Dvoretskov R.M., Karachevtsev F.N., Burkovskaya N.P., Savina K.V. Determination of boron nitride BN in composite powder materials using inductively coupled plasma atomic emission spectrometry // Proceedings of VIAM. 2026. No. 5 (159). С. 174–185. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-5-174-185.

Determination of boron nitride BN in composite powder materials using inductively coupled plasma atomic emission spectrometry

Dvoretskov R.M., Karachevtsev F.N., Burkovskaya N.P., Savina K.V.
Abstract

The growing use of boron nitride powder for the manufacture of coatings has led to the need for its quantitative determination in the composition of industrial materials – in composite powders for the production of run-in coatings for gas turbine engines. In this paper, a method is proposed for the determination of boron nitride in composite coatings by inductively coupled plasma atomic emission spectrometry with two pre-sample preparation options: fusion with sodium hydroxide and autoclave decomposition in acids.

Keywords
boron nitride, composite materials, workable coatings, abrasion coatings, chemical analysis, analytical control, atomic emission spectroscopy, inductively coupled plasma, fusion, microwave decomposition
Reference list
  1. Kablov E.N., Antipov V.V. The role of new generation materials in ensuring the technological sovereignty of the Russian Federation. Vestnik Rossiyskoy akademii nauk, 2023, vol. 93, no. 10, pp. 907–916. DOI: 10.31857/S0869587323100055.
  2. Migunov V.P., Farafonov D.P., Degovets M.L., Stupina T.I. Sealing materials for flowing path of GTE. Aviacionnye materialy i tehnologii, 2012, no. S, pp. 94–97.
  3. Turchenko M.V., Lebedeva Yu.E., Prokofiev V.A., Zhitnyuk S.V. Investigation of the boron nitride effect on the machinability of SiC–ZrB2 system ceramic material. Trudy VIAM, 2024, no. 2 (132), pp. 57–66. Available at: http://www.viam-works.ru (accessed: August 03, 2025). DOI: 10.18577/2307-6046-2024-0-2-57-66.
  4. Voronov V.A., Chainikova A.S., Lebedeva Yu.E., Zhitnyuk S.V. Production, physico-mechanical and tribotechnical properties of hot-pressed carbon-ceramic composite material on the basis of silicon carbide. Aviation materials and technologies, 2022, no. 2 (67), pp. 74–84. Available at: http://www.journal.viam.ru (accessed: August 03, 2025). DOI: 10.18577/2713-0193-2022-0-2-74-84.
  5. Zhivushkin A.A., Polyansky S.B., Tikhomirova E.A. et al. Applied and promising sealing materials in the products of JSC «UEC-Klimov». Proc. XI All-Rus. Conf. on Testing and Research of Material Properties «TestMat» «Physical and Mechanical Testing, Strength, Reliability, High-Temperature Testing». Moscow: VIAM, 2019, pp. 429–438.
  6. Farafonov D.P., Migunov V.P., Sarayev A.A., Leshchev N.E. Abradability and erosion resistance of seals in turbine engine air-gas channel. Trudy VIAM, 2018, no. 8 (68), pp. 70–80. Available at: http://www.viam-works.ru (accessed: October 02, 2025). DOI: 10.18577/2307-6046-2018-0-8-70-80.
  7. Farafonov D.P., Leshchev N.E., Afanasiev-Khodykin A.N., Artemenko N.I. Abrasive wear-resistant seal materials of the gas turbine engine flow section. Aviacionnye materialy i tehnologii, 2019, no. 3 (56), pp. 67–74. DOI: 10.18577/2071-9140-2019-0-3-67-74.
  8. Abrasion-resistant sealing coating (operating temperature up to 800°C): pat. 2791541C1 Rus. Federation; appl. 27.06.22; publ. 09.03.23.
  9. Maltsev I.M., Getmanovsky Yu.A. Production and properties of rolled products from clad powders NPG-80 and Nibon-20. Izvestiya vysshikh uchebnykh zavedeniy. Poroshkovaya metallurgiya i funktsionalnye pokrytiya, 2023, vol. 17, no. 1, pp. 5–11. DOI: 10.17073/1997-308X-2023-1-5-11.
