Serdcelyubova A.S., Kondakov P.V., Ponomarenko S.A. Studying the properties of paint and varnish coatings based of hydroxyl-containing acrylate copolymers // Proceedings of VIAM. 2026. No. 3 (157). С. 157–166. URL: https://www.viam-works.ru. DOI: 10.18577/2307-6046-2026-0-3-157-166.

Studying the properties of paint and varnish coatings based of hydroxyl-containing acrylate copolymers

Serdcelyubova A.S., Kondakov P.V., Ponomarenko S.A.
Abstract

The article presents the study results of model paint and varnish compositions based on experimental hydroxyl-containing organosoluble acrylate copolymers.The chemical composition of the polymer matrix was assessed using gas chromatography-mass spectrometry, was determined the technological properties of the compositions, as well as physical, mechanical and decorative properties of coatings based on them, analyzed kinetics of curing. The possibility of using the studied copolymers in composition of paints and varnishes for obtaining coatings used in atmosphere conditions was determined.

Keywords
protective coatings, paints and varnishes, acrylate copolymers, acrylate enamels, acrylic urethane materials, film-forming, pyrolytic chromatography
Reference list
  1. Kablov E.N. New Generation Materials and Digital Technologies for Their Processing. Vestnik Rossiyskoy akademii nauk, 2020, vol. 90, no. 4, pp. 331–334.
  2. Kablov E.N. The Role of Fundamental Research in the Creation of New Generation Materials. Reports of the XXI Mendeleev Congress on General and Applied Chemistry: in 6 vols. St. Petersburg, 2019, vol. 4, p. 24.
  3. Kablov E.N. The Role of State Research Centers of the Russian Federation in Ensuring National Security. Perspektivnye tekhnologii dlya sistem bezopasnosti, 2023, no. 1, pp. 4–9.
  4. Erofeev V.T., Smirnov I.V., Voronov P.V., Afonin V.V., Kablov E.N. et al. Study of the durability of polymer coatings under the influence of climatic factors of the Black Sea coast. Fundamentalnye issledovaniya, 2016, no. 11-5, pp. 911–924.
  5. Kablov E.N., Semenova L.V., Eskov A.A., Lebedeva T.A. Complex systems of paint and varnish coatings for the protection of metal polymer composite materials, as well as their contact joints from the influence of aggressive factors. Lakokrasochnyye materialy i ikh primenenie, 2016, no. 6, pp. 32–35.
  6. Gorbovets M.A., Nikolaev E.V., Startsev V.O. Climate testing of Arctic materials. Part 1. Requirements for materials. Aviation materials and technologies, 2024, no. 4 (77), pp. 180–188. Available at: http://www.journal.viam.ru (accessed: April 20, 2025). DOI: 10.18577/2713-0193-2024-0-4-180-188.
  7. Kozlova A.A., Kondrashov E.K. Influence of molecular weight and elemental composition of isocyanates on the properties of fluoropolyurethane enamels. Aviation materials and technologies, 2023, no. 4 (73), pp. 92–100. Available at: http://www.journal.viam.ru (accessed: April 17, 2025). DOI: 10.18577/2713-0193-2023-0-4-92-100.
  8. Serdtselyubova A.S., Merkulova Yu.I., Zagora A.G., Kurshev E.V. Research of film-forming parameters and protective properties of basecoat/clearcoat system. Aviation materials and technologies, 2023, no. 1 (70), pp. 93–104. Available at: http://www.journal.viam.ru (accessed: April 15, 2025). DOI: 10.18577/2713-0193-2023-0-1-93-104.
  9. Gorbovets M.A., Nikolaev E.V., Startsev V.O. Climate testing of Arctic materials. Part 2. Test requirements. Aviation materials and technologies, 2025, no. 1 (78), pp. 138–147. Available at: http://www.journal.viam.ru (accessed: April 15, 2025). DOI: 10.18577/2713-0193-2025-0-1-138-147.
  10. Abrosimova L.F., Shakirova O.G. Anticorrosive paint and varnish material based on acrylic copolymers. Evraziyskiy Soyuz Uchenykh, 2016, no. 1 (22), pp. 21–23.
  11. Muratkina E.E. Acrylic copolymers in the production of paints and varnishes for road markings. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2009, no. 1–2, pp. 15–17.
  12. Brock T., Grotteklaus M., Mischke P. European Paints and Coatings Guide. Ed. U. Zorrell. Moscow: Paint-Media, 2007, 548 p.
  13. Kondrashov E.K., Semenova L.V., Kuznetsova V.A. et al. Development of aviation paints and varnishes. Vse materialy. Entsiklopedicheskiy spravochnik, 2012, no. 5, pp. 49–55.
  14. Shvets N.I., Zastrogina O.B., Minakov V.T., Matveeva I.A. Influence of tin carboxylates on the process of organosilicic oligomer binder curing and properties of the three-dimensional reinforced material on its base. Aviacionnye materialy i tehnologii, 2016, no. 2 (41), pp. 40–44. DOI: 10.18577/2071-9140-2016-0-2-40-44.
  15. Ponomarenko S.A., Shimkin A.A. Chromatographic methods of analysis: application possibilities in the aviation industry (review). Zavodskaya laboratoriya. Diagnostika materialov, 2017, no. 83 (4), pp. 5–13.
  16. State Standard 28614–90 (ISO 7270-87). Rubber. Identification of polymers (individual polymers and blends) by pyrolytic gas chromatography. Moscow: Publ. house of standards, 1990, 11 p.
  17. Sharabanova I.A., Spiridonova R.R., Kochnev A.M. Effect of ethylene glycol oligomers on the properties of polyamide esters. Vestnik Kazanskogo tekhnologicheskogo universiteta, 2011, no. 23, pp. 104–108.
  18. Kovalenko L.G. Modification of reactive oligomers with blocked isocyanates. Plastmassy, 1986, no. 11, pp. 34–37.