Kashapov O.S., Pavlova T.V., Istrakova A.R., Kalashnikov V.S. Effect of iron content on mechanical properties of forgings from heat-resistance titanium alloy VT41 // Proceedings of VIAM. 2015. No. 10. Ст. 01. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2015-0-10-1-1.

Effect of iron content on mechanical properties of forgings from heat-resistance titanium alloy VT41

Kashapov O.S., Pavlova T.V., Istrakova A.R., Kalashnikov V.S.
Abstract

The structure and mechanical properties of forgings from heat-resistant near-α-titanium alloy VТ41 with different iron content are examined in this paper. It has been established that the increase in the iron content leads to the increase in strength proper-ties of the material in the working temperature range and some decrease in characteris-tics of ductility and toughness. Increasing the iron content is accompanied with increased sensitivity to stress concentrators under different types of tests.

Reference list
  1. Kashapov O.S., Pavlova T.V., Istrakova A.R., Kalashnikov V.S. Vlijanie soderzhanija zheleza na mehanicheskie svojstva prutkov iz zharoprochnogo titanovogo splava VT41 [Influence of the content of iron on mechanical properties of bars from heat resisting BT41 titanium alloy] //Trudy VIAM. 2015. №3. St. 02 (viam-works.ru).
  2. Kashapov O.S., Pavlova T.V., Nochovnaja N.A. Vlijanie rezhimov termicheskoj obrabotki na strukturu i svojstva zharoprochnogo titanovogo splava dlja lopatok KVD [Influence of modes of thermal processing on structure and property of heat resisting titanium alloy for KVD blades] //Aviacionnye materialy i tehnologii. 2010. №2. S. 8–14.
  3. Kashapov O.S., Pavlova T.V. Issledovanie vlijanija parametrov struktury polufabrikatov iz splava VT41 na mehanicheskie svojstva [Research of influence of parameters of structure of semi-finished products from alloy ВТ41 on mechanical properties] //Vestnik MGTU im. N.Je. Baumana. 2015. №2. S. 136–143.
  4. Ilyin A., Kolachev B., Volodin V., Ryndenkov D. About the purposefulness of comprasion of titanium alloys in terms of aluminium and Molybdenium equivalents /In: Titanium–99. Science and technology. 1999. P. 53–60.
  5. Sposob termicheskoj obrabotki vysokoprochnyh (α+β)-titanovyh splavov [Way of thermal processing high-strength (α +β)-titanium alloys]: pat. 2465366 Ros. Federacija; opubl. 15.09.2011.
  6. Sposob termomehanicheskoj obrabotki izdelij iz titanovyh splavov [Way of thermomechanical processing of products from titanium alloys]: pat. 2457273 Ros. Federacija; opubl. 05.04.2011.
  7. Horev A.I. Teoreticheskie i prakticheskie osnovy povyshenija konstrukcionnoj prochnosti sov-remennyh titanovyh splavov [Theoretical and practical bases of increase of constructional durability of modern titanium alloys] //Tehnologija legkih splavov. 2007. №2. S. 144–153.
  8. Horev A.I. Razrabotka konstrukcionnyh titanovyh splavov dlja izgotovlenija detalej i uzlov aviakosmicheskoj tehniki [Development of structural titanium alloys for manufacturing of details and nodes of aerospace equipment] //Svarochnoe proizvodstvo. 2009. №3. S. 13–23.
  9. Kashapov O.S. Kinetika izmenenija mikrostruktury prutkovoj lopatochnoj zagotovki iz splava VT41 v zavisimosti ot temperaturno-vremennyh parametrov termicheskoj obrabotki [Kinetics of change of microstructure of bar scapular preparation from alloy ВТ41 depending on temperature and time parameters of thermal processing] //Perspektivnye materialy. 2008. №5. S. 137–140.
  10. Titanium-base alloy: pat. 87 30 5197 EP; pabl. 01.06.1988.
  11. Russo P.A., Yu K.O. Effect of Ni, Fe, and primary alpha on the creep of alpha-beta processed and annealed Ti–6Al–2Sn–4Zr–2Mo–0,09Si /In: Titanium–99. Science and technology. 1999. P. 596–603.
  12. Russo P.A., Yu K.O. Effect of Ni, Fe, and Si on the creep of Ti–6Al–2Sn–4Zr–6Mo /In: Titanium–99. Science and technology. 1999. P. 713–720.
  13. Kashapov O.S., Pavlova T.V., Istrakova A.R., Kalashnikov V.S. Povyshenie prochnostnyh harakteristik zharoprochnyh psevdo-α-titanovyh splavov [Increase of strength characteristics heat resisting псевдо-α-титановых alloys] //Aviacionnye materialy i tehnologii. 2014. №S5. C. 73–80.
  14. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period to 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  15. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] //Nauka i zhizn'. 2010. №4. S. 2–7.
  16. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  17. Kablov E.N. Materialy dlja izdelija «Buran» – innovacionnye reshenija formirovanija shestogo tehnologicheskogo uklada [Materials for the product «Buran» – innovative solutions of forming of the sixth technological way] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
  18. Pavlova T.V., Kashapov O.S., Nochovnaja N.A., Beljaev M.S. Sovremennye titanovye splavy i tehnologii, primenjaemye dlja detalej i uzlov GTD [Modern titanium alloys and the technologies applied to details and GTD nodes] /V sb. tezisov dokladov nauch.-tehnich. kongressa po dvigatelestroeniju «Dvigateli–2012». M.: ASSAD. 2012. S. 347–349.
  19. Horev A.I., Belov S.P., Glazunov S.G. Metallovedenie titana i ego splavov [Metallurgical science of titanium and its alloys]. M.: Metallurgija. 1992. 352 s.