R. R. Ivankov, A. I. Gulyaev Approaches to the analysis of the adhesive contact area when testing using a modified pull-out method from a «loop-knot». Part 2 // Proceedings of VIAM. 2026. No. 9 (163). С. 196-208. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-9-196-208.
Approaches to the analysis of the adhesive contact area when testing using a modified pull-out method from a «loop-knot». Part 2
1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru
Abstract
This article proposes a new method for determining the area of adhesive contact during the testing of samples using the modified pull-out method. The obtained values of adhesive strength between the Russian carbon fiber UMT42S-3K and the epoxy binder VSE-30 using the improved pull-out method were compared with the values obtained using the reference pull-out and push-out methods. The article also presents the areas of adhesive contact after testing using the push-out method.
Keywords
optical microscopy, adhesion, strength, carbon fibers, epoxy binder, scanning electron microscopy, push-out test
Reference list
- Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Zhelezina G.F., Kulagina G.S., Sidorina A.I., Soloveva N.A. Fatigue of constructional organoplastics. Aviacionnye materialy i tehnologii, 2014, no. 1, pp. 89-100. Available at: http://www.journal.viam.ru (accessed: May 15, 2026). DOI: 10.18577/2713-0193-2024-0-1-98-100.
- Nacharkina A.V., Valueva M.I., Zelenina I.V., Shosheva A.L. High-temperature carbon fiber reinforced plastics based on bismaleinimide binders. Aviation materials and technologies, 2024, no. 4 (77), pp. 43-61. Available at: http://www.journal.viam.ru (accessed: May 15, 2026). DOI: 10.18577/2713-0193-2024-0-4-43-61.
- Skuridina N.S., Bolshakov V.A., Klimenko O.N., Barinov D.Ya. Investigation of the kinetics of curing of an epoxy binder in a prepreg based on an equal-strength fabric using multivariate regression methods. Trudy VIAM, 2025, no. 11 (153), pp. 12-22. Available at: http://www.viamworks.ru (accessed: May 15, 2026). DOI: 10.18577/2307-6046-2025-0-11-12-22.
- Amirova L.R., Khamidullin O.L., Zalyalova G.M., Amirova L.M. Assessment of kinetic parameters of the curing process of epoxyanhydride systems by DSC. Izvestiya Akademii nauk. Seriya khimicheskaya, 2017, no. 3, pp. 483-487.
- Engineered interfaces in fiber reinforced composites. Ed. J.K. Kim, Y.W. Mai. Elsevier, 1998, p. 416.
- Gorbatkina Yu.A., Ivanova-Mumzhieva V.G., Kuperman A.M. Adhesion of modified epoxy matrices to reinforcing fibers. Vysokomolekulyarnye sovedineniya. Ser.: A, 2016, vol. 58, no. 5, pp. 439-447. DOI: 10.7868/S2308112016050060.
- Kumar R., Cross W.M., Kjerengtron L., Kellar J.J. Fiber bias in nanoindentation of polymer matrix composites. Composite Interfaces, 2004, vol. 11, pp. 431-440.
- Qiu Y., Schwartz P. A new method for study of the fiber-matrix interface in composites: single fiber pull-out from a microcomposite. Journal of adhesion science and technology, 1991, vol. 5, no. 9, pp. 741-756.
- Gulyaev A.I., Medvedev P.N., Sbitneva S.V., Petrov A.A. Experimental research of «fiber-matrix» adhesion strength in carbon fiber epoxy/polysulphone composite. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 80-86. DOI: 10.18577/2071-9140-2019-0-4-80-86.
- Gulyayev A.I. Fiber-matrix adhesion strength measurement using nanoindentation (review). Trudy VIAM, 2019, no. 3 (75), pp. 68-78. Available at: http://www.viam-works.ru (accessed: March 05, 2026). DOI: 10.18577/2307-6046-2019-0-3-68-78.
- Jager J., Sause M.G.R., Burkert F. et al. Influence of plastic deformation on single-fiber push-out tests of carbon fiber reinforced epoxy resin. Composites. Part A, 2015, vol. 71, pp. 157-167.
