Ivankov R.R., Sidorina A.I., Kotomin S.V. The relationship between fiber wettability and adhesion value in the «fiber–polymer matrix» system // Proceedings of VIAM. 2026. No. 6 (160). С. 154–165. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-6-154-165.

The relationship between fiber wettability and adhesion value in the «fiber–polymer matrix» system

Ivankov R.R., Sidorina A.I., Kotomin S.V.
Abstract

In the article the adhesion of VSE-30 epoxy binder to fibers from various manufacturers was determined. The wettability of the carbon fiber surface by the epoxy binder was assessed. The article studies the relationship between horizontal impregnation and the adhesion strength. The carbon fibers are washed from the epoxy impregnation using a Soxhlet extractor. Photographs of the carbon fiber surface were obtained using a scanning electron microscope.

Keywords
carbon fibers, wettability, epoxy binder, finish coat, polymer composite material
Reference list
  1. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Rudskoy A.I. Technological heredity in the production and operation of structural materials. Tekhnologiya metallov, 2019, no. 2, pp. 2–10.
  3. Tkachuk A.I., Donetsky K.I., Terekhov I.V., Karavaev R.Yu. The use of thermosetting matrices for the manufacture of polymer composite materials by the non-autoclave molding methods. Aviation materials and technology, 2021, no. 1 (62), pp. 22–33. Available at: https://www.journal.viam.ru (accessed: September 02, 2025). DOI: 10.18577/2713-0193-2021-0-1-22-33.
  4. Yarullin R.R. Modification of epoxy resins as a method for producing composite materials with specified physical and mechanical characteristics (review). Plasticheskie massy, 2024, no. 5, pp. 11–17. DOI: 10.35164/0554-2901-2024-05-11-17.
  5. Voitenko V.A., Privalova N.M. Modification of compounds based on epoxy resins. Nauchnye trudy KubGTU, 2019, no. 7, pp. 288–295.
  6. Maksimova Yu.R., Shabalkina T.Yu., Yumanova L.A. et al. Modification of epoxy resin with furfuryl alcohol. Nauchnye izvestiya, 2022, no. 29, pp. 232–234.
  7. Lyubibogov A.A., Khamzina D.A., Borisov S.V. et al. Modification of ED-20 epoxy resin with copper and ammonium phosphates. Klei. Germetiki. Tekhnologii, 2025, no. 5, pp. 42–48. DOI: 10/31044/1813-7008-2025-0-5-42-48.
  8. Kilyakov D.A., Tatarkanov A.A. Modification of epoxy resins with carbon nanotubes (review). Theory and practice of priority scientific research: Coll. of sci. papers based on the materials of the X Int. Sci. and Pract. Conf. Smolensk: Naukosfera, 2019, pp. 44–49.
  9. Mukhamedgaliev B.A. Development of a technology for modifying ED-20 epoxy resin with phosphorus-containing polymers. Khimicheskaya promyshlennost segodnya, 2005, no. 3, pp. 44–47.
  10. Sadygov Sh.F., Ishchenko N.Ya., Nazaraliev Kh.G., Agaeva S.A. Halogen-containing modifiers for epoxy resins. Plasticheskie massy, 2011, no. 4, pp. 34–26.
  11. Mukhametov R.R., Petrova A.P. Thermosetting binders for polymer composites (review). Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 48–58. DOI: 10.18577/2071-9140-2019-0-3-48-58.
  12. Nurmukhametova A.N., Khamidullin A.R., Zenitova L.A. Carbon fiber. Obtaining, modification, properties, areas of application. Butlerovskiye soobshcheniya, 2020, vol. 62, no. 5, pp. 1–44.
  13. Grigoryan N.S., Gubanov A.A., Vagramyan T.A., Korshak Yu.V. Electrochemical modification of the surface of carbon fiber. Zhurnal prikladnoy khimii, 2015, vol. 88, no. 7, pp. 1059–1065.
  14. Andrianova N.N., Borisov A.M., Vorobyova E.A. et al. Modification of the Carbon Fiber Surface by Irradiation with Plasma Ions with Energies from Hundreds of eV to Tens of KeV. Yadernaya fizika i inzhiniring, 2024, vol. 15, no. 3, pp. 224–231. DOI: 10.56304/S2079562923030028.
  15. Morozov S.V. Influence of Carbon Fiber Surface Modification on the Physicomechanical Characteristics of Carbon Fiber Reinforced Plastics. Polzunovskiy Vestnik, 2022, no. 1, pp. 134–138.
  16. Klimenko I.V. Pitch-Based Carbon Fibers: State of Production and Property Modification. Khimicheskaya fizika, 2022, vol. 41, no. 2, pp. 70–77.
  17. Ivankov R.R. Determination of the strength of the adhesive bond between carbon fibers and an epoxy matrix. Physical and mechanical tests, strength and reliability of modern structural and functional materials: Proc. XVII All-Rus. Conf. on Testing and Research of Material Properties «TestMat». Moscow, 2025, pp. 140–162.
