A. V. Nacharkina, I. V. Zelenina, L. V. Cherfas, G. B. Eldyaeva, A. G. Gunyaeva Influence of storage conditions on properties of bismaleimid prepreg and carbon fiber composite based on it // Proceedings of VIAM. 2026. No. 9 (163). С. 71-85. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-9-71-85.

Influence of storage conditions on properties of bismaleimid prepreg and carbon fiber composite based on it

A. V. Nacharkina1, I. V. Zelenina1, L. V. Cherfas1, G. B. Eldyaeva1, A. G. Gunyaeva1

1Federal State Unitary Enterprise «All-Russian Scientific-Research Institute of Aviation Materials» of National Research Center «Kurchatov Institute», Moscow, Russia; admin@viam.ru

Abstract

The effect of various storage conditions on the properties of the carbon fiber prepreg VKU-74 based on a heat-resistant melt bismaleimide binder and equal-strength carbon fabric was studied. The assessment of the physical and mechanical characteristics of carbon fiber VKU-74 samples made from prepreg after storage under various conditions. Based on the results of the conducted research, the warranty period for storing prepreg in a room at a temperature of 20±5 °С, in a refrigerator at 0÷5 °С, and in a freezer at –18±5 °С has been established.

Keywords
polymer composite materials, prepreg, high-temperature carbon fiber reinforced plastics, melt bismaleimide binder, storage conditions, guaranteed shelf life
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3-33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Chursova L.V., Babin A.N., Mukhametov R.R., Panina N.N. Developments of FSUE VIAM in the field of melt binders for polymer composite materials. Polimernye materialy i tekhnologii, 2016, vol. 2, no. 2, pp. 37-42.
  3. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48-58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  4. Startsev V.O., Antipov V.V., Slavin A.V., Gorbovets M.A. Modern domestic polymer composite materials for aviation industry (review). Aviation materials and technologies, 2023, no. 2 (71), pp. 122-144. Available at: http://www.journal.viam.ru (accessed: May 05, 2026). DOI: 10.18577/2713-0193-2023-0-2-122-144.
  5. Iredale R.J., Ward C., Hamerton I. Modern advances in bismaleimide resin technology: A 21st century perspective on the chemistry of addition polyimides. Progress in Polymer Science, 2017, vol. 69, pp. 1-21.
  6. Nacharkina A.V., Zelenina I.V., Smirnov A.V., Boychuk A.S. Influence of the molding method on the structure and properties of carbon fiber reinforced plastics based on bismaleimide binder. Trudy VIAM, 2025, no. 9 (151), pp. 35-49. Available at: http://www.viam-works.ru (accessed: May 25, 2026). DOI: 10.18577/2307-6046-2025-0-9-35-49.
  7. Xu X., Peng G., Zhang B. et al. Material performance, manufacturing methods, and engineering applications in aviation of carbon fiber reinforced polymers: A comprehensive review. Thin-Walled Structures, 2025, vol. 209, art. 112899. DOI: 10.1016/j.tws.2024.112899.
  8. Nacharkina A.V., Valueva M.I., Zelenina I.V., Shosheva A.L. High-temperature carbon fiber reinforced plastics based on bismaleimide binders. Aviation materials and technologies, 2024, no. 4 (77), pp. 43-61. Available at: http://www.journal.viam.ru (accessed: May 20, 2026). DOI: 10.18577/2713-0193-2024-0-4-43-61.
  9. Evsyukov S.E., Pohlmann T., ter Wiel M. Modern approaches to the processing of bismaleimide resins. Current trends in polymer science, 2020, vol. 20, pp. 1-28.
  10. Bismaleimide Prepreg Systems Market - Global Forecast 2026-2032. Researchandmarkets. Available at: https://www.researchandmarkets.com/reports/6122216/bismaleimide-prepreg-systems-market-global#src-pos-1 (accessed: June 18, 2026).