- Wang S.-W., Khan A., Sands R., Vasudevan A.K. A novel nanoindentor technique for measuring fibre-matrix interfacial strengths in composites. Journal of Materials Science Letters, 1992, vol. 11, pp. 739-741.
- Desaeger M., Verpoest I. On the use of the micro-indentation test technique to measure the interfacial shear strength of fibre-reinforced polymer composites. Composites Science and Technology, 1993, vol. 48, pp. 215-226.
- Janczak J., Burki G., Rohr L. Interfacial characterisation of MMCs and CMCs using SEM-pushout technique. Key Engineering Materials, 1997, vol. 127-131, pp. 623-630.
- Haeberle D.C. The use of nanoindentation to determine composite interfacial shear strength and the effects of environmental aging: Thesis for the Degree of Master of Science in Engineering Science and Mechanics. Blacksburg, 2001, 112 p.
- Chawla N., Chawla K.K., Koopman M. et al. Thermal-shock behavior of a Nicalon-fiberreinforced hybrid glass-ceramic composite. Composites Science and Technology, 2001, vol. 61, pp. 1923-1930.
- Gallo S.C., Li X., Zhang Z. et al. Viscoelastic response of carbon fiber reinforced polymer during push-out tests. Composites Part A, 2018, vol. 112, pp. 178-185.
- Urena A., Rams J., Escalera M.D., Sanchez M. Characterization of interfacial mechanical properties in carbon fiber/aluminium matrix composites by the nanoindentation technique. Composites Science and Technology, 2005, vol. 65, pp. 2025-2038.
- Mueller W.M., Moosburger-Will J., Sause M.G.R., Horn S. Microscopic analysis of single-fiber push-out tests on ceramic matrix composites performed with Berkovich and flat-end indenter and evaluation of interfacial fracture toughness. Journal of the European Ceramic Society, 2013, vol. 33, pp. 441-451.
- Kotomin S.V., Obidin I.M., Pavlyuchkova E.A. Calculation of the adhesive bond strength of reinforcing fibers with polymers using the «loop» method. Mekhanika kompozitnykh materialov, 2022, vol. 58, no. 1, pp. 197–212.
- Gorbatkina Yu.A., Ivanova-Mumzhieva V.G. Influence of the polymer–fiber joint size on the change in adhesion strength under various external influences. Part 1. Scale dependence of the adhesion strength of fiber–thermosetting binder joints under normal conditions. Klei. Germetiki. Tekhnologii, 2025, no. 9, pp. 25–31. DOI: 10.31044/1813-7008-2025-0-9-25-31.
- Kotomin S.V., Obidin I.M., Pavlyuchkova E.A. Scale factor in testing adhesive joints of heteroaramid threads using the «loop» method. Klei. Germetiki. Tekhnologii, 2023, no. 11, pp. 35–40.
- Ivankov R.R., Sidorina A.I., Kotomin S.V. Determination of the strength of the adhesive bond between Russian carbon fibers and an epoxy matrix using the «loop» pull-out test. Trudy VIAM, 2025, no. 12 (154), pp. 170–184. Available at: http://www.viam-works.ru (accessed: May 25, 2026). DOI: 10.18577/2307-6046-2025-0-12-170-184.
- Gorbatkina Yu.A., Ivanova-Mumzhieva V.G. Effect of the size of polymer-fiber joints on the change in adhesion strength under various external influences. Part 2. Effect of the size of thermosetting binder-fiber joints on the temperature dependence of their adhesion strength. Klei. Germetiki. Tekhnologii, 2025, no. 10, pp. 33–37. DOI: 10.31044/1813-7008-2025-0-10-33-37.
- Nelyub V.A. Experimental evaluation of the elastic modulus of the adhesive bond of the epoxy matrix – carbon fiber with a metal coating system. Sovremennye naukovemykie tekhnologii, 2019, no. 6, pp. 96–100.
The article was submitted
2026-07-31
approved and accepted for publication after reviewing
2026-08-31