Butuzov A.V., Lebedeva Yu.E., Semina A.V., Serkova E.A., Lonskii S.L. Influence of the nature and concentration of the wetting-dispersing additive on the rheological properties and stability of highly filled ceramic slurries based on aluminum oxide // Proceedings of VIAM. 2026. No. 4 (158). С. 85–103. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-4-85-103.

Influence of the nature and concentration of the wetting-dispersing additive on the rheological properties and stability of highly filled ceramic slurries based on aluminum oxide

Butuzov A.V., Lebedeva Yu.E., Semina A.V., Serkova E.A., Lonskii S.L.
Abstract

The article investigates the effect of the nature and concentration of wetting and dispersing additives on the rheological properties and stability of model ceramic slurries based on (meth)acrylate resin and aluminum oxide. The influence of the mass fraction of aluminum oxide on the rheology and stability of ceramic slurries is presented. Stable highly filled ceramic slurries with an alumina particle content of 51,5; 55,4 and 60,0 vol. % and low viscosity 2,16; 4,09 and 6,06 Pa∙s at a shear rate of 30 s–1 at a temperature of 25 °C were obtained.

Keywords
aluminum oxide, ceramic slurries, additive technologies, wetting and dispersing additives, rheology, sedimentation
Reference list
  1. Aza A., Chevalier J., Fantozzi G. et al. Crack growth resistance of alumina, zirconia and zirconia toughened alumina ceramics for joint prostheses. Biomaterials, 2002, no. 23 (3), pp. 937–945. DOI: 10.1016/s0142-9612(01)00206-x.
  2. Tolkacheva A.S. Ceramic Technology for Electronics Materials. Part 1. Ekaterinburg: Ural Univ. Press, 2019, 124 p.
  3. Kablov E.N. Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030». Aviacionnye materialy i tehnologii, 2015, no. 1 (34), pp. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  4. Kang J., Song X.G., Hu S.P. et al. Wetting and brazing of alumina by Sn0,3Ag0,7Cu–Ti alloy. Metallurgical and Materials Transactions A, 2017, vol. 48 (12), pp. 5870–5878. DOI: 10.1007/s11661-017-4371-8.
  5. Willmann G. Ceramic femoral heads for total hip arthroplasty. Advanced Engineering Materials, 2000, vol. 2 (3), pp. 114–122.
  6. Denry I., Kelly J.R. Emerging ceramic-based materials for dentistry. Journal of Dental Research, 2014, vol. 93 (12), pp. 1235–1242. DOI: 10.1177/0022034514553627.
  7. Wei L., Zhang J., Yu F. A novel fabrication of yttriastabilized-zirconia dense electrolyte for solid oxide fuel cells by 3D printing technique. International Journal of Hydrogen Energy, 2019, vol. 44 (12), pp. 6182–6191. DOI: 10.1016/j.ijhydene.2019.01.071.
  8. Fei J., Qiaolei L., Kun Y. et al. Optimisation and application of high solid loading stereolithography 3D printing ceramic cores slurry. Ceramics International, 2024, vol. 50 (2), pp. 3574–3583. DOI: 10.1016/j.ceramint.2023.11.107.
  9. Turchenko M.V., Lebedeva Yu.E., Butuzov A.V., Svetogorov K.I., Vaganova M.L., Chainikova A.S. Production of high-density alumina ceramics by laser stereolithography. Liquid crystals and «smart» nanomaterials (XI Chistyakov readings): collection of papers. All-Rus. sci. conf. with Int. participation. Ivanovo: Publ. house of Ivanovo State Univ., 2025, p. 40.
  10. Bondareva N.S., Buonomo B., Manca O., Sheremet M.A. Heat transfer inside cooling system based on phase change material with alumina nanoparticles. Applied Thermal Engineering, 2018, vol. 144, pp. 972–981. DOI: 10.1016/j.applthermaleng.2018.09.002.