  10. Sintered sealing material for gas turbine engines: pat. Rus. Federation; appl. 18.12.17; publ. 04.09.19.
  11. Karpov Yu.A., Baranovskaya V.B. Analytical Control – an Integral Part of Materials Diagnostics. Zavodskaya laboratoriya. Diagnostika materialov, 2017, vol. 83, no. 1, pp. 5–12.
  12. Lidin R.A., Molochko V.A., Andreeva L.L. Chemical Properties of Inorganic Substances. Moscow: Khimiya, 2000, 480 p.
  13. Kurdyumov A.V., Pilyankevich A.N., Shulman L.A. et al. Polymorphic Modifications of Carbon and Boron Nitride: Reference Book. Moscow: Metallurgiya, 1994, 318 p.
  14. Ryashentsev D.S. Structure and Electronic Properties of New Polymorphic Varieties of Boron Nitride: thesis, Cand. Sc. (Phys.&Math.). Chelyabinsk, 2023, 148 p.
  15. Karpov Yu.A., Baranovskaya V.B. Problems of standardization of chemical analysis methods in metallurgy. Zavodskaya laboratoriya. Diagnostika materialov, 2019, vol. 85, no. 1–2, pp. 5–14.
  16. Baranovskaya V.B., Medvedevskikh M.Yu., Karpov Yu.A. Actual problems of the quality of chemical analysis. Analitika i kontrol, 2021, vol. 25, no. 4, pp. 273–279. DOI: 10.15826/analitika.2021.25.4.005.
  17. Otto M. Modern methods of analytical chemistry: in 2 vols. Trans. from Germ. Ed. A.V. Garmash. Moscow: Tekhnosfera, 2003, 416 p.
  18. Lepilina M.Yu., Yakubenko E.V., Ermolaeva T.N., Baranovskaya V.B. Development of a method for X-ray fluorescence analysis of zinc-aluminum-magnesium alloys. Zavodskaya laboratoriya. Diagnostika materialov, 2024, vol. 90, no. 2, pp. 5–11. DOI: 10.26896/1028-6861-2024-90-2-5-11.
  19. Dvoretskov R.M., Slavin A.V., Letov A.F., Karachevtsev F.N. Determination of trace elements of rare earth metals and Ca, Mg, V, Zr, Hf in nickel alloys by atomic emission spectrometry. Zhurnal analiticheskoy khimii, 2020, vol. 75, no. 8, pp. 682–691. DOI: 10.31857/S004445022008006X.
  20. Karachevtsev F.N., Dvoretskov R.M., Zagvozdkina T.N. Determination of silver in aluminum alloys by atomic emission spectrometry with inductively coupled plasma. Aviation materials and technologies, 2022, no. 1 (66), pp. 143–152. Available at: http://www.journal.viam.ru (accessed: August 03, 2025). DOI: 10.18577/2713-0193-2022-0-1-143-152.
  21. Surikov V.T. Acid dissolution of silicon and its compounds for analysis by inductively coupled plasma mass spectrometry. Analitika i kontrol, 2008, vol. 12, no. 3–4, pp. 93–100.
  22. Dulnev K.V., Sevalnev G.S., Pahomkina T.N., Buzenkov A.V. Study of changes in microstructure, grain size and nitrogen concentration depending on heat treatment temperature of high-strength structural high-nitrogen steel. Aviation materials and technologies, 2025, no. 3 (80), pp. 3–14. Available at: http://www.journal.viam.ru (accessed: October 02, 2025). DOI: 10.18577/2713-0193-2025-0-3-3-14.
  23. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  24. Nemodruk A.A., Karalova Z.K. Analytical Chemistry of Boron. Moscow: Nauka, 1964, 285 p.
  25. Bock R. Decomposition Methods in Analytical Chemistry. Moscow: Khimiya, 1984, 432 p.
  26. Negina V.R., Kozyreva E.A., Degtyareva O.F. et al. Analysis of Boron, Its Compounds, and Press Compositions: A Practical Guide. Moscow: Atomizdat, 1978, 92 p.
  27. Vasilyeva M.G., Lalykina V.M., Makharashvili N.A. et al. Analysis of Boron and Its Inorganic Compounds. Ed. by E.E. Baroni. Moscow: Atomizdat, 1965, 268 p.
  28. Yadav A., Bulakh N., Gupta A. et al. Rapid determination of impurity of boron nitride in amorphous boron powder using inductively coupled plasma-atomic emission spectrometry (ICP-AES) and ion chromatography (IC). Analytical Methods, 2017, vol. 9, no. 21, pp. 3141–3150. DOI: 10.1039/c7ay00140a.