhno-sti snizhenija teplovydelenija pri gorenii kompozicionnogo materiala putem izmenenija ego struktury [Research of possibility of decrease in heat release when burning composite material by change of its structure] //Aviacionnye materialy i tehnologii. 2012. №1. S. 27–30.
  16. Barbot'ko S.L. Pozharobezopasnost' aviacionnyh materialov [Fire safety of aviation materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 431–439.
  17. Barbot'ko S.L. Puti obespechenija pozharnoj bezopasnosti aviacionnyh materialov [Ways of ensuring fire safety of aviation materials] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 121–126.
  18. Naumov I.S., Petrova A.P., Chajkun A.M. Reziny uplotnitel'nogo naznachenija i snizhenie ih gorjuchesti [Rubbers of sealing assignment and decrease in their combustibility] //Vse materialy. Jenciklopedicheskij spravochnik. 2013. №5. S. 28–35.
  19. Mitina E.L., Naumov I.S. Samozatuhajushhij material na osnove kombinacii hloroprenovogo i butadienovogo kauchukov [Self-fading material on the basis of combination of chloroprene and butadiyenovy rubbers] //Klei. Germetiki. Tehnologii. 2012. №6. S. 9–12.
  20. Mitina E.L., Barbot'ko S.L. Vlijanie antipirenov na gorjuchest' dekorativnyh rezin na osnove kombinacii butadien-stirol'nogo i butadienovogo kauchukov [Influence of antipyrines on combustibility of decorative rubbers on the basis of combination of styrenr-butadiene and butadiyenovy rubbers] //Klei. Germetiki. Tehnologii. 2012. №3. S. 17–21.
  21. Naumov I.S., Chajkun A.M., Eliseev O.A. Rossijskie i mezhdunarodnye standarty na metody ispytanij rezin, syryh rezinovyh smesej i vysokomolekuljarnyh kauchukov [The Russian and international standards on test methods of rubbers, crude rubber mixes and high-molecular rubbers] //Vse materialy. Jenciklopedicheskij spravochnik. 2014. №11. S. 4–13.
  22. Aviacionnye pravila. Gl. 25. Normy letnoj godnosti samoletov transportnoj kategorii [Aviation rules. Hl. 25. Standards of the flight validity of airplanes of transport category]. 3-e izd. M.: OAO Aviaizdat. 2009. 274 s.
  23. OST 1 90094–79. Polimernye materialy. Metod opredelenija gorjuchesti dekorativno-otdelochnyh i konstrukcionnyh polimernyh materialov [Polymeric materials. Method of determination of combustibility of decorative and finishing and constructional polymeric materials].
  24. Eliseev O.A., Krasnov L.L., Zajceva E.I., Savenkova A.V. Razrabotka i modificirovanie jelastomernyh materialov dlja primenenija vo vseklimaticheskih uslovijah [Development and modifying of elastomeric materials for application in vseklimatichesky conditions] //Aviacionnye materialy i tehnologii. 2012. №S. S. 309–314.
  25. Chajkun A.M., Eliseev O.A., Naumov I.S., Venediktova M.A. Osobennosti morozostojkih rezin na osnove razlichnyh kauchukov [Features of cold-resistant rubbers on the basis of different rubbers] //Trudy VIAM. 2013. №12. St. 04 (viam-works.ru).
  26. Naumov I.S., Barbot'ko S.L., Petrova A.P., Malysheva G.V. Vlijanie antipirenov na svojstva uplotnitel'noj reziny na osnove jetilen-propilen-dienovogo kauchuka (JePDK) [Influence of antipyrines on properties of sealing rubber on basis ethylene-propylene-diene rubber (EPDR)] //Vse materialy. Jenciklopedicheskij spravochnik. 2014. №5. S. 31–34.