  11. Huang D.-S., Chen T.-C., Tsai L.-T., Lin M.-T. Design of fins with a grooved heat pipe for dissipation of heat from high-powered automotive LED headlights. Energy Conversion Management, 2019, vol. 180, pp. 550–558. DOI: 10.1016/j.enconman.2018.11.021.
  12. Minatto F.D., Milak P., De Noni A. et al. Multilayered ceramic composites – a review. Advances in Applied Ceramics, 2015, vol. 114 (3), pp. 127–138. DOI: 10.1179/1743676114Y.0000000215.
  13. Leo S., Tallon C., Stone N., Franks G.V. Near-netshaping methods for ceramic elements of (body) armor systems. Journal of the American Ceramic Society, 2015, vol. 97, pp. 3013–3033. DOI: 10.1111/jace.13192.
  14. Klocke F. Modern approaches for the production of ceramic components. Journal of the European Ceramic Society, 1997, vol. 17, pp. 457–465. DOI: 10.1016/S0955-2219(96)00163-X.
  15. Wang X., Luo Y. Diameter prediction of removal particles in Al2O3 ceramic laser cutting based on vapor-to-melt ratio. Journal of Materials Processing Technology, 2018, vol. 251, pp. 109–117. DOI: 10.1016/j.jmatprotec.2017.08.011.
  16. Wang J., Zhang J., Feng P. Effects of tool vibration on fiber fracture in rotary ultrasonic machining of C/SiC ceramic matrix composites. Composites Part B: Engineering, 2017, vol. 129, pp. 233–242. DOI: 10.1016/j.compositesb.2017.07.081.
  17. Kablov E.N. The Present and Future of Additive Technologies. Metally Evrazii, 2017, no. 1, pp. 2–6.
  18. Kablov E.N. Additive Technologies – the Dominant Focus of the National Technological Initiative. Intellekt i tekhnologii, 2015, no. 2 (11), pp. 52–55.
  19. Turchenko M.V., Lebedeva Yu.E., Belyachenkov I.O., Prokofiev V.A. Obtaining of ceramic materials by stereolithography method. Trudy VIAM, 2023, no. 9 (127). pp. 79–89. Available at: http://www.viam-works.ru (accessed: September 04, 2025). DOI: 10.18577/2307-6046-2023-0-9-79-89.
  20. Turchenko M.V., Lebedeva Yu.E., Kolmogorov A.Yu., Gurov D.A., Chainikova A.S. Possibility of using layer-by-layer deposition technology (FDM) to produce ceramic products. Trudy VIAM, 2024, no. 8 (138), pp. 64–76. Available at: http://www.viam-works.ru (accessed: October 12, 2025). DOI: 10.18577/2307-6046-2024-0-8-64-76.
  21. Lacelle T., Sampson K.L., Sarvestani H.Y. et al. Additive manufacturing of polymer derived ceramics: materials, methods, and applications. APL Materials, 2023, vol. 11, pp. 1–29. DOI: 10.1063/5.0151661.
  22. Tumbleston J.R., Shirvanyants D., Ermoshkin N. et al. Continuous liquid interface production of 3D objects. Science, 2015, vol. 347, pp. 1349–1352. DOI: 10.1126/science.aaa2397.
  23. Malaev I.A., Pivovarov M.L. Additive technologies: application in medicine and pharmacy. Vestnik farmatsii, 2019, no. 2 (84), pp. 98–107.
  24. Butuzov A.V., Semina A.V. Preceramic polymers for the production of ceramic products by vat photopolymerization. Part 1. Methods of production and properties. Trudy VIAM, 2025, no. 3 (145), pp. 70–88. Available at: http://www.viam-works.ru (accessed: September 04, 2025). DOI: 10.18577/2307-6046-2025-0-3-70-88.
  25. Camargo I.L., Morais M.M., Fortulan C.A., Branciforti M.C. A review on the rheological behavior and formulations of ceramic suspensions for vat photopolymerization. Ceramics International, 2021, vol. 47, pp. 11906–11921. DOI: 10.1016/j.ceramint.2021.01.031.
