Yashin M.S., Shpagin A.S., Vostrikov A.V. Improvement of the mechanical properties of granulated heat-resistant nickel-based alloys by their complex alloying // Proceedings of VIAM. 2026. No. 6 (160). С. 19–31. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-6-19-31.

Improvement of the mechanical properties of granulated heat-resistant nickel-based alloys by their complex alloying

Yashin M.S., Shpagin A.S., Vostrikov A.V.
Abstract

This review analyzes the influence of alloying elements on the mechanical properties of granulated high-temperature nickel alloys. It is shown that the introduction of alloying elements such as Al, Ti, W, Mo, Nb, Ta, and Hf into the alloys contributes to material strengthening. Alloying with γ-forming elements such as Co and Cr leads to an increased creep resistance at temperatures up to 750 °C and heat resistance. A small content of microalloying elements such as B and Zr also has a positive effect on ductility.

Keywords
nickel-based heat-resistant alloy, granules, granule metallurgy, pressure treatment, deformation, hot isostatic pressing, alloying
Reference list
  1. Echin A.B., Bondarenko Yu.A., Kolodyazhny M.Yu., Surova V.A. Review of perspective high-temperature superalloys based on refractory non-metallic materials for production of gas turbine engines. Aviation materials and technologies, 2023, no. 3 (72), pp. 30–41. Available at: http://www.journal.viam.ru (accessed: October 13, 2025). DOI: 10.18577/2713-0193-2023-0-3-30-41.
  2. Min P.G., Vadeev V.E. The development and introduction into serial production of the new superalloy VZhL125 for the advanced aviation engines vanes. Aviation materials and technologies, 2023, no. 1 (70), pp. 3–16. Available at: http://www.journal.viam.ru (accessed: October 13, 2025). DOI: 10.18577/2713-0193-2023-0-1-3-16.
  3. Kolyadov E.V., Visik E.M., Gerasimov V.V., Bityutskaya O.N. Features of the morphology of the structure of nickel superalloy depending on the values of the axial and radial temperature gradients at the crystallization front. Aviation materials and technologies, 2024, no. 2 (75), pp. 15–24. Available at: http://www.journal.viam.ru (accessed: October 13, 2025). DOI: 10.18577/2713-0193-2024-0-2-15-24.
  4. Narsky A.R., Deynega G.I., Kuzmina I.G. Obtaining a fine-grained structure of castings from nickel superalloys using a cobalt aluminate modifier. Aviation materials and technologies, 2023, no. 3 (72), pp. 3–14. Available at: http://www.journal.viam.ru (accessed: October 13, 2025). DOI: 10.18577/2713-0193-2023-0-3-3-14.
  5. Garibov G.S. Development Prospects of Domestic Disk Granulated Heat-Resistant Nickel Alloys for New Types of Aviation Equipment. Tekhnologiya legkikh splavov, 2017, no. 1, pp. 7–18.
  6. Garibov G.S. Current Level of Development of Powder Metallurgy of Heat-Resistant Nickel Alloys. Tekhnologiya legkikh splavov, 2000, no. 6, pp. 58–69.
  7. Shmotin Yu.N., Starkov R.Yu., Logunov A.V., Danilov D.V. Advanced Materials and Manufacturing Technologies for Turbine Disks. Tekhnologiya legkikh splavov, 2013, no. 4, pp. 132–134.
  8. Vostrikov A.V., Sukhov D.I. The production of powders by PREP method for addictive manufacturing – current situation and development prospects. Trudy VIAM, 2016, no. 8, pp. 17–23. Available at: http://www.viam-works.ru (accessed: December 15, 2025). DOI: 10.18577/2307-6046-2016-0-8-3-3.
  9. Inozemtsev A.A., Anoshkin N.F., Bashkatov I.G. et al. Application of disks made of heat-resistant nickel alloy granules in serial gas turbine engines of aviation and ground equipment. Advanced technologies of light and special alloys. Moscow: Fizmatlit, 2006, pp. 371–376.
  10. Dreshfield R.L., Miner R.V. Effects of Thermally Induced Porosity on an as-HIP Powder Metallurgy Superalloy Effects of Thermally Induced Porosity on an as-HIP Powder Metallurgy Superalloy. International Journal of Powder Metallurgy, 1980, vol. 12, pp. 83–87.
  11. Garibov G.S., Tlyusten T.Yu. VILS gas stators. Zagotovitelnye proizvodstva v mashinostroyenii, 2010, no. 7, pp. 28–32.
  12. Garibov G.S., Grits N.M., Volkov A.M. et al. Metallographic aspects of the production of disk blanks from granulated heat-resistant nickel alloys by the HIP method. Tekhnologiya legkikh splavov, 2014, no. 3, pp. 54–58.
  13. Eisen W. PM Superalloys: past, present, and future. New jet enjine designs and advanced engines may lead to the increased usage of improved PM superalloys in the future. Materials World, 1996, no. 4, pp. 22–24.
  14. Skibin V.A., Solonin V.I., Palkin V.A. Works of leading aircraft engine manufacturing companies on the creation of advanced aircraft engines. Moscow: CIAM, 2004, 421 p.
  15. Superalloy optimized for high-temperature performance in high-pressure turbine disks: pat. 6521175 USA; appl. 09.02.98; publ. 18.02.03.
