Chabina E.B., Alekseev A.A., Filonova E.V., Lukinа E.A. The use of methods of analytical microscopy and x-ray diffraction analysis for the study of the structural phase state materials // Proceedings of VIAM. 2013. No. 5. Ст. 06. URL: https://www.viam-works.ru.

The use of methods of analytical microscopy and x-ray diffraction analysis for the study of the structural phase state materials

Chabina E.B., Alekseev A.A., Filonova E.V., Lukinа E.A.
Abstract

The report on the specific examples show how the methods of analytical microscopy (optical, laser scanning, scanning and transmission electron microscopy) and X-ray microprobe analysis was used to study the structure-phase state of various materials aero-tional purposes: heat-resistant nickel alloys, aluminum alloys, hardening sculpt nanostructured and nanolayer coatings.