  18. Ivankov R.R., Sidorina A.I., Kotomin S.V. Determination of the strength of the adhesive bond between Russian carbon fibers and an epoxy matrix using the «loop» pull-out test. Trudy VIAM, 2026, no. 12 (154), pp. 170–184. Available at: http://www.viam-works.ru (accessed: October 15, 2025). DOI: 10.18577/2307-6046-2025-0-12-170-184.
  19. Gorbatkina Yu.A. Adhesion strength in polymer-fiber systems. Moscow: Khimiya, 1987, 192 p.
  20. Gorbatkina Yu.A., Zhuravleva O.A., Ivanova-Mumzhieva V.G., Chebotarev V.P. Effect of polysulfone molecular weight on the adhesion of epoxy-polysulfone binders to fibers. Plasticheskie massy, 2017, no. 5–6, pp. 14–17.
  21. Nelyub V.A., Guskov A.M., Belov P.A. On the design of carbon fiber-reinforced plastics for tensile testing taking into account fiber adhesion to the matrix. Aktualnye problemy gumanitarnykh i yestestvennykh nauk, 2014, no. 12-1, pp. 62–66.
  22. Nelyub V.A. Experimental evaluation of the elastic modulus of the adhesive bond of the epoxy matrix – carbon fiber with a metal coating system. Sovremennye naukoyemkie tekhnologii, 2019, no. 6, pp. 96–100.
  23. Oreshko E.I., Erasov V.S., Yakovlev N.O., Utkin D.A. Methods for determining the mechanical characteristics of materials using indentation (review). Aviation materials and technology, 2021, no. 1 (62), рр. 104–118. Available at: http://www.journal.viam.ru (accessed: October 15, 2025). DOI: 10.18577/2713-0193-2021-0-1-104-118.
  24. Gulyayev A.I. Fiber-matrix adhesion strength measurement using nanoindentation (review). Trudy VIAM, 2019, no. 3 (75), рр. 68–78. Available at: http://www.viam-works.ru (accessed: October 15, 2025). DOI: 10.18577/2307-6046-2019-0-3-68-78.
  25. Timoshkov P.N., Goncharov V.A., Usacheva M.N., Khrulkov A.V. Features of technology and polymer composite materials for the manufacture of wings of advanced aircraft (review). Trudy VIAM, 2022, no. 1 (107), рр. 66–75. Available at: http://www.viam-works.ru (accessed: October 15, 2025). DOI: 10.18577/2307-6046-2022-0-1-66-75.
  26. Belinis P.G., Donetskiy K.I., Lukyanenko Yu.V., Rogozhnikov V.N., Mayer Yu., Bystrikova D.V. Volume reinforcing solid-woven preforms for manufacturing of polymer composite materials (review). Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 18–26. DOI: 10.18577/2071-9140-2019-0-4-18-26.
  27. Rekhviashvili S.Sh., Kishtikova E.V. Surface tension, linear tension and contact angle of a small drop under isothermal conditions. Fizikokhimiya poverkhnosti i zashchita materialov, 2014, vol. 50, no. 1, pp. 3–7. DOI: 10.7868/S0044185614010112.
  28. Valueva M.I., Zelenina I.V., Khaskov M.A., Gulyaev A.I. Preparation of carbon fibers to interphase coating deposition for ceramic matrix composites. Trudy VIAM, 2017, no. 10 (58), pp. 79–89. Available at: http://www.viam-works.ru (accessed: October 15, 2025). DOI: 10.18577/2307-6046-2017-0-10-9-9.
  29. Zlobina I.V., Bekrenev N.V., Churikov D.O. Evaluation of filler wettability by binder in the process of ultrasound-assisted prepreg manufacturing for three-dimensional printing with continuous carbon fiber-reinforced filaments. Izvestiya Saratovskogo universiteta. Novaya seriya. Ser.: Fizika, 2024, vol. 24, no. 1, pp. 52–61. DOI: 10.18500/1817-3020-2024-24-1-52-61.
  30. Ilyin S.O., Kotomin S.V. The effect of nanoparticles and their anisometry on the adhesion and strength of hybrid epoxy nanocomposites reinforced with carbon fiber. Journal of Composites Science, 2023, vol. 7, no. 4, p. 147.
  31. Kudryavtseva A.N., Tkachuk A.I., Grigorieva K.N., Gurevich Ya.M. The use of epoxy resin system VSE-30, processed by the infusion technology, for the manufacture of low and medium loaded structural polymer composite materials. Trudy VIAM, 2019, no. 1 (73), pp. 31–39. Available at: http://www.viam-works.ru (accessed: October 15, 2025). DOI: 10.18577/2307-6046-2019-0-1-31-39.
  32. Kotomin S.V., Obidin I.M., Pavlyuchkova E.A. Calculation of the strength of the adhesive bond of reinforcing fibers with polymers using the «loop» method. Mekhanika kompozitnykh materialov, 2022, vol. 58, no. 1, pp. 197–212.
  33. Kotomin S.V., Obidin I.M., Pavlyuchkova E.A. Scale factor in testing adhesive-glue joints of heteroaramid yarns using the «loop» method. Klei. Germetiki. Tekhnologii, 2023, no. 11, pp. 35–40.
  34. Gulyaev A.I., Medvedev P.N., Sbitneva S.V., Petrov A.A. Experimental research of «fiber–matrix» adhesion strength in carbon fiber epoxy/polysulphone composite. Aviacionnye materialy i tehnologii, 2019, no. 4 (57), pp. 80–86. DOI: 10.18577/2071-9140-2019-0-4-80-86.