  26. Sarychev I.A., Butuzov A.V., Serkova E.A., Dolgova E.V. Photocurable acrylate compositions (review). Trudy VIAM, 2022, no. 9 (115), pp. 68–82. Available at: http://www.viam-works.ru (accessed: April 04, 2025). DOI: 10.18577/2307-6046-2022-0-9-68-82.
  27. Ligon S.C., Liska R., Stampfl J. et al. Polymers for 3D printing and customized additive manufacturing. Chemical Reviews, 2017, vol. 117, pp. 10212–10290. DOI: 10.1021/acs.chemrev.7b00074.
  28. Zhang K., Xie C., Wang G. et al. High solid loading, low photosensitive Al2O3 slurry for stereolithography based additive manufacturing. Ceramics International, 2019, vol. 45 (1), pp. 203–208. DOI: 10. 1016/j.ceramint.2018.09.152.
  29. Zhang S., Sha N., Zhao Z. Surface modification of α-Al2O3, with dicarboxylic acids for the preparation of UV-curable ceramic suspensions. Journal of the European Ceramic Society, 2017, vol. 37, pp. 1607–1616. DOI: 10.1016/j.jeurceramsoc.2016.12.013.
  30. Wu X., Lian Q., Li D. et al. Influence of boundary masks on dimensions and surface roughness using segmented exposure in ceramic 3D printing. Ceramics International, 2019, vol. 45 (3), pp. 3687–3697. DOI: 10.1016/j. ceramint.2018.11.031.
  31. Goswami A., Ankit K., Balashanmugam N. et al. Optimization of rheological properties of photopolymerizable alumina suspensions for ceramic microstereolithography. Ceramics International, 2014, vol. 40 (2), pp. 3655–3665. DOI: 10. 1016/j.ceramint.2013.09.059.
  32. Chartier T., Dupas C., Geffroy P.M. et al. Influence of irradiation parameters on the polymerization of ceramic reactive suspensions for stereolithography. Journal of the European Ceramic Society, 2017, vol. 37 (15), pp. 4431–4436. DOI: 10.1016/j.jeurceramsoc.2017.05.050.
  33. Hinczewski C., Corbel S., Chartier T. Ceramic suspensions suitable for stereolithography. Journal of the European Ceramic Society, 1998, vol. 18, pp. 583–590. DOI: 10.1016/S0955-2219(97)00186-6.
  34. Chartier T., Chaput C., Doreau F., Loiseau M. Stereolithography of structural complex ceramic parts. Journal of Materials Science, 2002, vol. 37, pp. 3141–3147. DOI: 10.1023/A:1016102210277.
  35. Li K.H., Zhao Z. The effect of the surfactants on the formulation of UV-curable SLA alumina suspension. Ceramics International, 2017, vol. 43, pp. 4761–4767. DOI: 10.1016/j.ceramint.2016.11.143.
  36. Alves P.L., Verza J.R., Luz A.P. Reological behavior of alumina suspensions for additive manufacturing using digital light processing. Materials Research, 2023, vol. 26 (1), pp. 1–6. DOI: 10.1590/1980-5373-MR-2023-0270.
  37. Verkhoshansky Ya.Yu., Tkachev D.A. Development and study of material for stereolithographic 3D printing based on Al2O3. Physics. Technologies. Innovations: abstract of report. XI Int. Youth Scientific Conf. Ekaterinburg: Ural Federal Univ. Publ. House, 2024, pp. 580–581.
  38. Richardson J.F., Zaki W.N. Sedimentation and fluidisation: Part I. Transactions of the Institution of Chemical Engineers, 1954, vol. 32, pp. 35–53. DOI: 10.1016/S0263-8762(97)80006-8.
  39. Mityukov A.V. Highly concentrated suspensions with matrices based on polymer compositions for powder injection molding: thesis, Cand. Sc. (Tech.), Мoscow, 2022, 145 р.
  40. Liu D.M. Particle packing and rheological property of highly-concentrated ceramic suspensions: ϕm determination and viscosity prediction. Journal of Materials Science, 2000, vol. 35, pp. 5503–5507. DOI: 10.1023/A:1004885432221.