  16. Logunov A.V., Zavodov S.A., Danilov D.V. Development and study of a new nickel-based heat-resistant alloy for gas turbine disks. Vestnik RGATA im. P.A. Soloveva, 2019, no. 1 (48), pp. 62–68.
  17. Supersolvus processing for tantalum-containing nickel base superalloys: pat. 5662749 USA; appl. 07.06.95; publ. 02.09.97.
  18. Cao W.D., Kennedy R.L. New developments in wrought 718-type superalloys. Acta Metallurgica Sinica (English Letters), 2005, no. 1, pp. 39–46.
  19. Samoilov A.I., Kablov E.N., Petrushin N.V., Roshchina I.N. Dimensional mismatch of the crystal lattices of the γ- and γʹ-phases in nickel-rhenium-containing heat-resistant alloys. Aviatsionnye materialy i tekhnologii, 2004, no. 1, pp. 48–57.
  20. Khryashchev I.I., Danilov D.V., Logunov A.V. Development of an economically alloyed nickel-based heat-resistant alloy for gas turbine blades. Vestnik Moskovskogo aviatsionnogo instituta, 2019, no. 2 (26), pp. 205–208.
  21. Reed R.C. The Superalloys. Fundamentals and Applications. Cambridge: University Press, 2006, 372 p.
  22. Gayada J., Gabb T.P. Fatigue Behavior of a Third Generation PM Disk Superalloy. NASA-TM, 2008, 26 p.
  23. Guedou J., Augustins-Lecallier I., Caron P. Development of a New Fatigue and Greep Resistant PM Nickel-Base Superalloy for Disk Applications. Superalloys 2008. Pennsylvania: TMS, 2008, pp. 21–30.
  24. Nickel base superalloy: pat. 7208116 USA; appl. 26.09.01; publ. 24.04.07.
  25. Cu Y., Cui C., Harada H. et al. Development of Ni–Co-Base Alloys for High-Temperature Disk Applications. Superalloys 2008. Pensylvania: TMS, 2008, pp. 53–62.
  26. Rice D., Kantzos P., Hann B. et al. P/M Alloy 10 – A 700°C Capable Nickel-Based Superalloy for Turbine Disk Applications. Superalloys 2008. Pennsylvania: TMS, 2008, pp. 139–148.
  27. Shein E.A. Tendencies in the field of alloying and microalloying of heat resisting single-crystal alloys on the basis of nickel (review). Trudy VIAM, 2016, no. 3, pp 10–22. Available at: http://www.viam-works.ru (accessed: October 13, 2025). DOI: 10.18577/2307-6046-2016-0-3-2-2.
  28. High strength powder metallurgy nickel base alloy: pat. 6468368 USA; appl. 20.03.00; publ. 22.10.02.
  29. Nickel-base superalloys and components formed thereof: pat. 20100329876 USA; appl. 30.06.09; publ. 02.12.10.
  30. Garibov G.S., Grits N.M. V.I. Dobatkin and metallurgy of granules of heat-resistant nickel alloys. Tekhnologiya legkikh splavov, 2015, no. 2, pp. 34–39.
  31. Garibov G.S., Grits N.M., Vostrikov A.V., Fedorenko E.A. Development of a new high-strength alloy VV751P for advanced gas turbine engines. Tekhnologiya legkikh splavov, 2009, no. 1, pp. 34–39.
  32. Beresnev A.G., Razumovsky V.I., Lozovoy A.Yu. et al. Development of alloying theory for the creation of a new generation of heat-resistant nickel alloys obtained by powder metallurgy methods. Tekhnologiya legkikh splavov, 2012, no. 2, pp. 52–61.
  33. Garibov G.S., Grits N.M., Vostrikov A.V., Fedorenko E.A. Development and study of a new granulated high-strength heat-resistant nickel alloy VV752P for promising aviation products. Tekhnologiya legkikh splavov, 2011, no. 1, pp. 7–11.
  34. Eliseev Yu.S., Maslenkov S.B., Geikin V.A., Poklad V.A. Technology of creating permanent joints in the production of gas turbine engines. Moscow: Science and Technology, 2001, 544 p.
  35. Ber L.B., Kazberovich A.M. The influence of alloying and some structural factors on the set of characteristics of disk blanks made of granulated heat-resistant nickel alloys EP741NP, VV750P, VV751P, VV752P and VV753P. Tekhnologiya legkikh splavov, 2019, no. 3, pp. 16–33.
  36. Forde P.T. Tantalum in superalloys. Advanced Materials and Processes, 1996, no. 149 (4), pp. 39–40.
  37. Garibov G.S., Grits N.M. Ways to Create New High-Heat-Resistant Granulated Alloys for Advanced Aircraft Engines. Tekhnologiya legkikh splavov, 2012, no. 3, pp. 35–43.
  38. Garibov G.S., Vostrikov A.V., Grits N.M., Fedorenko E.A. Development of New Granulated Heat-Resistant Nickel Alloys for the Production of Aircraft Engine Disks and Shafts. Tekhnologiya legkikh splavov, 2010, no. 2, pp. 34–43.
  39. Method for Obtaining a Product from VV751P Alloy with High Strength and Heat Resistance: pat. 2453398 Rus. Federation; appl. 14.06.11; опубл. 20.06.12.
  40. Heat-resistant nickel alloy: pat. 2697674 Rus. Federation; appl. 24.05.19; опубл. 16.08.19.
  41. Volkov A.M., Vostrikov A.V., Bakradze M.M. Development of a new granulated heat-resistant nickel alloy VZh178P for promising aircraft gas turbine engines. Promising heat-resistant nickel deformable alloys and technologies for their processing: Proc. All-Rus. sci. and tech. conf. Moscow, 2018, pp. 25–38.