  11. Mosiyuk V., Bukharov S., Baranov A. Manufacture of Molding Tooling Based on TEIS-53 Heat-Resistant Resin. Key Engineering Materials (Materials Science Forum). Switzerland: Trans Tech Publication Ltd, 2022, vol. 910, pp. 351-356. DOI: 10.4028/p-st7n2q.
  12. Valueva M.I., Zelenina I.V., Nacharkina A.V., Boychuk A.S. Determination of the guaranteed shelf life of high-temperature polyimide carbon fiber reinforced plastic prepreg. Trudy VIAM, 2023, no. 10 (128), pp. 64-81. Available at: http://www.viam-works.ru (accessed: May 14, 2026). DOI: 10.18577/2307-6046-2023-0-10-64-81.
  13. Cherfas L.V., Gunyaeva A.G., Komarova O.A., Antyufeva N.V. The analysis of nanomodified prepreg shelf life by its reactivity at storage. Trudy VIAM, 2016, no. 1 (37), pp. 99-106. Available at: http://www.viam-works.ru (accessed: May 21, 2026). DOI: 10.18577/2307-6046-2016-0-1-99-106.
  14. Gapankova E.I., Latyshevich I.A. Evaluation of the Effect of Storage Duration on the Properties of Prepregs. Oil and Gas Chemistry-2022: Proceedings of the V Int. Sc. and Tech. Forum on Chemical Technologies and Oil and Gas Refining. Minsk, 2022, pp. 88–91.
  15. Bobovich B.B. Polymer Structural Materials (Structure, Properties, Application). Moscow: FORUM INFRA-M, 2014, 400 p.
  16. Kerber M.L., Vinogradov V.M., Golovkin G.S. et al. Polymer Composite Materials: Structure, Properties, Technology: Textbook. Ed. A.A. Berlin. St. Petersburg: Profession, 2008, 560 p.
  17. Mikhailin Yu. A. Fibrous polymer composite materials in engineering. St. Petersburg: Scientific Foundations and Technologies, 2013, 719 p.
  18. Guseva M.A., Petrova A.P. Possibilities of rheology in the study of binders for polymer composite materials. Vse materialy. Entsiklopedicheskiy spravochnik, 2021, no. 7, pp. 38–44.
  19. Veshkin E.A., Postnov V.I., Strelnikov S.V., Abramov P.A., Satdinov R.A. Experience in the Application of Process Control of Semi-finished Products Made of Polymer Composite Materials. Izvestiya Samarskogo nauchnogo tsentra RAN, 2014, vol. 16, no. 6 (2), pp. 393–398.
  20. Shimkin A.A., Safronov A.M. Quality Control of Polymer Binders and Prepregs by the DSC Method. Zavodskaya laboratoriya. Diagnostika materialov, 2016, vol. 82, no. 8, pp. 30–33.
  21. Frigione M., Kenny J.M. Effects of storage aging on the cure kinetics of bismaleimide prepregs. Advances in Polymer Technology, 2005, vol. 24, no. 4, pp. 253–265. DOI: 10/1002/adv.20048.
  22. Tomchani O.V., Vorvul S.V., Khabenko A.V. et al. Study of the properties of melt epoxy-bismaleimide binder and composites based on it. Designs and technologies for producing products from non-metallic materials: collection of abstracts of reports of the 18th Int. sc. and tech. conf. Obninsk, 2010, pp. 33–36.
  23. Bismaileimide binders. Available at: https://itecma.ru/products/svyazuyushchie/bismailemidnye-svyazuyushchie (accessed: June 02, 2026).
  24. Prepregs. Available at: https://www.hexcel.com/products/prepregs-resins/hexply-prepregs (accessed: June 02, 2026).
  25. CYCOM-5250-4 TECHNICAL DATA SHEET CYCOM®. Available at: https://hongrunplastics.com/public/uploads/images/20260203/CYCOM%205250-4.pdf (accessed: June 02, 2026).
  26. BMI resin. Available at: https://www.toraytac.com/media/4ac868f6-f136-4b14-92d6-0f777b3a24cf/g6JoSw/TAC/Documents/Data_sheets/Thermoset/UD%20tapes%20and%20prepregs/RS-8HT_BMI_PDS.pdf (accessed: June 02, 2026).
  27. RM-3002 Bismaileimide resin. Available at: https://www.lookpolymers.com/pdf/Renegade-Materials-Corporation-RM-3002-Bismaleimide-BMI-Resin-IM7-12K-Carbon-Uni-tape.pdf (accessed: June 02, 2026).